Method and system for processing oil and gas well cuttings utilizing existing slurry processing equipment
    1.
    发明申请
    Method and system for processing oil and gas well cuttings utilizing existing slurry processing equipment 有权
    利用现有浆料加工设备加工油气井的方法和系统

    公开(公告)号:US20070051539A1

    公开(公告)日:2007-03-08

    申请号:US11222272

    申请日:2005-09-08

    IPC分类号: E21B21/06

    CPC分类号: E21B41/0057 E21B21/066

    摘要: A method for integrating a batch cement process with a cuttings reinjection process, the method comprising: equipping a batch cement skid with a particle classifier and a grinding pump, such that the batch cement skid sequentially implements the cuttings reinjection process and the batch cement process is disclosed. An apparatus for performing a batch cement process and a cuttings reinjection process, the apparatus comprising: a first tank and a second tank, a particle classifier having a coarse effluent stream feeding into the first tank and a fine effluent stream feeding into the second tank, and a grinding pump in fluid communication with the first tank and the particle classifier is also disclosed.

    摘要翻译: 一种用于将批量水泥工艺与切屑再注入工艺相结合的方法,所述方法包括:将批料水泥滑块装备有颗粒分级机和研磨泵,使得批量水泥滑移顺序地实施切屑回注工艺,并且分批水泥工艺是 披露 一种用于执行分批水泥工艺和切屑再注入工艺的装置,所述装置包括:第一罐和第二罐,具有进入第一罐的粗流出物流和进入第二罐的精细流出物流的颗粒分级器, 并且还公开了与第一罐和颗粒分级器流体连通的研磨泵。

    METHOD FOR COATING SPARK PLUG THREADS WITH A POLYTETRAFLUOROETHYLENE MIXTURE
    2.
    发明申请
    METHOD FOR COATING SPARK PLUG THREADS WITH A POLYTETRAFLUOROETHYLENE MIXTURE 审中-公开
    用聚四氟乙烯混合物涂抹火花塞螺纹的方法

    公开(公告)号:US20140220234A1

    公开(公告)日:2014-08-07

    申请号:US13946297

    申请日:2013-07-19

    申请人: Kevin Stewart

    发明人: Kevin Stewart

    IPC分类号: H01T21/02

    摘要: The invention relates to a method for coating spark plug threads with a polytetrafluoroethylene mixture comprising the steps of (a) bringing the spark plug to room temperature of 21° C. to 26° C. (70° F. to 79° F.); (b) mixing the polytetrafluoroethylene mixture thoroughly and filtering the material through a 100-mesh stainless steel screen (0.146 mm openings); (c) applying a minimum dry film thickness of 20 microns to 30 microns (0.8 mil to 1.2 mil) to the spark plug thread; and (d) baking the spark plug for 15 minutes at a metal temperature of 232° C. to 260° C. (450° F. to 500° F.).

    摘要翻译: 本发明涉及一种用聚四氟乙烯混合物涂覆火花塞螺纹的方法,包括以下步骤:(a)使火花塞的室温为21°C至26°C(70°F至79°F) ; (b)彻底混合聚四氟乙烯混合物,并通过100目不锈钢筛网(0.146毫米开口)过滤材料; (c)向火花塞螺纹施加20微米至30微米(0.8密耳至1.2密耳)的最小干膜厚度; 和(d)在金属温度为232℃至260℃(450°F至500°F)下烘烤火花塞15分钟。

    Method for coating spark plug threads with a polytetrafluoroethylene mixutre
    3.
    发明授权
    Method for coating spark plug threads with a polytetrafluoroethylene mixutre 有权
    用聚四氟乙烯混合物涂覆火花塞螺纹的方法

    公开(公告)号:US09231384B2

    公开(公告)日:2016-01-05

    申请号:US13946297

    申请日:2013-07-19

    申请人: Kevin Stewart

    发明人: Kevin Stewart

    摘要: The invention relates to a method for coating spark plug threads with a polytetrafluoroethylene mixture comprising the steps of (a) bringing the spark plug to room temperature of 21° C. to 26° C. (70° F. to 79° F.); (b) mixing the polytetrafluoroethylene mixture thoroughly and filtering the material through a 100-mesh stainless steel screen (0.146 mm openings); (c) applying a minimum dry film thickness of 20 microns to 30 microns (0.8 mil to 1.2 mil) to the spark plug thread; and (d) baking the spark plug for 15 minutes at a metal temperature of 232° C. to 260° C. (450° F. to 500° F.).

