Abstract:
The present disclosure provides a modified starch composition. The modified starch composition includes starch with a terminal siloxane having 100 parts by weight, water having 30-70 parts by weight, and a polyol having 5-35 parts by weight. The present disclosure also provides a starch composite foam material and method for preparing the same.
Abstract:
In one embodiment, A flame-retardant thermoplastic starch material, including (A1) 100 parts by weight of starch; (A2) 5 to 75 parts by weight of plasticizer; and (A3) 5 to 30 parts by weight of organic phosphonate flame-retardant, wherein the organic phosphonate flame-retardant has the following formula (I): wherein X is a trivalent aliphatic hydrocarbon radical containing 3 to 12 carbon atoms; R1 and R2 are independently C1 to C8 alkyl; and n is 0 or 1.
Abstract:
Disclosed is a high thermally conductive composite, including a first composite and a second composite having a co-continuous and incompatible dual-phase manner. The first composite consists of glass fiber distributed in polyphenylene sulfide (PPS), acrylonitrile-butadiene-styrene copolymer (ABS), polybutylene terephthalate (PBT), poly(ε-caprolactam) (Nylon 6), polyhexamethylene adipamide (nylon 66), or polypropylene (PP). The second composite consists of carbon material distributed in polyethylene terephthalate.