SILICON MONOXIDE VAPOR DEPOSITION MATERIAL, AND PROCESS, RAW MATERIAL AND APPARATUS FOR PRODUCING THE SAME
    1.
    发明申请
    SILICON MONOXIDE VAPOR DEPOSITION MATERIAL, AND PROCESS, RAW MATERIAL AND APPARATUS FOR PRODUCING THE SAME 审中-公开
    硅氧化物蒸气沉积材料及其制备原料及其制造方法

    公开(公告)号:US20070166219A1

    公开(公告)日:2007-07-19

    申请号:US11470954

    申请日:2006-09-07

    IPC分类号: C01B33/113

    摘要: A high-purity silicon monoxide vapor deposition material which, in the formation of a film by vapor deposition, is effective in inhibiting splashing, and which has an average bulk density of 2.0 g/cml and a Vickers hardness of 500 or higher; a process for producing a high-purity silicon monoxide vapor deposition material consisting of SiO and metal impurities as the remainder, the total amount of the impurities being, 50 ppm or smaller, which comprises conducting a degassing, treatment in a raw-material chamber at a temperature lower than the sublimation temperature of silicon monoxide, raising the temperature to sublimate silicon monoxide, and depositing the silicon monoxide on a substrate in a deposition chamber. and a raw material for the silicon monoxide vapor deposition material which comprises silicon metal particles and silicon dioxide particles, the average particle size of each particulate material being I to 40 μm and/or the two particulate

    摘要翻译: 通过气相沉积形成膜的高纯度一氧化硅气相沉积材料有效地防止飞溅,平均堆积密度为2.0g / cm 3,维氏硬度为500或更高; 制备由SiO和金属杂质构成的高纯度一氧化硅气相沉积材料作为其余部分的方法,所述杂质的总量为50ppm以下,其包括在原料室中进行脱气处理 温度低于一氧化硅的升华温度,升高温度以升温一氧化硅,并将一氧化硅沉积在沉积室中的基板上。 以及包含硅金属颗粒和二氧化硅颗粒的一氧化硅气相沉积材料的原料,每个颗粒材料的平均粒度为I至40μm和/或两个颗粒

    PROCESS FOR PRODUCING SPHERICAL TITANIUM ALLOY POWDER
    2.
    发明申请
    PROCESS FOR PRODUCING SPHERICAL TITANIUM ALLOY POWDER 审中-公开
    生产球形钛合金粉的方法

    公开(公告)号:US20090107294A1

    公开(公告)日:2009-04-30

    申请号:US12299854

    申请日:2007-03-22

    IPC分类号: B22F9/08

    摘要: In production of a titanium alloy spherical powder by a gas atomizing method, the difference in alloy composition depending on the product particle size is reduced economically. To achieve this, sponge titanium particles and additive metal element particles are mixed by means of a mixer having a pulverizing function such as a ball mill. The mixed particles are compressed to form a rod-formed raw material for melting. The formed rod-formed raw material for melting is powderized by a gas atomizing method. In the mixing step, the additive metal element particles are pulverized, or ground depending on the kind of particles, and solidly adhered to the surface of the sponge titanium particles, so that uniform mixing is possible.

    摘要翻译: 在通过气体雾化法生产钛合金球形粉末时,经济地降低了根据产品粒度的合金组成的差异。 为了实现这一点,海绵钛颗粒和添加金属元素颗粒通过具有粉碎功能的混合器如球磨机混合。 将混合的颗粒压缩以形成用于熔化的棒状原料。 通过气体雾化法将形成的棒状熔融原料粉化。 在混合步骤中,添加金属元素颗粒根据颗粒的种类被粉碎或研磨,并牢固地附着在海绵钛颗粒的表面上,使得均匀混合是可能的。

    GAS-TURBINE COOLING SYSTEM AND GAS-TURBINE COOLING METHOD
    3.
    发明申请
    GAS-TURBINE COOLING SYSTEM AND GAS-TURBINE COOLING METHOD 审中-公开
    气涡轮冷却系统和气体涡轮冷却方法