    摘要翻译: 本发明涉及一种用聚四氟乙烯混合物涂覆火花塞螺纹的方法,包括以下步骤:(a)使火花塞的室温为21°C至26°C(70°F至79°F) ; (b)彻底混合聚四氟乙烯混合物,并通过100目不锈钢筛网(0.146毫米开口)过滤材料; (c)向火花塞螺纹施加20微米至30微米(0.8密耳至1.2密耳)的最小干膜厚度; 和(d)在金属温度为232℃至260℃(450°F至500°F)下烘烤火花塞15分钟。

    APPARATUS AND METHOD FOR SHARING A CACHED SECURITY PROFILE IN A DATABASE ENVIRONMENT
    5.
    发明申请
    APPARATUS AND METHOD FOR SHARING A CACHED SECURITY PROFILE IN A DATABASE ENVIRONMENT 失效
    在数据库环境中共享缓存安全配置文件的方法和方法

    公开(公告)号:US20070288695A1

    公开(公告)日:2007-12-13

    申请号:US11843800

    申请日:2007-08-23

    IPC分类号: G06F12/14

    摘要: An apparatus, system, and method are provided for sharing a cached security profile in a database environment. The apparatus, system, and method include a cache module for caching a security profile accessible to primary tasks and secondary tasks. An identification module is provided that distinguishes between primary tasks authorized to refresh the security profile and secondary tasks. A refresh module cooperates with the cache module and identification module to selectively refresh the security profile in response to a refresh request and expiration of the security profile such that an old version of the security profile is retained for use by secondary tasks until an execution window closes.

    摘要翻译: 提供了一种用于在数据库环境中共享缓存的安全配置文件的装置,系统和方法。 装置,系统和方法包括用于缓存主要任务和次要任务可访问的安全简档的高速缓存模块。 提供了识别模块,区分被授权刷新安全配置文件和辅助任务的主要任务。 刷新模块与高速缓存模块和识别模块协作以响应于刷新请求和安全性配置文件的到期来选择性地刷新安全性配置文件,使得旧版本的安全配置文件被保留以供辅助任务使用,直到执行窗口关闭 。

    POLYMERIZABLE PHOTOCHROMIC COMPOSITIONS WITH MULTIPLE INITIATORS
    6.
    发明申请
    POLYMERIZABLE PHOTOCHROMIC COMPOSITIONS WITH MULTIPLE INITIATORS 审中-公开
    具有多个发射体的可聚合的光致变色组合物

    公开(公告)号:US20070257238A1

    公开(公告)日:2007-11-08

    申请号:US11696895

    申请日:2007-04-05

    IPC分类号: G02B1/04

    CPC分类号: C08F4/38 C09K9/02 C09K2211/14

    摘要: Provided is a method of preparing a photochromic polymeric article including: (a) providing a fluid polymerizable composition of: at least one monomer; a first initiator for inducing polymerization of the monomer at a first temperature; and a second initiator for inducing further polymerization at a second temperature higher than the first temperature; (b) heating the polymerizable composition to at least the first temperature whereby the first initiator induces polymerization of the monomer at the first temperature to produce a polymerizate; (c) heating the polymerizate of (b) to at least the second temperature to further polymerize the polymerizate; and (d) contacting the polymerizate with an organic photochromic substance to incorporate the organic photochromic substance into the polymerizate. Photochromic articles prepared by the method are also provided.

    摘要翻译: 提供一种制备光致变色聚合物制品的方法,包括:(a)提供一种流体可聚合组合物:至少一种单体; 在第一温度下引发单体聚合的第一引发剂; 和在高于第一温度的第二温度下诱导进一步聚合的第二引发剂; (b)将可聚合组合物加热到至少第一温度,由此第一引发剂在第一温度下引发单体的聚合以产生聚合物; (c)将(b)的聚合物加热至至少第二温度以进一步聚合聚合物; 和(d)使聚合物与有机光致变色物质接触,以将有机光致变色物质并入聚合物中。 还提供了通过该方法制备的光致变色制品。

    Photochromic coating compositions, methods of making coated articles and articles thereof
    7.
    发明申请
    Photochromic coating compositions, methods of making coated articles and articles thereof 审中-公开
    光致变色涂料组合物,制造涂布制品的方法及其制品

    公开(公告)号:US20060093844A1

    公开(公告)日:2006-05-04

    申请号:US11231867

    申请日:2005-09-22

    IPC分类号: B32B27/30 B05D5/06 G02B5/00

    摘要: Described are ungelled coating compositions of photochromic material, precursor materials for a first polymer polymerizable by free-radical initiated polymerization and precursor materials for a second or additional polymer(s) different from the first polymer. When the second polymer is selected from polyurethane, poly(urea-urethane) and mixtures thereof, the precursor materials include at least one blocked polyisocyanate. Also described are methods of making photochromic articles using the ungelled coating compositions and the photochromic articles produced using these methods.

    摘要翻译: 描述了光致变色材料的未凝胶化涂料组合物,用于通过自由基引发聚合可聚合的第一聚合物的前体材料和用于不同于第一聚合物的第二或另外的聚合物的前体材料。 当第二聚合物选自聚氨酯,聚(脲 - 氨基甲酸酯)及其混合物时,前体材料包括至少一种封端多异氰酸酯。 还描述了使用未凝胶化涂料组合物制备光致变色制品的方法和使用这些方法制备的光致变色制品。

    Retaining mechanisms for prosthetic valves
    8.
    发明授权
    Retaining mechanisms for prosthetic valves 有权
    人工瓣膜固定机构

