摘要:
A polypropylene thermoplastic resin composition comprising (a) a modified crystalline polypropylene of a crystalline polypropylene comprising said modified crystalline polypropylene and (b) a modified polyamide obtained by partially or wholly grafting a polyamide with a clay mineral. A polypropylene thermoplastic resin composition comprising, in addition to the above polypropylene thermoplastic resin composition comprising the components (a) and (b), one or any combination of the following components (c), (d) and (e): (c) an ethylene-.alpha.-olefin copolymer rubber or a modified ethylene-.alpha.-olefin copolymer rubber, (d) a block copolymer between a monovinyl-substituted aromatic hydrocarbon and a conjugated diene, a hydrogenation product of said block copolymer, or a modification product of said block copolymer, and (e) an inorganic filler. The modified polyamide as the component (b), obtained by modifying a polyamide with a clay mineral has good compatibility with or good dispersibility in the component (a), i.e. the modified crystalline polypropylene or the crystalline polypropylene comprising the modified crystalline polypropylene. Therefore, the polypropylene thermoplastic resin composition comprising these components (a) and (b) has excellent heat resistance and excellent impact resistance.
摘要:
A polypropylene thermoplastic resin composition comprising (a) a modified crystalline polypropylene of a crystalline polypropylene comprising said modified crystalline polypropylene and (b) a modified polyamide obtained by partially or wholly grafting a polyamide with a clay mineral. A polypropylene thermoplastic resin composition comprising, in addition to the above polypropylene thermoplastic resin composition comprising the components (a) and (b), one or any combination of the following components (c), (d) and (e): (c) an ethylene-.alpha.-olefin copolymer rubber or a modified ethylene-.alpha.-olefin copolymer rubber, (d) a block copolymer between a monovinyl-substituted aromatic hydrocarbon and a conjugated diene, a hydrogenation product of said block copolymer, or a modification product of said block copolymer, and (e) an inorganic filler. The modified polyamide as the component (b), obtained by modifying a polyamide with a clay mineral has good compatibility with or good dispersibility in the component (a), i.e. the modified crystalline polypropylene or the crystalline polypropylene comprising the modified crystalline polypropylene. Therefore, the polypropylene thermoplastic resin composition comprising these components (a) and (b) has excellent heat resistance and excellent impact resistance.
摘要:
The polypropylene resin composition of the present invention can be obtained by melt mixing:(a) a modified polypropylene obtained by grafting a crystalline propylene-ethylene block copolymer with an unsaturated carboxylic acid, or a crystalline polypropylene containing the modified polypropylene,(b) a polyamide, and(c) a modified ethylene-.alpha.-olefin copolymer rubber obtained by grafting an ethylene-.alpha.olefin copolymer rubber with an unsaturated carboxylic acid. This composition is superior in low temperature impact resistance, rigidity, heat resistance and oil resistance.
摘要:
A polypropylene resin composition having excellent rigidity, impact resistance and formability (moldability) and thus useful for the interior parts of automobile, includes (A) a crystalline E/P block copolymer containing a fraction Ac soluble in p-xylene at room temperature and having an ethylene content of 18 to 22%; (B) a crystalline E/P block copolymer containing a fraction Bc soluble in p-xylene at room temperature and having an ethylene content of 27 to 40% and (C) talc particles having an average size of 3 to 5 .mu.m and largest size less than 20 .mu.m, in which composition, (a) the p-xylene-soluble fractions Ac and Bc are in contents As and Bs based on the total weight of the copolymers (A) and (B) and satisfying As+Bs=7 to 17% by weight and As/(A +Bs)=0.1 to 0.6; (b) an isotactic pentad fraction of propylene in each of copolymers (A) and (B) is 96% or more, and the mixture of the copolymers (A) and (B) has a MFR of 20 to 35 g/10 min at 230.degree. C. under 2160 g load; and (c) the copolymers (A) and (B) are in a total weight content of 50 to 95% and talc (C) is in a weight content of 5 to 50%.
