Process for the preparation of elastomer/bitumen compositions and their
application as road surfacings
    2.
    发明授权
    Process for the preparation of elastomer/bitumen compositions and their application as road surfacings 失效
    制备弹性体/沥青组合物的方法及其作为道路表面处理的应用

    公开(公告)号:US5883162A

    公开(公告)日:1999-03-16

    申请号:US860153

    申请日:1997-08-20

    摘要: Functionalized elastomer/bitumen compositions with a broad plasticity range are produced by contacting a bitumen or bitumen mixture with an elastomer, a functionalizing agent and optionally a peroxide compound at 100.degree.-230.degree. C. under stirring conditions. The funtionalizing agent is a thiolcarboxylic acid having 3 or more carbon atoms, a thiolcarboxylic acid ester and specifically a disulphide having carboxylic groupings or carboxylic esters. The compositions may be used either directly or in diluted form to produce bitumous binders for making road surfacings, coated materials and sealing coatings.

    摘要翻译: PCT No.PCT / FR96 / 01614 Sec。 371日期1997年8月20日 102(e)日期1997年8月20日PCT提交1998年10月16日PCT公布。 出版物WO97 / 14754 日期1997年04月24日在搅拌条件下,通过使沥青或沥青混合物与弹性体,官能化剂和任选的过氧化物在100℃-230℃下接触来制备具有宽塑性范围的功能化弹性体/沥青组合物。 赋形剂是具有3个或更多个碳原子的硫醇羧酸,硫羟羧酸酯,特别是具有羧基或羧酸酯的二硫化物。 组合物可以直接或以稀释的形式使用以产生用于制造路面,涂层材料和密封涂层的沥青粘合剂。

    Process for the preparation of polymer/bitumen compositions and their
use in coatings
    3.
    发明授权
    Process for the preparation of polymer/bitumen compositions and their use in coatings 有权
    聚合物/沥青组合物的制备方法及其在涂料中的应用

    公开(公告)号:US6087420A

    公开(公告)日:2000-07-11

    申请号:US202750

    申请日:1998-12-18

    摘要: The invention provides a method for producing bitumen/polymer compositions which consists of contacting, between 100.degree. C. and 230.degree. C. and under agitation, a bitumen or a mixture of bitumens with at least one styrene and butadiene copolymer having a global butadiene content ranging between 50% and 95 wt. % and a content of butadiene 1,2 double-bond structural units ranging between 12% and 50 wt % of the copolymer, and, preferably, also a sulphuring coupling agent or a functionalizing agent. The bitumen/polymer compositions are usable, directly or after dilution, for forming bitumen/polymer binders for surfacing materials.

    摘要翻译: PCT No.PCT / FR98 / 00788 Sec。 371 1998年12月18日第 102(e)1998年12月18日日期PCT提交1998年4月17日PCT公布。 第WO98 / 47966号公报 日期1998年10月29日本发明提供了一种生产沥青/聚合物组合物的方法,其包括在100℃和230℃之间并在搅拌下使沥青或沥青与至少一种苯乙烯和丁二烯共聚物 全球丁二烯含量在50%至95%之间。 %,丁二烯1,2双键结构单元的含量在共聚物的12重量%〜50重量%之间,优选也为硫化偶联剂或官能化剂。 沥青/聚合物组合物可直接或在稀释后用于形成表面材料的沥青/聚合物粘合剂。

    Process for the preparation of bitumen-polymer composition
    4.
    发明授权
    Process for the preparation of bitumen-polymer composition 失效
    沥青聚合物组合物的制备方法

    公开(公告)号:US5508112A

    公开(公告)日:1996-04-16

    申请号:US505371

    申请日:1995-07-21

    IPC分类号: C08L95/00 C10C3/02 B32B11/00

    摘要: A process is provided for the preparation of bitumen-polymer compositions wherein bitumen is mixed at a composition between 100.degree. C. and 230.degree. C. with a block copolymer of styrene and a conjugated diene and a coupling agent containing a sulphur-donor compound for a duration of at least 10 minutes. The coupling agent is comprised of an elementary sulphur vulcanization agent and at least one sulphur-donor vulcanization accelerator from among morpholine disulphide, N,N'-disulphide of caprolactam and thiuram polysulphides.

