    摘要: A ferritic heat-resistant steel, which exhibits excellent creep characteristics even at a high temperature exceeding 600° C., comprises, on the basis of percent by weight, 1.0 to 13% of chromium, 0.1 to 8.0% of cobalt, 0.01 to 0.20% of nitrogen, 3.0% or less of nickel, 0.01 to 0.50% of one or more of elements selected from a group consisting of vanadium, niobium, tantalum, titanium, hafnium, and zirconium that are MX type precipitate forming elements, and 0.01% or less of carbon and a balance being substantially iron and inevitable impurities, wherein the MX type precipitates precipitate on grain boundaries and in entire grains and the grain boundary existing ratio of an M23C6 type precipitate precipitating on the grain boundaries is 50% or less.

    摘要翻译: 即使在超过600℃的高温下也具有优异的蠕变特性的铁素体系耐热钢,以重量百分比计含有1.0〜13%的铬,0.1〜8.0%的钴,0.01〜0.20 的氮,3.0%以下的镍,0.01〜0.50%的选自钒系,铌,钽,钛,铪和锆的元素中的一种或多种元素,为MX型沉淀形成元素,0.01% 或更少的碳和余量基本上是铁和不可避免的杂质,其中MX型沉淀物在晶界和整个晶粒中沉淀,并且M 23 C 6的晶界存在比例 在晶界析出的/ SUB型析出物的浓度为50%以下。

    High Temperature Bolt Material
    2.
    发明申请
    High Temperature Bolt Material 审中-公开
    高温螺栓材料

    公开(公告)号:US20080216927A1

    公开(公告)日:2008-09-11

    申请号:US10569485

    申请日:2004-08-27

    IPC分类号: C21D1/78 C22C38/30 C22C38/22

    摘要: A high temperature bolt material, characterized in that it is a ferrite steel comprising 8 wt % or more of Cr and having a tempered martensite structure and can be used in a high temperature region of higher than 500° C.; and a method for producing the high temperature bolt material which comprises subjecting the above-mentioned steel material to a heat treatment comprising a quenching or normalizing at a temperature of 1000° C. or higher and then to a tempering at a temperature of 730° C. or higher. The above ferrite steel high temperature bolt material is excellent in characteristics of the resistance to stress relaxation.

    摘要翻译: 一种高温螺栓材料,其特征在于,其为含有8重量%以上的Cr且具有回火马氏体组织的铁素体钢,可用于高于500℃的高温区域。 以及一种生产高温螺栓材料的方法,该方法包括对上述钢材进行包括在1000℃或更高的温度下骤冷或归一化的热处理,然后在730℃的温度下回火 。 或更高。 上述铁素体高温螺栓材料具有优异的耐应力松弛特性。

    Method for the preparation of an alcohol from hydrocarbon
    3.
    发明授权
    Method for the preparation of an alcohol from hydrocarbon 失效
    从烃制备醇的方法

    公开(公告)号:US5104504A

    公开(公告)日:1992-04-14

    申请号:US588095

    申请日:1990-09-21

    CPC分类号: C07C29/36 Y02P20/52

    摘要: A efficient photochemical method for the preparation of an alcohol compound, e.g., benzyl alcohol, from a non-olefin hydrocarbon compound, e.g., benzene, was proposed in which a mixture of the non-olefin hydrocarbon compound as the starting material and a hydrogen donor compound, which is a cycloalkane of 5 to 16 carbon atoms in a molecule, e.g., cyclooctane, or an aliphatic alcohol of up to 10 carbon atoms in a molecule, e.g., isopropyl alcohol, is irradiated with light under an atmosphere of carbon monoxide in the presence of a complex compound of rhodium or iridium, of which at least one of the ligands is preferably a monophosphine or bisphosphine compound. The method is advantageous in that the reaction can proceed under mild reaction conditions and that the amount of the aldehyde compound formed in the reaction mixture as a by-product is very small as compared with conventional methods so as to greatly facilitate isolation of the desired alcohol product from the reaction mixture.

    摘要翻译: 提出了一种用于制备来自非烯烃烃化合物例如苯的醇化合物(例如苄醇)的有效光化学方法,其中以非烯烃烃化合物作为原料的混合物和氢供体 化合物,其是分子中具有5至16个碳原子的环烷烃,例如环辛烷或分子中具有至多10个碳原子的脂族醇,例如异丙醇,在一氧化碳气氛下用光照射 存在铑或铱的复合化合物,其中至少一种配体优选为单膦或双膦化合物。 该方法的优点在于反应可以在温和的反应条件下进行,并且与常规方法相比,作为副产物的反应混合物中形成的醛化合物的量非常小,以便极大地促进所需醇的分离 反应混合物中的产物。

    Thermal storage and transport
    5.
    发明授权
    Thermal storage and transport 失效
    热存储和运输

    公开(公告)号:US06936791B1

    公开(公告)日:2005-08-30

    申请号:US09526026

    申请日:2000-03-15

    摘要: The carrying case for storing and transporting heated articles includes a thermal storage assembly having a heat retention member for absorbing and retaining sensible heat and for releasing the sensible heat of a extended period time. The thermal storage assembly includes a heating coil assembly secured to a surface of the heat retention member. The heating coil assembly includes a resistive heating coil disposed adjacent to the heat retention member. The heating coil has a power cord connected to the coil with the coil being retained within a sealed thermally conductive pouch.