    公开(公告)号:US09326853B2

    公开(公告)日:2016-05-03

    申请号:US13188988

    申请日:2011-07-22

    IPC分类号: A61F2/24

    摘要: Disclosed herein are representative embodiments of methods, apparatus, and systems used to deliver a prosthetic heart valve to a deficient valve. In one embodiment, for instance, a support structure and an expandable prosthetic valve are advanced through the aortic arch of a patient using a delivery system. The support structure is delivered to a position on or adjacent to the surface of the outflow side of the aortic valve (the support structure defining a support-structure interior). The expandable prosthetic valve is delivered into the aortic valve and into the support-structure interior. The expandable prosthetic heart valve is expanded while the expandable prosthetic heart valve is in the support-structure interior and while the support structure is at the position on or adjacent to the surface of the outflow side of the aortic valve, thereby causing one or more native leaflets of the aortic valve to be frictionally secured between the support structure and the expanded prosthetic heart valve.

    摘要翻译: 这里公开了用于将假性心脏瓣膜递送到缺陷阀的方法,装置和系统的代表性实施例。 在一个实施例中,例如,支撑结构和可扩张的假体瓣膜通过使用递送系统的患者的主动脉弓前进。 支撑结构被传送到主动脉瓣(支撑结构限定支撑结构内部)的流出侧的表面上或邻近的位置。 可膨胀假体瓣膜被输送到主动脉瓣并进入支撑结构内部。 可扩张假体心脏瓣膜膨胀,而可扩张假体心脏瓣膜处于支撑结构内部,而支撑结构处于主动脉瓣的流出侧表面上或邻近主动脉瓣的流出侧的位置,从而导致一个或多个本机 主动脉瓣的小叶被摩擦地固定在支撑结构和扩张的假体心脏瓣膜之间。

    Optical elements that include curable film-forming compositions containing blocked isocyanate adhesion promoters
    9.
    发明申请
    Optical elements that include curable film-forming compositions containing blocked isocyanate adhesion promoters 有权
    包括含有封端异氰酸酯粘合促进剂的可固化成膜组合物的光学元件

    公开(公告)号:US20070054131A1

    公开(公告)日:2007-03-08

    申请号:US11221188

    申请日:2005-09-07

    申请人: Kevin Stewart

    发明人: Kevin Stewart

    IPC分类号: B32B27/40

    摘要: Described are optical elements made of a substrate and a curable film-forming composition applied to at least a portion of the substrate to form a coating thereon. The curable film-forming composition comprises: i) a resinous material comprising a monomer, oligomer, and/or polymer containing reactive functional groups; ii) a curing agent having two or more reactive functional groups that are reactive with functional groups in the resinous material of i); and iii) a material different from i) and ii), comprising a blocked isocyanate group blocked with a blocking agent capable of deblocking at a low temperature. The material of iii) is present in the curable film-forming composition at least in an amount sufficient to improve adhesion between the curable film-forming composition and the substrate and/or a superposed coating compared to a substantially identical optical element that does not comprise the material of iii) in the curable film-forming composition.

    摘要翻译: 描述了由基材和可固化成膜组合物制成的光学元件,其施加到基材的至少一部分以在其上形成涂层。 可固化成膜组合物包括:i)包含含有反应性官能团的单体,低聚物和/或聚合物的树脂材料; ii)具有与i)的树脂材料中的官能团反应的具有两个或多个反应性官能团的固化剂; 和iii)不同于i)和ii)的材料,其包含用能够在低温下解封的封闭剂封闭的封端异氰酸酯基团。 在可固化成膜组合物中存在至少足以提高可固化成膜组合物与基材和/或重叠涂层之间的粘合力的量的iii)的材料与基本相同的不包含 可固化成膜组合物中的iii)的材料。

    Photochromic materials
    10.
    发明申请
    Photochromic materials 有权
    光致变色材料

    公开(公告)号:US20060022176A1

    公开(公告)日:2006-02-02

    申请号:US10903770

    申请日:2004-07-30

    IPC分类号: G02F1/00 G02F1/01

    CPC分类号: C07D311/78 C07D311/92

    摘要: Various non-limiting embodiments disclosed herein related to photochromic materials comprising the reaction product of (a) at least one ring-opening cyclic monomer, and (b) a photochromic initiator. Other non-limiting embodiments related to photochromic materials represented by: wherein S′ comprises the at least one ring-opened cyclic monomer as set forth herein. Other non-limiting embodiments related to photochromic compositions, optical elements, and methods of inhibiting migration of a photochromic material in a polymeric material using the photochromic materials disclosed herein. Methods of making such photochromic materials, compositions, and optical elements are also disclosed.

    摘要翻译: 本文公开的各种非限制性实施方案涉及包含(a)至少一个开环环状单体和(b)光致变色引发剂的反应产物的光致变色材料。 与由下式表示的光致变色材料相关的其它非限制性实施方案:其中S'包含如本文所述的至少一种开环环状单体。 与光致变色组合物有关的其它非限制性实施方案,光学元件以及使用本文公开的光致变色材料抑制光致变色材料在聚合物材料中迁移的方法。 还公开了制备这种光致变色材料,组合物和光学元件的方法。