    公开(公告)号:US20140338362A1

    公开(公告)日:2014-11-20

    申请号:US14344465

    申请日:2012-09-12

    IPC分类号: F02C6/18 F02C7/16

    摘要: A gas turbine can efficiently be cooled by using steam, without using high-pressure steam generated in an exhaust-heat recovery boiler and without decreasing the high-pressure steam generation. This cooling system is provided with a gas turbine; an exhaust-heat recovery boiler having a high-pressure system that generates high-pressure steam by means of heat exchange with exhaust heat from the gas turbine, a high-pressure drum that supplies water and steam to the high-pressure system, a medium-pressure system that generates medium-pressure steam by means of heat exchange with the exhaust heat from the gas turbine, and a medium-pressure drum that supplies water and steam to the medium-pressure system; a medium-pressure steam pipe that connects the medium-pressure system and a cooling system of the gas turbine and that supplies the medium-pressure steam from the medium-pressure system to the cooling system; and a steam supplying pipe that connects the high-pressure drum and the medium-pressure drum.

    摘要翻译: 燃气轮机可以通过使用蒸汽而被有效地冷却,而不使用在废热回收锅炉中产生的高压蒸汽,而不会降低高压蒸汽产生。 该冷却系统设有燃气轮机; 具有高压系统的废热回收锅炉,其通过与来自燃气轮机的废热进行热交换而产生高压蒸汽,向高压系统供给水和蒸汽的高压罐,介质 压力系统,通过与来自燃气轮机的废热进行热交换产生中压蒸汽;以及中压鼓,其向中压系统供水和蒸汽; 中压蒸汽管,其连接中压系统和燃气轮机的冷却系统,并将中压蒸汽从中压系统供应到冷却系统; 以及连接高压鼓和中压鼓的蒸汽供给管。

    Molecular assembly
    4.
    发明授权
    Molecular assembly 有权
    分子装配

    公开(公告)号:US08063207B2

    公开(公告)日:2011-11-22

    申请号:US12237795

    申请日:2008-09-25

    IPC分类号: C07F9/80 C07F15/00

    CPC分类号: C07F15/0066

    摘要: A molecular assembly comprising a host metal complex with a space formed therein, and compounds having substituents enclosed in the metal complex within the space and molecular chains bonded to the substituents and extending to the exterior of the metal complex, wherein two or more substituents are enclosed in the same space of the metal complex.

    摘要翻译: 包含其中形成有空间的主体金属络合物的分子组合物,以及封闭在空间内的金属络合物中的取代基和与取代基键合并延伸至金属络合物外部的分子链的化合物,其中封闭了两个或多个取代基 在同一个空间的金属复合体。

    SYNTHESIS METHOD OF POLYMER COMPLEX CRYSTAL
    5.
    发明申请
    SYNTHESIS METHOD OF POLYMER COMPLEX CRYSTAL 有权
    聚合物复合晶体的合成方法

    公开(公告)号:US20100105901A1

    公开(公告)日:2010-04-29

    申请号:US12530240

    申请日:2009-03-07

    IPC分类号: C07F3/06

    摘要: Disclosed is a synthesis method for synthesizing in a short time and selectively a microcrystal of a polymer complex having three three-dimensionally and regularly arranged channels.Specifically disclosed is a synthesis method of a polymer complex crystal wherein (1) a metallic solution, which is a mixture of zinc halide(II) and a solvent A that can dissolve the zinc halide, is mixed with (2) a ligand solution, which is a mixture of a tridentate ligand that has three coordination sites coordinated to zinc of the zinc halide and a solvent B that can dissolve the tridentate ligand, to be a single-phase solution, thereby synthesizing a microcrystal of a polymer complex having a three-dimensional coordination network formed by coordinating the tridentate ligand to the zinc and having channels that are three-dimensionally and regularly arranged in the three-dimensional coordination network.

    摘要翻译: 公开了一种用于在短时间内合成具有三个三维和规则排列的通道的聚合物复合物的微晶体的合成方法。 具体公开了一种聚合物络合物晶体的合成方法,其中(1)将卤化锌(II)和可溶解卤化锌的溶剂A的混合物的金属溶液与(2)配体溶液混合, 其是具有与卤化锌的锌配位的三个配位点和能够溶解三齿配体的溶剂B的三齿配体的混合物,作为单相溶液,由此合成具有三元组分的聚合物配合物的微晶体 通过将三齿配体与锌配位并且具有三维和规则地排列在三维协调网络中的通道形成的三维配位网络。

    Refrigerating apparatus
    6.
    发明授权
    Refrigerating apparatus 有权
    制冷装置

    公开(公告)号:US07246498B2

    公开(公告)日:2007-07-24

    申请号:US10447291

    申请日:2002-09-11

    IPC分类号: F25B31/00 F25B41/00 F25B43/00

    摘要: A liquid injection type scroll compressor is used to a refrigerating apparatus using hydrocarbon fluoride refrigerant which does not contain chlorine (HFC-125/HFC-143a/HFC-134a) as an operating fluid and an amount of an injected liquid is controlled according to a discharge temperature of the compressor. Further, ester oil and/or ether oil is used as refrigerator oil and a dryer is disposed in a refrigerating cycle. With this arrangement, a refrigerating cycle operation can be stably realized in a wide range without almost changing the arrangement of a conventional refrigerating apparatus.

