摘要:
A method for producing a condensation polymerization reaction polymer, comprising a guide polymerization step in which a molten prepolymer is supplied to the top edge of a wire guide to obtain the condensation polymerization reaction polymer, the wire guide comprising a vertical wire group consisting of a plurality of vertical wires extending in the vertical direction, which are mutually spaced in alignment at an arrangement pitch L1 (mm). In the guide polymerization step, the molten prepolymer aggregates so that a molten prepolymer mass is formed on the vertical wire, and a molten prepolymer mass is formed wherein, the width of the molten prepolymer mass measured in an alignment direction of the vertical wires at a position 200 mm below the top edge being represented as L2 (mm), the width L2 of at least a portion of the molten prepolymer mass satisfies the inequality (1). L1
摘要:
A polyethylene terephthalate resin which is obtained by melt polymerization at a reduced pressure or in an inert gas atmosphere and has the following properties (A) to (F): (A) the intrinsic viscosity [η] is 0.4-2.5 Dl/g; (B) the content of carboxy groups present at polymer ends is 30 meq/kg or lower; (C) the acetaldehyde content is 10 ppm or lower; (D) a hexafluoroisopropanol solution of the resin, when analyzed by the transmission method, has a hue which has an L value of 99 or larger and a b value of 0.4 or smaller; (E) the Mw/Mn is 1.8-2.3; and (F) the cyclic trimer content is 5 wt. % or lower.
摘要:
Disclosed is a method for producing an aromatic polycarbonate, which comprises treating a molten aromatic polycarbonate prepolymer (obtained by reacting an aromatic dihydroxy compound with a diaryl carbonate) with an inert gas under a predetermined pressure to thereby cause the molten prepolymer to absorb the inert gas, and subjecting the resultant molten prepolymer having the inert gas absorbed therein to polymerization, under a pressure lower than the above-mentioned predetermined pressure employed for the inert gas absorption, to thereby polymerize the prepolymer to a predetermined degree of polymerization. By the method of the present invention, a high quality aromatic polycarbonate which is colorless and has excellent mechanical properties can be produced at high polymerization rate even without using a large amount of an inert gas. Further, even if the production of an aromatic polycarbonate is conducted in a continuous manner, the molecular weight of the produced aromatic polycarbonate can be maintained at a desired level, so that the high quality polycarbonate can be stably produced for a prolonged period of time. Therefore, the method of the present invention is commercially very advantageous.
摘要:
A process for producing a polyacetal copolymer, which comprises copolymerizing formaldehyde and a compound selected from the group consisting of alkylene oxides, poly(alkylene oxides), cyclic formals and poly (cyclic formals) in the presence of a Lewis acid and an anionic polymerization catalyst with the exception of metal chelate compounds.
摘要:
Disclosed is a system for producing a polycondensation polymer comprising (A) an inert gas absorption device for causing a molten polycondensation prepolymer to absorb an inert gas to thereby obtain (&agr;) a molten prepolymer having the inert gas absorbed therein, (B) a polymerizer device for polymerizing inert gas-absorbed molten prepolymer (&agr;) under reduced pressure, and (C) a pipe for transferring inert gas-absorbed molten prepolymer (&agr;) from absorption device (A) to polymerizer device (B), wherein absorption device (A) and polymerizer device (B) are arranged in this order and connected to each other through pipe (C). Also disclosed is a method for producing a polycondensation polymer by using the above-mentioned system. By the use of the system or method of the present invention, it has become possible to produce a colorless, high quality polycondensation polymer at high polymerization rate even without using a large amount of an inert gas.
摘要:
A method for producing an aromatic polycarbonate which comprises subjecting to a transesterification polymerization reaction at least one polymerizable material for an aromatic polycarbonate, the transesterification reaction being performed in one or more polymerizers which is or are connected through a pipeline system toward an outlet for a final aromatic polycarbonate product, wherein the pipeline system comprises one or more pipes, through which a molten aromatic polycarbonate having a number average molecular weight increased by the transesterification polymerization reaction is passed while contacting an inner wall of the pipe or pipes, the pipeline system having at least one viscous polycarbonate passage region in which a molten aromatic polycarbonate having a number average molecular weight of 6,000 or more is passed through the pipe, wherein the pipe in the at least one viscous polycarbonate passage region is heated to provide a temperature difference in the range of from -3.degree. C. to 50.degree. C. between the temperature (.degree.C.) of the outer wall of the pipe and the temperature (.degree.C.) of the aromatic polycarbonate in the polymerizer from which the aromatic polycarbonate is passed through the pipe. By the method of the present invention, a high quality aromatic polycarbonate which is not only highly colorless but also has a low foreign matter content can be easily produced.
