摘要:
A method of preparing a catalyst for producing acrolein by oxidation of propylene at high space velocity, said catalyst is a Mo—Bi—Fe—Co based composite metal oxide. Producing unsaturated aldehyde via partial oxidation of lower unsaturated olefin at high space velocity using said catalyst is suitable for process with or without off-gas recirculating. Said catalyst is prepared by co-precipitation, the reaction conditions for using said catalyst to produce unsaturated aldehyde are, the space velocity of unsaturated lower olefin relative to catalyst being 120˜200 h-1(STP), reaction temperature being 300˜420° C. and absolute pressure being 0.1˜0.5 MPa; a single-stage unsaturated lower olefin conversion ratio of greater than 98.0% and carbon oxide yield of less than 3.3% with an overall yield of unsaturated lower aldehyde and acid of greater than 94.0% are obtained. The process to prepare the said catalyst is simple, easy to be repeated, and capable of industrial scale-up.
摘要:
A method of preparing a catalyst for producing acrolein by oxidation of propylene at high space velocity, said catalyst is a Mo—Bi—Fe—Co based composite metal oxide. Producing unsaturated aldehyde via partial oxidation of lower unsaturated olefin at high space velocity using said catalyst is suitable for process with or without off-gas recirculating. Said catalyst is prepared by co-precipitation, the reaction conditions for using said catalyst to produce unsaturated aldehyde are, the space velocity of unsaturated lower olefin relative to catalyst being 120˜200 h-1(STP), reaction temperature being 300˜420° C. and absolute pressure being 0.1˜0.5 MPa; a single-stage unsaturated lower olefin conversion ratio of greater than 98.0% and carbon oxide yield of less than 3.3% with an overall yield of unsaturated lower aldehyde and acid of greater than 94.0% are obtained. The process to prepare the said catalyst is simple, easy to be repeated, and capable of industrial scale-up.
摘要:
The present invention provides a complex oxide catalyst whose general formula is Mo12VaCubWcXdYeOf/Z. reducing agent needs to be added into the catalyst during the preparation process of the active component of the catalyst and (or) molding process of the catalyst. Specifically, X is at least one selected from a group consisting of Nb, Sb, Sr, Ba and Te; Y is at least one selected from a group consisting of La, Ce, Nd, Sm and Cs; “a” is ranging from 2 to 8; “b” is ranging from 1 to 6; “c” is ranging from 0.5 to 5; “d” is ranging from 0.01 to 4; “e” is ranging from 0.01 to 4; f is determined by the oxidation state of the component element; Z is silicon powder; the reducing agent is C2˜C6 diol or polyol.
摘要:
The present invention provides a complex oxide catalyst whose general formula is Mo12VaCubWcXdYeOf/Z. reducing agent needs to be added into the catalyst during the preparation process of the active component of the catalyst and (or) molding process of the catalyst. Specifically, X is at least one selected from a group consisting of Nb, Sb, Sr, Ba and Te; Y is at least one selected from a group consisting of La, Ce, Nd, Sm and Cs; “a” is ranging from 2 to 8; “b” is ranging from 1 to 6; “c” is ranging from 0.5 to 5; “d” is ranging from 0.01 to 4; “e” is ranging from 0.01 to 4; f is determined by the oxidation state of the component element; Z is silicon powder; the reducing agent is C2˜C6 diol or polyol.
摘要:
The present invention provides a preparation process of complex oxides catalyst containing Mo, Bi, Fe and Co, which comprising steps as following: dissolving precursor compounds of the components for catalyst and complexing agent in water to obtain a solution, and then drying, molding and calcining the solution to obtain catalyst. The catalyst is used for gas phase oxidation of light alkenes to unsaturated aldehydes. The catalyst has high activity, selectivity and stability. The reaction condition is mild. The preparation process of the catalyst is easy to operate and can be used for mass production.
摘要:
The present invention provides a preparation process of complex oxides catalyst containing Mo, Bi, Fe and Co, which comprising steps as following: dissolving precursor compounds of the components for catalyst and complexing agent in water to obtain a solution, and then drying, molding and calcining the solution to obtain catalyst. The catalyst is used for gas phase oxidation of light alkenes to unsaturated aldehydes. The catalyst has high activity, selectivity and stability. The reaction condition is mild. The preparation process of the catalyst is easy to operate and can be used for mass production.
摘要:
A method of methacrylate production includes the steps of providing methacrylate gas mixture; absorbing said gas mixture by water to form a solution mixture; introducing said solution mixture into a distillation column, separating impure methacrylate from said solution mixture in said distillation column that solution of said impure methacrylate is collected at said stripping section of said distillation column; and removing acetic acid from said impure methacrylate to produce methacrylate. It effectively enhances the separation capacity of the distillation column, lowers the whole column pressure drop and operation temperature, avoids the polymerization tendency of the methacrylate under high temperature, to make the water content of the bottom discharging decreases to 0.6%, acetic acid content reduces to below 2%, methyl acrylic content of the top column water phase decreases to 0.5%, thereby reduces the methacrylate products unit consumption and improves the product quality.