摘要:
Methods are disclosed for forming a varied impurity profile for a collector using scattered ions while simultaneously forming a subcollector. In one embodiment, the invention includes: providing a substrate; forming a mask layer on the substrate including a first opening having a first dimension; and substantially simultaneously forming through the first opening a first impurity region at a first depth in the substrate (subcollector) and a second impurity region at a second depth different than the first depth in the substrate. The breakdown voltage of a device can be controlled by the size of the first dimension, i.e., the distance of first opening to an active region of the device. Numerous different sized openings can be used to provide devices with different breakdown voltages using a single mask and single implant. A semiconductor device is also disclosed.
摘要:
The present invention provides a unique device structure and method that provides increased transistor performance in integrated bipolar circuit devices. The preferred embodiment of the present invention provides improved high speed performance by providing reduced base resistence. The preferred design forms the extrinsic base by diffusing dopants from a dopant source layer and into the extrinsic base region. This diffusion of dopants forms at least a portion of the extrinsic base. In particular, the portion adjacent to the intrinsic base region is formed by diffusion. This solution avoids the problems caused by traditional solutions that implanted the extrinsic base. Specifically, by forming at least a portion of the extrinsic base by diffusion, the problem of damage to base region is minimized. This reduced damage enhances dopant diffusion into the intrinsic base. Additionally, the formed extrinsic base can have improved resistence, resulting in an improved maximum frequency for the bipolar device. Additionally, the extrinsic base can be formed with a self-aligned manufacturing process that reduces fabrication complexity.
摘要:
The preferred embodiment of the present invention provides a buried layer that improves the latch up immunity of digital devices while providing isolation structures that provide noise isolation for both the digital and analog devices. The buried layer of the preferred embodiment is formed to reside within or below the subcollector region in the transistor. Additionally, in the preferred embodiment the subcollector is isolated from buried layer outside the transistor region by deep isolation trenches formed at the edges of the subcollector. Additionally, an array of deep isolation trenches provides increased isolation between devices where needed. Thus, the preferred embodiment of the present invention provides an integrated circuit structure and method that provides improved latchup immunity while also providing improved noise tolerance.
摘要:
Methods are disclosed for forming a varied impurity profile for a collector using scattered ions while simultaneously forming a subcollector. In one embodiment, the invention includes: providing a substrate; forming a mask layer on the substrate including a first opening having a first dimension; and substantially simultaneously forming through the first opening a first impurity region at a first depth in the substrate (subcollector) and a second impurity region at a second depth different than the first depth in the substrate. The breakdown voltage of a device can be controlled by the size of the first dimension, i.e., the distance of first opening to an active region of the device. Numerous different sized openings can be used to provide devices with different breakdown voltages using a single mask and single implant. A semiconductor device is also disclosed.
摘要:
Methods of manufacturing a semiconductor structure are disclosed including a deep trench isolation in which a channel stop is formed in the form of an embedded impurity region in the substrate prior to the deep trench etch and formation of transistor devices (FEOL processing) on the substrate. In this fashion, the FEOL processing thermal cycles can activate the impurity region. The deep trench isolations are then formed after FEOL processing. The method achieves the reduced cost of forming deep trench isolations after FEOL processing, and allows the practice of sharing of a collector level between devices to continue. The invention also includes the semiconductor structure so formed.
摘要:
Methods of manufacturing a semiconductor structure are disclosed including a deep trench isolation in which a channel stop is formed in the form of an embedded impurity region in the substrate prior to the deep trench etch and formation of transistor devices (FEOL processing) on the substrate. In this fashion, the FEOL processing thermal cycles can activate the impurity region. The deep trench isolations are then formed after FEOL processing. The method achieves the reduced cost of forming deep trench isolations after FEOL processing, and allows the practice of sharing of a collector level between devices to continue.
摘要:
The present invention provides a unique device structure and method that provides increased transistor performance in integrated bipolar circuit devices. The preferred embodiment of the present invention provides improved high speed performance by providing reduced base resistence. The preferred design forms the extrinsic base by diffusing dopants from a dopant source layer and into the extrinsic base region. This diffusion of dopants forms at least a portion of the extrinsic base. In particular, the portion adjacent to the intrinsic base region is formed by diffusion. This solution avoids the problems caused by traditional solutions that implanted the extrinsic base. Specifically, by forming at least a portion of the extrinsic base by diffusion, the problem of damage to base region is minimized. This reduced damage enhances dopant diffusion into the intrinsic base. Additionally, the formed extrinsic base can have improved resistence, resulting in an improved maximum frequency for the bipolar device. Additionally, the extrinsic base can be formed with a self-aligned manufacturing process that reduces fabrication complexity.
摘要:
A field effect transistor and method of fabricating the field effect transistor. The field effect transistor, including: a gate electrode formed on a top surface of a gate dielectric layer, the gate dielectric layer on a top surface of a single-crystal silicon channel region, the single-crystal silicon channel region on a top surface of a Ge including layer, the Ge including layer on a top surface of a single-crystal silicon substrate, the Ge including layer between a first dielectric layer and a second dielectric layer on the top surface of the single-crystal silicon substrate.
摘要:
A method and structure for a transistor that includes an insulator and a silicon structure on the insulator. The silicon structure includes a central portion and Fins extending from ends of the central portion. A first gate is positioned on a first side of the central portion of the silicon structure. A strain-producing layer could be between the first gate and the first side of the central portion of the silicon structure and a second gate is on a second side of the central portion of the silicon structure.
摘要:
A SiGe bipolar transistor containing substantially no dislocation defects present between the emitter and collector region and a method of forming the same are provided. The SiGe bipolar transistor includes a collector region of a first conductivity type; a SiGe base region formed on a portion of said collector region; and an emitter region of said first conductivity type formed over a portion of said base region, wherein said collector region and said base region include carbon continuously therein. The SiGe base region is further doped with boron.