摘要翻译:一种芳族聚碳酸酯的制造方法,其特征在于,对至少一种芳族聚碳酸酯的聚合性材料进行酯交换聚合反应,所述酯交换反应是在一个或多个聚合反应器中进行的,所述聚合反应器是通过管道系统连接到出口, 芳族聚碳酸酯产品,其中管道系统包括一个或多个管道,使通过酯交换聚合反应增加数均分子量的熔融芳族聚碳酸酯通过该管道接触管道或管道的内壁,管道系统具有 至少一个粘性聚碳酸酯通道区域,其中数均分子量为6000以上的熔融芳族聚碳酸酯通过管,其中加热至少一个粘性聚碳酸酯通道区域中的管道以提供在该范围内的温度差 的-3 DE 在管道外壁的温度(℃)和温度(℃)之间,在聚合器中芳族聚碳酸酯通过管道的温度(℃)之间变化到50℃。 通过本发明的方法,可以容易地制备高品质的芳族聚碳酸酯,其不仅高度无色,而且异物含量低。
摘要:
The present invention provides a method of producing polyalkylene terephthalate, which comprises: introducing a prepolymer of polyalkylene terephthalate that is in a molten state comprising 70 mol % or more of ethylene terephthalate or 1,4-butylene terephthalate repeating units and having an intrinsic viscosity [η] between 0.2 and 2 dl/g through a feed opening to a polymerization reactor; discharging the introduced prepolymer from holes of a perforated plate; and polymerizing the prepolymer under reduced pressure, while allowing the prepolymer to fall along the surface of a support that is open towards the outside at a temperature between the [crystalline melting point−10° C.] of the prepolymer or higher and the [crystalline melting point+30° C.] of the prepolymer or lower under the conditions represented by a formula S1/S2>1, wherein S1 is the surface area of falling polyalkylene terephthalate, and S2 is the area where the support is in contact with polyalkylene terephthalate.
摘要:
A method for producing a polycondensation polymer, which comprises: introducing a prepolymer of a polycondensation polymer into a polymerization reactor through a feed opening in a molten state; discharging the introduced prepolymer through holes of a perforated plate; and then polycondensing the prepolymer under reduced pressure, while allowing the prepolymer to fall along a support, wherein the perforated plate has two or more areas and polycondensation is performed by introducing a prepolymer and/or a polymer modifier into each of the areas and discharging the introduced prepolymer and/or polymer modifier through holes of each of the areas.
摘要:
The present invention provides a method of producing polyalkylene terephthalate, which comprises: introducing a prepolymer of polyalkylene terephthalate that is in a molten state comprising 70 mol % or more of ethylene terephthalate or 1,4-butylene terephthalate repeating units and having an intrinsic viscosity [η] between 0.2 and 2 dl/g through a feed opening to a polymerization reactor; discharging the introduced prepolymer from holes of a perforated plate; and polymerizing the prepolymer under reduced pressure, while allowing the prepolymer to fall along the surface of a support that is open towards the outside at a temperature between the [crystalline melting point−10° C.] of the prepolymer or higher and the [crystalline melting point+30° C.] of the prepolymer or lower under the conditions represented by a formula S1/S2>1, wherein S1 is the surface area of falling polyalkylene terephthalate, and S2 is the area where the support is in contact with polyalkylene terephthalate.
摘要翻译:本发明提供一种聚对苯二甲酸亚烷基酯的制造方法,其特征在于,包括:引入聚对苯二甲酸亚烷基酯的预聚物,所述聚对苯二甲酸亚烷基酯处于熔融状态,所述聚对苯二甲酸亚烷基酯包含70摩尔% eta]为0.2-2d / g,通过聚合反应器的进料口; 从多孔板的孔排出引入的预聚物; 并且在减压下聚合预聚物,同时允许预聚物在预聚物的[结晶熔点-10℃]之间或更高的[温度]之间的温度沿着向外开口的载体表面落下 熔点+ 30℃],或者在由式S 1 / S 2 SUB> 1表示的条件下更低,其中S 1, SUB>是下降的聚对苯二甲酸亚烷基酯的表面积,S 2 O 2是支撑体与聚对苯二甲酸亚烷基酯接触的区域。
摘要:
A method for producing a molded product consisting of a resin polymerized by a melt polycondensation reaction, comprising continuous feeding of a prepolymer in molten state from a prepolymer feeding port to a polymerization reactor, discharging from holes of a porous plate, followed by polymerization while dropping along a supporting substrate under reduced pressure, and molding by transferring to at least one molding machine in molten state without solidification, wherein transfer pressure to said molding machine is controlled so as to maintain at an arbitrary pressure from 0.1 to 100 MPa (absolute pressure).