摘要:
There is provided a modified conjugated diene-based polymer having a silyl group substituted with one or more alkoxy groups, and one or more nitrogen atoms on the chain ends of a conjugated diene-based polymer, the modified conjugated diene-based polymer being obtained by polymerizing a conjugated diene compound, or copolymerizing a conjugated diene compound with an aromatic vinyl compound, by using a polyfunctional anionic polymerization initiator prepared from a polyvinyl aromatic compound and an organolithium compound in a range of a molar ratio (the polyvinyl aromatic compound/the organolithium compound) of from 0.05 to 1.0, so as to obtain the conjugated diene-based polymer, and by reacting a living polymer end of the conjugated diene polymer with the compound having a silyl group substituted with two or more alkoxy groups, and one or more nitrogen atoms.
摘要:
There is provided a modified conjugated diene-based polymer having a silyl group substituted with one or more alkoxy groups, and one or more nitrogen atoms on the chain ends of a conjugated diene-based polymer, the modified conjugated diene-based polymer being obtained by polymerizing a conjugated diene compound, or copolymerizing a conjugated diene compound with an aromatic vinyl compound, by using a polyfunctional anionic polymerization initiator prepared from a polyvinyl aromatic compound and an organolithium compound in a range of a molar ratio (the polyvinyl aromatic compound/the organolithium compound) of from 0.05 to 1.0, so as to obtain the conjugated diene-based polymer, and by reacting a living polymer end of the conjugated diene polymer with the compound having a silyl group substituted with two or more alkoxy groups, and one or more nitrogen atoms.
摘要:
There are provided a modified conjugated diene-based polymer having a good balance between the hysteresis loss properties and the wet skid resistance, practically sufficient abrasion resistance and fracture strength, and high processability when formed into a vulcanized product, and a modified conjugated diene-based polymer composition. A method for producing a modified conjugated diene-based polymer, comprising: a polymerization step of polymerizing a conjugated diene compound or copolymerizing a conjugated diene compound with an aromatic vinyl compound using an alkali metal compound or an alkaline earth metal compound as a polymerization initiator to obtain a conjugated diene-based polymer having a reactive end, and a modifying step of reacting a compound having a specific structure with the reactive end of the conjugated diene-based polymer.
摘要:
A method for producing a modified conjugated diene-based polymer having a good balance between the hysteresis loss properties and the wet skid resistance, practically sufficient abrasion resistance and breaking strength, and high processability when formed into a vulcanized product is provided. A method for producing a modified conjugated diene-based polymer, comprising: a polymerization step of polymerizing a conjugated diene compound, copolymerizing conjugated diene compounds, or copolymerizing a conjugated diene compound with an aromatic vinyl compound using an alkali metal compound or an alkaline earth metal compound as a polymerization initiator to obtain a conjugated diene-based polymer having an active end, and a modifying step of reacting a compound represented by following formula (1) with the active end of the conjugated diene-based copolymer.
摘要:
There are provided a modified conjugated diene-based polymer having a good balance between the hysteresis loss properties and the wet skid resistance, practically sufficient abrasion resistance and fracture strength, and high processability when formed into a vulcanized product, and a modified conjugated diene-based polymer composition. A method for producing a modified conjugated diene-based polymer, comprising: a polymerization step of polymerizing a conjugated diene compound or copolymerizing a conjugated diene compound with an aromatic vinyl compound using an alkali metal compound or an alkaline earth metal compound as a polymerization initiator to obtain a conjugated diene-based polymer having a reactive end, and a modifying step of reacting a compound having a specific structure with the reactive end of the conjugated diene-based polymer.
摘要:
A method for producing a modified conjugated diene-based polymer having a good balance between the hysteresis loss properties and the wet skid resistance, practically sufficient abrasion resistance and breaking strength, and high processability when formed into a vulcanized product is provided. A method for producing a modified conjugated diene-based polymer, comprising: a polymerization step of polymerizing a conjugated diene compound, copolymerizing conjugated diene compounds, or copolymerizing a conjugated diene compound with an aromatic vinyl compound using an alkali metal compound or an alkaline earth metal compound as a polymerization initiator to obtain a conjugated diene-based polymer having an active end, and a modifying step of reacting a compound represented by following formula (1) with the active end of the conjugated diene-based copolymer.
摘要:
A hydrogenated block copolymer which comprises at least two polymer blocks A each mainly comprising an aromatic vinyl hydrocarbon compound monomer unit and at least two hydrogenated polymer blocks B each mainly comprising a butadiene monomer unit, at least 90% of the olefinically unsaturated double bonds in said polymer block mainly comprising a butadiene monomer unit before hydrogenation having been hydrogenated, wherein at least one of the block at the terminal of the hydrogenated block copolymer is the polymer block B, wherein the proportion of the terminal polymer blocks B in the hydrogenated block copolymer is at least 0.1 wt % but less than 9.1 wt %, wherein the proportion of the aromatic vinyl hydrocarbon compound in the hydrogenated block copolymer exceeds 10 wt % but less than 25 wt %, wherein the 1,2-bond content of the polymer blocks mainly comprising a butadiene monomer unit before hydrogenation is, on average, at least 62 mole % but less than 99 mol %, and wherein the difference &Dgr;Tc (Tc1−Tc2) between the crystallization initiating temperature (Tc1) of the isotactic homopolypropylene and the crystallization initiating temperature (Tc2) of a mixture thereof with the hydrogenated block copolymer is at least 1.5° C.