摘要:
A process of producing a semiconductor device having a highly reliable groove isolation structure with a desired radius of curvature formed at the groove upper edge and without formation of any step. The device is produced by reducing the stress generation around the groove upper edge of an element isolation groove on a semiconductor substrate, thereby optimizing the shape of an element isolation groove and making the device finer and improving the device electric characteristics.
摘要:
A process of producing a semiconductor device having a highly reliable groove isolation structure with a desired radius of curvature formed at the groove upper edge and without formation of any step. The device is produced by reducing the stress generation around the groove upper edge of an element isolation groove on a semiconductor substrate, thereby optimizing the shape of an element isolation groove and making the device finer and improving the device electric characteristics.
摘要:
A semiconductor device having a highly reliable groove isolation structure with a desired radius of curvature formed at the groove upper edge and without formation of any step, there is produced by reducing the stress generation around the groove upper edge of an element isolation groove on a semiconductor substrate, thereby optimizing the shape of an element isolation groove and making the device finer and improving the device electric characteristics.
摘要:
A process of producing a semiconductor device having a highly reliable groove isolation structure with a desired radius of curvature formed at the groove upper edge and without formation of any step. The device is produced by reducing the stress generation around the groove upper edge of an element isolation groove on a semiconductor substrate, thereby optimizing the shape of an element isolation groove and making the device finer and improving the device electric characteristics.
摘要:
A semiconductor device having a highly reliable groove isolation structure with a desired radius of curvature formed at the groove upper edge and without formation of any step, there is produced by reducing the stress generation around the groove upper edge of an element isolation groove on a semiconductor substrate, thereby optimizing the shape of an element isolation groove and making the device finer and improving the device electric characteristics.
摘要:
A silicon oxide film 2 which is exposed from a side wall of a groove 4a is etched to displace the silicon oxide film 2 backward toward an active region. The displacement amount is set to be equal to or more than a film thickness (Tr) of a silicon oxide film 5 to be formed on an inner wall of the groove 4a in a later thermal oxidation step and equal to or less than twice the film thickness (Tr) thereof. A shoulder portion of the groove 4a can be rounded by a low-temperature heat treatment at 1000.degree. C. or less, by controlling a heat treatment period such that the film thickness (Tr) of the silicon oxide film 5 is more than the film thickness (Tp) of the silicon oxide film 2 and equal to or less than three times the film thickness (Tr) thereof (Tp
摘要:
A shallow groove isolation structure (SGI) electrically insulates adjoining transistors on a semiconductor substrate. A pad oxide film is formed on the semiconductor substrate and an oxidation inhibition film is formed on the pad oxide film. Parts of the oxide inhibition film and pad oxide film are removed to form the groove. In particular, the pad oxide film is removed from an upper edge of the groove within a range of 5 to 40 nm. A region of the groove is oxidized in an oxidation environment with a cast ratio of hydrogen (H.sub.2) to oxygen (O.sub.2) being less than or equal to 0.5. At this ratio, the oxidizing progresses under low stress at the upper groove edges of the substrate thereby enabling rounding of the upper groove edges without creating a level difference at or near the upper groove edge on the substrate surface.
摘要:
A semiconductor device free from electric failure in transistors at upper trench edges can be produced by a simplified process comprising basic steps of forming a pad oxide film on the circuit-forming side of a semiconductor substrate; forming an oxidation prevention film on the pad oxide film; removing the oxidation presention film and the pad oxide film at a desired position, thereby exposing the surface of the semiconductor substrate; horizontally recessing the pad oxide film, etching the exposed surface of the semiconductor substrate by isotropic etching; forming a trench to a desired depth, using the oxidation prevention film as a mask; horizontally recessing the pad oxide film; oxidizing the trench formed in the semiconductor substrate; embedding an embedding isolation film in the oxidized trench; removing the embedding isolation film formed on the oxidation prevention film; removing the oxidation prevention film formed on the circuit-forming side of the semiconductor substrate; and removing the pad oxide film formed on the circuit-forming side of the semiconductor substrate, where round upper trench edges with a curvature can be obtained, if necessary, by conducting isotropic etching of exposed surface of the semiconductor substrate and horizontally recessing of the pad oxide film before the oxidation of the trench, whereby only one oxidation step is required.
摘要:
A semiconductor device and process of forming the device are described. The process includes forming a pad oxide film on the circuit-forming side of a semiconductor substrate; forming an oxidation prevention film on the pad oxide film; removing the oxidation prevention film and the pad oxide film at a desired position, thereby exposing the surface of the semiconductor substrate; horizontally recessing the pad oxide film; etching the exposed surface of the semiconductor substrate by isotropic etching; forming a trench to a desired depth, using the oxidation prevention film as a mask; horizontally recessing the pad oxide film; and oxidizing the trench formed in the semiconductor substrate. The produced device has round upper trench edges obtained by conducting isotropic etching of the exposed surface of the semiconductor substrate and horizontally recessing of the pad oxide film before the oxidation of the trench, whereby only one oxidation step is required.
摘要:
A method for manufacturing a semiconductor device includes the steps of (1) forming a pad oxide film of 5 nm or more on a circuit forming surface of a semiconductor substrate; (2) forming an oxidation inhibition film on the pad oxide film; (3) forming grooves of a given depth with the oxidation inhibition film as a mask; (4) receding the pad oxide film; (5) oxidizing the grooves formed on the semiconductor substrate in the range of 0