    摘要翻译: 液体注入型涡旋压缩机用于使用不含氯的氟化氢氟化烃制冷剂(HFC-125 / HFC-143a / HFC-134a)作为工作流体的制冷装置,并且根据 压缩机的排放温度。 此外,使用酯油和/或醚油作为冷冻机油,在制冷循环中设置干燥机。 通过这种结构,可以在宽范围内稳定地实现冷冻循环操作,而几乎不改变传统制冷装置的布置。

    Method of manufacturing preform for compounding use
    9.
    发明授权
    Method of manufacturing preform for compounding use 失效
    复合用预制棒的制造方法

    公开(公告)号:US06571858B2

    公开(公告)日:2003-06-03

    申请号:US09956555

    申请日:2001-09-20

    申请人: Makoto Fujita

    发明人: Makoto Fujita

    IPC分类号: B22D1902

    摘要: A method of manufacturing a preform for compounding use which, is to be impregnated with a molten metal to be compounded with a matrix material, is provided. The method includes the step of mixing short fibers, ceramic particles and a binder material together to make a mixture. The average of lengths of the short fibers is 100 to 200 &mgr;m while the volumetric percentage of the short fibers is 1 to 7%. The content of the binder material in the mixture is 0.3 to 5.0 mass %. The method includes also the steps of forming the mixture so as to have a predetermined shape, and sintering the mixture at a temperature of 1000 to 1150° C. to form the preform. Thus, it is restrained that the preform is deformed or an un-reinforced region is formed in the compounded portion.

    摘要翻译: 本发明提供一种制造用于复合用预成型体的方法,该预成型体将被浸渍在与基质材料混合的熔融金属中。 该方法包括将短纤维,陶瓷颗粒和粘合剂材料混合在一起以制备混合物的步骤。 短纤维的长度平均为100〜200μm,短纤维的体积比为1〜7%。 混合物中的粘合剂材料的含量为0.3〜5.0质量%。 该方法还包括形成混合物以具有预定形状的步骤,并在1000至1150℃的温度下烧结混合物以形成预成型体。 因此,限制了预成型件在复合部分中变形或未增强区域。

    Throttle control apparatus of internal combustion engine and throttle control method
    10.
    发明授权
    Throttle control apparatus of internal combustion engine and throttle control method 失效
    内燃机节气门控制装置和节气门控制方法

    公开(公告)号:US06332450B1

    公开(公告)日:2001-12-25

    申请号:US09577831

    申请日:2000-05-25

    IPC分类号: F02D902

    摘要: In a throttle control apparatus of an internal combustion engine, when the driver operates an accelerator so as to cause a motor vehicle to proceed to a steady-state running mode, a target throttle opening amount is no longer controlled to a throttle opening amount that depends upon an operated amount of the accelerator. Instead, the throttle opening amount is controlled to a value that provides a steady-state required torque. In this manner, the vehicle is immediately brought into a desired steady-state running mode, without requiring the driver to repeatedly operate the accelerator since the accelerator operation is not directly reflected by the throttle opening amount. Thus, the driver need not frequently repeat accelerator operations when the vehicle enters a steady-state running mode, thus assuring improved driveability.

    摘要翻译: 在内燃机的节气门控制装置中,当驾驶员操作加速器以使机动车辆进入稳态行驶模式时,目标节气门开度不再被控制为取决于节气门开度 在操作量的加速器上。 而是将节气门开度控制为提供稳态所要求的转矩的值。 以这种方式,车辆立即进入期望的稳态行驶模式,而不需要驾驶员重复操作加速器,因为加速器操作不直接反映在节气门开度上。 因此,当车辆进入稳态运行模式时,驾驶员不需要频繁地重复加速器操作,从而确保提高驾驶性能。