    摘要翻译: 提供了一种制备沥青聚合物组合物的方法,其中沥青在100℃和230℃之间的组合物与苯乙烯和共轭二烯的嵌段共聚物和含有硫供体化合物的偶联剂混合, 持续时间至少10分钟。 偶联剂由硫代吗啉,己内酰胺的N,N'-二硫化物和秋兰姆多硫化物中的至少一种硫供体硫化促进剂组成。

    Bitumen/polymer compositions with improved stability and their
application in carrying out surfacing operations
    6.
    发明授权
    Bitumen/polymer compositions with improved stability and their application in carrying out surfacing operations 失效
    具有改进的稳定性的沥青/聚合物组合物及其在进行表面处理操作中的应用

    公开(公告)号:US6020404A

    公开(公告)日:2000-02-01

    申请号:US983300

    申请日:1998-01-07

    CPC分类号: C08L95/00

    摘要: Bitumen/polymer compositions are provided containing a bitumen or a mixture of bitumens and, reckoned by weight of bitumen, 0.3% to 20% of at least one primary polymer selected among certain elastomers and plastomers and 0.01% to 12% of at least one olefinic polymer bearing epoxy or COOH groupings. The compositions are useful, directly or after dilution, to form bitumen/polymer binders for carrying out road surfacing, for coated materials or waterproof coatings.

    摘要翻译: PCT No.PCT / FR97 / 00811 Sec。 371日期:1998年4月13日 102(e)日期1998年4月13日PCT提交1997年5月6日PCT公布。 公开号WO97 / 43341 日期1997年11月20日提供含有沥青或沥青混合物的沥青/聚合物组合物,以沥青重量计,0.3%至20%的至少一种选自某些弹性体和塑性体的主要聚合物和0.01%至12% 的至少一种含有环氧基或COOH基团的烯烃聚合物。 组合物可直接或经稀释后可用于形成沥青/聚合物粘合剂,用于进行道路铺面,涂层材料或防水涂料。

    Process for the preparation of bitumen-polymer compositions containing a
crosslinked elastomer and a functionalized olefinic polymer
    7.
    发明授权
    Process for the preparation of bitumen-polymer compositions containing a crosslinked elastomer and a functionalized olefinic polymer 失效
    制备含有交联弹性体和官能化烯烃聚合物的沥青聚合物组合物的方法

    公开(公告)号:US6011094A

    公开(公告)日:2000-01-04

    申请号:US669412

    申请日:1996-07-09

    IPC分类号: C08L95/00

    CPC分类号: C08L95/00

    摘要: Bitumen/polymer compositions having improved mechanical properties are produced by stirring together, at a temperature of 100-230.degree. C., a bitumen or bitumen mixture, a sulphur-curable elastomer and a polymeric additive consisting of at least one functionalized olefin copolymer and a sulphur-donating coupling agent. The bitumen/polymer compositions may be used directly or in dilute form to make bituminous binders for road surfaces, coated materials and sealing coatings.

    摘要翻译: PCT No.PCT / FR95 / 01471 Sec。 371日期:1996年7月9日 102(e)日期1996年7月9日PCT 1995年11月8日PCT PCT。 WO96 / 15193 PCT出版物 日期1996年5月23日具有改善的机械性能的勃赖斯/聚合物组合物是通过在100-230℃的温度下一起搅拌沥青或沥青混合物,硫可固化的弹性体和由至少一种官能化的 烯烃共聚物和供硫偶联剂。 沥青/聚合物组合物可以直接或以稀释形式使用,以制造用于路面,涂覆材料和密封涂料的沥青粘合剂。

    Method for preparing bitumen/polymer compositions and use thereof
    8.
    发明授权
    Method for preparing bitumen/polymer compositions and use thereof 失效
    制备沥青/聚合物组合物的方法及其用途

