摘要:
A vulcanizable elastomer composition comprising an .alpha.-olefin copolymer comprising ethylene and an .alpha.-olefin(s) and an ethylene copolymer comprising ethylene and at least one member selected from the group consisting of acrylic and methacrylic esters, which has an excellent roll-processability and gives by vulcanization an elastomeric material having well-balanced properties in respect of resistance to heat and oil, low-temperature property and the like.
摘要:
An ethylene-.alpha.-olefin vulcanized rubber composition with excellent weather resistance and high transparency which is formed by vulcanizing with an organic peroxide an unvulcanized rubber composition comprising an ethylene-.alpha.-olefin rubber containing no metal oxide nor metal carbonate.
摘要:
The present invention provides an ethylene-acrylic acid ester copolymer giving low deformation during vulcanization and having a high dimensional accuracy and excellent properties, as well as a process for producing said copolymer.
摘要:
Herein is disclosed a vulcanizable rubber composition comprising a copolymer rubber constituted of ethylene, propylene and nonconjugated polyene, wherein ethylene/propylene molar ratio is 78/22 to 97/3 and the total content of propylene and nonconjugated polyene is 6 to 30% by mole in said copolymer rubber. By the use of the rubber composition of the present invention, a vulcanized product excellent in tensile strength, heat resistance, oil resistance, compression set resistance and flex behavior can be obtained. The vulcanized product can be used as automobile parts and other innumerable articles such as socket cover, heat resistant hose, electric wire, condenser cap, heat resistant belt, vibration-proof rubber, hoses weather strip, seal sponge, black side wall of tire, etc.
摘要:
Herein is disclosed a vulcanizable rubber composition comprising a copolymer rubber constituted of ethylene, propylene and nonconjugated polyene, wherein ethylene/propylene molar ratio is 78/22 to 97/3 and the total content of propylene and nonconjugated polyene is 6 to 30% by mole in said copolymer rubber. By the use of the rubber composition of the present invention, a vulcanized product excellent in tensile strength, heat resistance, oil resistance, compression set resistance and flex behavior can be obtained. The vulcanized product can be used as automobile parts and other innumerable articles such as socket cover, heat resistant hose, electric wire, condenser cap, heat resistant belt, vibration-proof rubber, hoses, weather strip, seal sponge, black side wall of tire, etc.
摘要:
In order to recover a polymer, such as styrene butadiene copolymer rubber, from a solution obtained by a solution polymerization of the corresponding comonomers, without degradation or deterioration of the polymer, the solution, ordinarily in 3 to 30% by weight concentration, is separated into the solvent and a more concentrated polymer solution of not less than 50% by weight, by heating the solution under a pressure at such a temperature (A) that the polymer does not decompose, heating a solvent, which is preferably the same as that for the solution, at a higher temperature than (A) above under a pressure, and joining the heated solution and the heated solvent in a mixer to convey to a flash evaporator.
摘要:
A process for the separation treatment of a polymer solution characterized by, in separating and recovering polymer and polymerization solvent by flashing a polymer solution, heating said polymer solution under an elevated pressure sufficient to maintain said solution in a liquid phase, sending said solution into a flashing tank kept at an inner surface temperature of 140.degree. C. or above and a pressure ranging from ordinary pressure to 5 kg/cm.sup.2 G, flashing said solution to evaporate and separate the solvent, thereby concentrating said solution so that concentration of the polymer in said solution becomes 80% by weight or more, and recovering the concentrated solution from the bottom part of the flashing tank.
摘要:
A process for preparing modified diene polymer rubbers having an increased impact resilience and a reduced hardness at low temperatures and useful as rubber materials for automobile tires and other industries which comprises producing an alkali metal-containing conjugated diene polymer, and reacting the alkali metal-containing polymer with a modifier selected from the group consisting of a nitroalkyl acrylate of the formula: ##STR1## wherein R.sup.1 and R.sup.2 are independently an alkyl group and n is an integer, and a nitroamino compound of the formula: ##STR2## wherein R.sup.3 to R.sup.6 are independently an alkyl group, and m is an integer, said alkali metal-containing diene polymer being prepared by a living anionic polymerization using an alkali metal-based catalyst or by an addition reaction of a diene polymer having conjugated diene units and an alkali metal-based catalyst in a hydrocarbon solvent. The modified diene polymers can be incorporated with usual rubber additives to provide rubber compositions for various purposes, and the cured products show an increased impact resilience and a reduced hardness at low temperatures.
摘要:
A modified copolymer rubber obtained by kneading at 200.degree.-280.degree. C.(A) at least one copolymer rubber material selected from the group consisting of an ethylene-.alpha.-olefin copolymer rubber having a number-average molecular weight of 10,000-100,000 and an ethylene content of 15-85% by weight and an ethylene-.alpha.-olefin-nonconjugated diene copolymer rubber having a number-average molecular weight of 10,000-100,000, an ethylene content of 15-85% by weight and a nonconjugated diene content of 3.0% by weight or less,(B) a free-radical initiator,(C) at least one vinyl aromatic monomer and(D) an unsaturated dicarboxylic anhydride, wherein the weight ratios of (B):(A), (C):(A), (D):(A) and (C):(D) are 0.005-1.0:100, 0.2-20:100, 0.5-15:100 and 0.1-3:1, respectively.The process is suited for industrially producing a modified copolymer rubber having a high bound unsaturated dicarboxylic anhydride content, a low tendency of increase of the Mooney viscosity [ML.sub.1+4 (121.degree. C.)], and an excellent moldability and storage stability without being obstructed by gel formation during the kneading. The modified copolymer rubber thus obtained can be advantageously used for thermoplastic elastomer, blending polymer adhesive etc.
摘要:
A process for preparing modified diene polymer rubbers having an increased impact resilience and a reduced hardness at low temperatures and useful as rubber materials for automobile tires and other industries which comprises producing an alkali metal-containing conjugated diene polymer, and reacting the alkali metal-containing polymer with a modifier selected from the group consisting of a nitro compound, a phosphoryl chloride compound of the formula: ##STR1## wherein R.sup.1 to R.sup.4 are independently an alkyl group, and an aminosilane compound of the formula: ##STR2## wherein R.sup.5 to R.sup.7 are independently an alkyl group or an alkoxyl group, R.sup.8 and R.sup.9 are independently an alkyl group, and n is an integer,said alkali metal-containing diene polymer being prepared by a living anionic polymerization using an alkali metal-based catalyst or by an addition reaction of a diene polymer having conjugated diene units and an alkali metal-based catalyst in a hydrocarbon solvent. The modified diene polymers can be incorporated with usual rubber additives to provide rubber compositions for various purposes, and the cured products show an increased impact resilience and a reduced hardness at low temperatures.