摘要:
A shaped article, in particular a support for image information layers prepared from a biaxially stretched film prepared from a polymer blend of 50 to 97 wt.% of a linear polyester and 3 to 50 wt.% of a polymer containing styrene, wherein the percentages relate to the sum of polyester and polymer containing styrene, is characterised by particularly-elevated covering power.
摘要:
Thermoplastic molding compositions containingA) ABS-type resin,B) aromatic polycarbonate resins,C) a compound bearing several carboxyl groups or mixtures thereof and optionallyD) further polymer resins,characterized in that an ABS resin with at least one basically acting additive is used as component A, component C is selected from compounds having a molecular weight of from 150 to 260 having at least two carboxyl groups (--COOH) in the molecule, and the weight ratio of basically acting additive in A: carboxyl groups in C is from 5:1 to 1:1.
摘要:
Molding compounds ofA) 5 to 95 parts by weight of a graft product of resin-forming monomers on a particulate silicone rubber having a total rubber content of from 30 to 90% by weight andB) 95 to 5 parts by weight of resin-forming monomers on a particulate EPDM rubber having a total rubber content of 10 to 50% by weight andC) 10 to 200 parts by weight (based on 100 parts by weight A+B) of a graft product of resin-forming monomers on a particulate acrylate rubber having a total rubber content of from 30 to 80% by weight.
摘要:
Thermoplastic moulding compounds containing(A) from 5 to 90 parts by weight of one or more thermoplastic polymers,(B) from 5 to 90 parts by weight of one or more graft polymers and(C) from 0.25 to 40 parts by weight of a copolymer having a sequential structure corresponding to the idealized formula (I)(A-X-B).sub.n (I)whereinA=a polymer of a cyclic carbonate,B=a polymer of another cyclic ester andX=a middle member containing both partial structures of A and B.
摘要:
Process for the preparation of thermoplastic copolymers of .alpha.-methylstyrene and acrylonitrile by continuous bulk copolymerization ofA. 30 to 50 mol % of .alpha.-methylstyrene andB. 70 to 50 mol % of acrylonitrileat temperatures from 60.degree. to 120.degree. C. with average residence times of 4 to 12 hours in the presence of initiators which supply free radicals, carried out in at least two continuously operated mixed tank reactors, characterized in that 100 molar parts of a monomer mixture ofA.sub.0. 34 to 52 mol % of .alpha.-methylstyrene andB.sub.0. 66 to 48 mol % of acrylonitrileare fed continuously into the first tank reactor per unit time, and, with back-mixing, are copolymerized up to a conversion of 5 to 30 molar parts to give a copolymer of the compositionA.sub.1. 49 to 53 mol % of .alpha.-methylstyrene andB.sub.1. 51 to 47 mol % of acrylonitrile,and the mixture consisting of 70 to 95 molar parts of the monomers A and B and 5 to 30 molar parts of the copolymer of the composition A.sub.1 -B.sub.1 is transferred continuously to the second tank reactor and is polymerized there up at a further conversion of 5 to 55 molar parts to a total conversion of 20 to 60 molar parts to give further copolymer of the compositionA.sub.1. 49 to 53 mol % of .alpha.-methylstyrene andB.sub.1. 51 to 47 mol % of acrylonitrile,0,5 to 11.5 molar parts of acrylonitrile being removed from the vapor condenser of the second tank reactor and recycled to the first tank reactor per unit time.
摘要:
A pigment preparation containing a pigment, a nonionic surface-active agent and, as a thermoplastic finishing agent, a copolymer which has an average molecular weight of 80,000 to 160,000 and consists of 90-50% by weight of .alpha.-methylstyrene and 10-50% by weight of acrylonitrile, and its use for the mass coloring of thermoplastic moulding compositions.
摘要:
Molding compounds of(A) 5 to 95% by weight of a graft product of a mixture of 50 to 100 parts by weight styrene, .alpha.-methyl styrene, vinyl toluene, methyl methacrylate or mixtures thereof and 0 to 50 parts by weight acrylonitrile on a particulate silicone rubber with a mean particle diameter (d.sub.50) of from 0.10 to 0.50 .mu.m having a total rubber content of from 30 to 90% by weight and(B) 95 to 5% by weight of a graft product of a mixture of 50 to 100 parts by weight styrene, .alpha.-methyl styrene, vinyl toluene, methyl methacrylate or mixtures thereof and 0 to 50 parts by weight acrylonitrile on a particulate acrylate rubber with a mean particle diameter (d.sub.50) of from 0.05 to 1.00 .mu.m having a total rubber content of 30 to 80% by weight.
摘要:
Elastic-thermoplastic or thermoplastic powder-form moulding compositions having uniform particles size and improved thermal stability and processes for their manufacture.
摘要:
Polycarboxylic acids and their salts corresponding to the following general formula[X]--(NHOC--Y--COO M).sub.n (I)in whichX is the residue of a hydrophobic, linear or branched vinyl oligomer having an average molecular weight M.sub.n of from 200 to 5000 and preferably from 300 to 3000,Y is the 1,2-vinylene, 1,2-ethylene, 1,3-propylene, 1,2-phenylene, 1,2-cyclohexen-4-ylene or 1,2-cyclohexylene group,n is a number of from 1.4 to 3.0 and preferably from 1.6 to 2.3 andM is hydrogen, an alkali metal, an ammonium, C.sub.1 -C.sub.4 alkylammonium or C.sub.2 -C.sub.3 hydroxyalkylammonium group, which are useful as surfactants and emulsifiers in aqueous systems.
摘要:
Process for the preparation of a thermoplastic moulding composition of 10 to 65% by weight of at least one graft polymer which is obtainable by emulsion polymerization of styrene and acrylonitrile in a weight ratio of 90:10 to 50:50, it being possible for all or some of the styrene to be replaced by .alpha.-methylstyrene or methyl methacrylate, in the presence of at least one rubber base, and the weight ratio of monomers employed to rubber polymer employed being 20:80 to 70:30, and 90 to 35% by weight of a copolymer of styrene and acrylonitrile in a weight ratio of 90:10 to 50:50, it being possible for all or some of the styrene to be replaced by .alpha.-methylstyrene or methyl methacrylate, wherein, to prepare the graft polymer, the grafting monomers and 0.05 to 1.00 part by weight (per 100 parts by weight of grafting monomer) of a mercaptan are added stepwise to the latex of the rubber base over a period of time, the part amount of the monomer added in each time interval .DELTA.t.sub.n+1 being 0.30 to 0.95 times the amount of monomer added in the preceding time interval .DELTA.t.sub.n at least in the first half of the period of time, and the total period of time comprising n time intervals where n=3 to 30, and each time interval .DELTA.t being 5 to 100 minutes long.