    公开(公告)号:US6011095A

    公开(公告)日:2000-01-04

    申请号:US981330

    申请日:1998-04-20

    摘要: Bitumen/polymer compositions are produced by contacting, between 100.degree. C. and 230.degree. C., under agitation, one bitumen or a mixture of bitumens with at least one olefinic polymer bearing epoxy or COOH groupings, then by incorporating in the product, an acid additive while the whole mixture is agitated at a range between 100.degree. C. and 230.degree. C. for at least 10 minutes. The product, which is subjected to treatment by the acid additive may still contain one or several additional polymers, for instance of the elastomer type cross-linkable with sulphur, and even be subjected to sulphur cross-linking before treatment. The bitumen/polymer compositions are useful directly or after dilution, to form binders for carrying out surfacing operations.

    摘要翻译: PCT No.PCT / FR97 / 00812 Sec。 371日期:1998年4月20日 102(e)1998年4月20日PCT PCT 1997年5月6日提交PCT公布。 公开号WO97 / 43342 PCT 日期1997年11月20日通过在100℃和230℃之间,在搅拌下,一个沥青或沥青与至少一种含有环氧或COOH基团的烯烃聚合物的混合物进行接触来制备基质/聚合物组合物, 在该产品中加入酸性添加剂,同时将整个混合物在100℃至230℃的范围内搅拌至少10分钟。 通过酸添加剂进行处理的产品可能还含有一种或多种另外的聚合物,例如可与硫交联的弹性体,甚至在处理前经受硫交联。 沥青/聚合物组合物可直接或稀释后使用,以形成用于进行表面处理操作的粘合剂。

    Method for preparing reinforced multigrade bitumen/polymer and use of
the resulting compositions for producing bitumen/polymer binders for
surface coatings
    9.
    发明授权
    Method for preparing reinforced multigrade bitumen/polymer and use of the resulting compositions for producing bitumen/polymer binders for surface coatings 失效
    用于制备增强多级沥青/聚合物的方法以及所得组合物用于生产用于表面涂层的沥青/聚合物粘合剂

    公开(公告)号:US5880185A

    公开(公告)日:1999-03-09

    申请号:US849865

    申请日:1997-08-22

    摘要: Bitumen/polymer compositions with a broadened plasticity range are produced by contacting a bitumen or bitumen mixture with a sulphur-cross-linkable elastomer and a sulphur-donating coupling agent, at 100.degree.-230.degree. C. and under stirring conditions, to produce a cross-linked bitumen/polymer composition, then adding to the composition, maintained at 100.degree.-232.degree. C. and under stirring conditions, an acidic additive selected from polyphosphoric acids, acids of formula R--(COO).sub.t --SO.sub.3 H wherein t=0 or 1 and R is a monovalent hydrocarbyl radical having up to 12 carbon atoms, and mixtures of both types of acid separately or jointly with sulphuric acid, and maintaining the resulting reaction medium at 100.degree.-230.degree. C. and under stirring conditions for at least ten minutes. The bitumen/polymer compositions may be used directly or in diluted form to produce bituminous binders for making road surfaces, coated materials or sealing coatings.

    摘要翻译: PCT No.PCT / FR96 / 01605 Sec。 371日期1997年8月22日 102(e)1997年8月22日PCT PCT 1996年10月15日PCT公布。 公开号WO97 / 14753 日期1997年04月24日具有扩大塑性范围的膨胀/聚合物组合物是通过在100-230℃和搅拌下使沥青或沥青混合物与硫可交联的弹性体和供硫偶联剂接触 条件下,制备交联沥青/聚合物组合物,然后向组合物中加入保持在100-232℃,在搅拌条件下,选自多磷酸,式R-(COO)t的酸的酸性添加剂 -SO 3 H,其中t = 0或1,R是具有至多12个碳原子的一价烃基,以及两种酸与硫酸分开或联合的混合物,并将所得反应介质保持在100-230℃。 并在搅拌条件下至少十分钟。 沥青/聚合物组合物可以直接或以稀释的形式使用,以生产用于制造路面,涂覆材料或密封涂料的沥青粘合剂。