    摘要翻译: 用于存储和运送加热制品的手提箱包括具有用于吸收和保持显热并用于释放延长的时间段的显热的保温构件的蓄热组件。 热存储组件包括固定到保温构件表面的加热线圈组件。 加热线圈组件包括邻近保温构件设置的电阻加热线圈。 加热线圈具有连接到线圈的电源线,线圈被保持在密封的导热袋内。

    Heat-resistant martensite alloy excellent in high-temperature creep rupture strength and ductility and process for producing the same
    7.
    发明授权
    Heat-resistant martensite alloy excellent in high-temperature creep rupture strength and ductility and process for producing the same 有权
    耐高温马氏体合金具有优异的高温蠕变断裂强度和延展性及其制造方法

    公开(公告)号:US07128791B2

    公开(公告)日:2006-10-31

    申请号:US10240176

    申请日:2002-01-30

    IPC分类号: C22C38/18

    摘要: The present invention provides a martensitic heat resistant alloy having a composition (A) comprising, % by weight: 0.03 to 0.15% of C; 0.01 to 0.9% of Si: 0.01 to 1.5% of Mn; 8.0 to 13.0% of Cr; 0.0005 to 0.015% of Al; no more than 2.0% of Mo; no more than 4.0% of W; 0.05 to 0.5% of V; 0.01 to 0.2% of Nb; 0.1 to 5.0% of Co; 0.008 to 0.03% of B; less than 0.005% of N: and Fe and inevitable impurities as the remainder, wherein (B) the contents (% by weight) of Mo, W, B and N satisfy the following formulae (1) and (2). B−0.772N>0.007  (1) W+1.916Mo−16.99B>2.0  (2) The martensitic heat resistant alloy of the present invention has excellent oxidation resistance, hot workability and ductility and exhibits high creep rupture strength in a range of relatively long rupture time at a high temperature.

    摘要翻译: 本发明提供具有组成(A)的马氏体系耐热合金,其组成为:重量%:C:0.03〜0.15% 0.01〜0.9%的Si:0.01〜1.5%的Mn; 8.0〜13.0%的Cr; 0.0005〜0.015%的Al; 不超过2.0%的Mo; 不超过4.0%的W; 0.05〜0.5%V; 0.01〜0.2%的Nb; 0.1〜5.0%的Co; 0.008〜0.03%B; 小于0.005%的N和Fe以及不可避免的杂质作为余量,其中(B)Mo,W,B和N的含量(重量%)满足下式(1)和(2)。 <?in-line-formula description =“In-line Formulas”end =“lead”?> B-0.772N> 0.007(1)<?in-line-formula description =“In-line Formulas”end =“tail “?> <?in-line-formula description =”In-line Formulas“end =”lead“?> W + 1.916Mo-16.99B> 2.0(2)<?in-line-formula description =”In-line 公式“end =”tail“?>本发明的马氏体系耐热合金具有优异的抗氧化性,热加工性和延展性,并且在高温下相对长的断裂时间的范围内表现出高的蠕变断裂强度。

    Humidity conditioner and humidity conditioning method using the same
    8.
    发明申请
    Humidity conditioner and humidity conditioning method using the same 审中-公开
    湿度调理剂和湿度调理方法使用相同

    公开(公告)号:US20070119301A1

    公开(公告)日:2007-05-31

    申请号:US10590714

    申请日:2005-02-25

    申请人: Fujio Abe

    发明人: Fujio Abe

    IPC分类号: B01D53/02 C01B31/16

    摘要: The present invention is a humidity conditioner having a configuration in which one or more water-soluble polymers are introduced into a three-dimensional framework that is formed by one or more crosslinked water-absorbing polymers. Here, for the water-absorbing polymers, either polyacrylate salt or one or more polyacrylate salt-polyvinyl alcohol copolymers can be used. For the water-soluble polymers, one or both of polyvinyl alcohol and polyisopropylacrylamide can be used.

    摘要翻译: 本发明是一种湿度调节剂,其具有一种或多种水溶性聚合物引入由一种或多种交联吸水聚合物形成的三维骨架中的构型。 这里,对于吸水性聚合物,可以使用聚丙烯酸酯盐或一种或多种聚丙烯酸酯盐 - 聚乙烯醇共聚物。 对于水溶性聚合物,可以使用聚乙烯醇和聚异丙基丙烯酰胺中的一种或两种。

    Thermal storage and transport
    9.
    发明授权
    Thermal storage and transport 失效
    热存储和运输

    公开(公告)号:US5892202A

    公开(公告)日:1999-04-06

    申请号:US706651

    申请日:1996-09-06

    摘要: The carrying case for storing and transporting heated articles includes a thermal storage assembly having a heat retention member for absorbing and retaining sensible heat and for releasing the sensible heat of a extended period time. The thermal storage assembly includes a heating coil assembly secured to a surface of the heat retention member. The heating coil assembly includes a resistive heating coil disposed adjacent to the heat retention member. The heating coil has a power cord connected to the coil with the coil being retained within a sealed thermally conductive pouch.

    摘要翻译: 用于存储和运送加热制品的手提箱包括具有用于吸收和保持显热并用于释放延长的时间段的显热的保温构件的蓄热组件。 热存储组件包括固定到保温构件表面的加热线圈组件。 加热线圈组件包括邻近保温构件设置的电阻加热线圈。 加热线圈具有连接到线圈的电源线,线圈被保持在密封的导热袋内。