摘要:
A polypropylene resin composition comprising the following components (A), (B), (C) and (D): (A) a crystalline ethylene-propylene block copolymer containing a room-temperature-p-xylene-soluble fraction Ac having an ethylene content of 12-26% by weight and an intrinsic viscosity (measured at 135.degree. C. in decalin) of 6 dl/g or more, (B) a crystalline ethylene-propylene block copolymer containing a room-temperature-p-xylene-soluble fraction Bc having an ethylene content of 27-50% by weight and an intrinsic viscosity (measured at 135.degree. C. in decalin) of 4 dl/g or less, (C) an ethylene-.alpha.-olefin copolymer obtained by polymerization using a single-site catalyst, having a molecular weight distribution (Mw/Mn) of 2.5 or less, a melt flow ratio (MI.sub.10 /MI.sub.2.16) of 6-15 (wherein MI.sub.10 is a melt index measured at 190.degree. C. under a load of 10 kg and MI.sub.2.16 is a melt index measured at 190.degree. C. under a load of 2.16 kg) and an .alpha.-olefin proportion of 70 mole % or less, and (D) a talc having an average particle diameter of 3-7 .mu.m as measured by laser diffraction. In the composition the weight ratios As and Bs of the room-temperature-p-xylene-soluble fractions Ac and Bc to the total weight of the components (A) and (B) satisfy the following formulas (1) and (2): As+Bs=7-15% by weight (1) As/(As+Bs)=0.1-0.6 (2) The polypropylene component contained in each of the components (A) and (B) has an isotactic pentad fraction (mmmm) of 96% or more, and the mixture of the components (A) and (B) has a melt flow rate (measured at 230.degree. C. under a load of 2,160 g) of 30-70 g/10-min, the total content of the components (A) and (B) is 50-80% by weight, the content of the component (C) is 5-20% by weight, and the content of the component (D) is 15-30% by weight, and the composition comprising the components (A), (B), (C) and (D) has a melt flow rate (measured at 230.degree. C. under a load of 2,160 g) of 25 g/10-min or more. The composition is superior in stiffness, resistance to heat deformation, impact resistance and moldability and can provide a molded article of good appearance.
摘要:
Disclosed is a polypropylene resin composition for car interior fittings, comprising (a) a crystalline polypropylene, (b) particular hydrogenated block copolymer(s), (c) particular hydrogenated block copolymer(s) different from (b), and (d) a particular talc.
摘要:
A polypropylene resin composition comprising:(A) 45 to 70% by weight of an ethylene-propylene block copolymer synthesized under the process comprising the steps of;(a) polymerizing propylene with a Ziegler-Natta catalyst to obtain a highly crystalline polypropylene that contain not less than 97% by weight of a fraction insoluble in boiling n-heptane, and(b) copolymerizing ethylene with the polypropylene (a), and which(a) contains 0.5 to 10% by weight of ethylene,(b) contains 5 to 20% by weight of a fraction being soluble in p-xylene at room temperature and having an intrinsic viscosity value of not less than 2 (measured in decalin at 135.degree. C.),(c) has a melt-flow index value of 30 to 100 g/10 min., and,(d) has a value of flexural modulus of not less than 18,000 kg/cm.sup.2,(B) 10 to 20% by weight of an amorphous ethylene-propylene copolymer having(a) an ethylene content of 70 to 90% by weight,(b) a Mooney viscosity value (ML.sub.1+4 at 100.degree. C.) of 5 to 70,(C) 5 to 15% by weight of an ethylene-.alpha.-olefin copolymer having(a) an .alpha.-olefin content of 5 to 15% by mole,(b) a value of gravity of not more than 0.91, and(c) a melt-flow index value of 2.2 to 50 g/10 min. at 230.degree. C.,(D) 1 to 10% by weight of an amorphous ethylene-butene copolymer having(a) a butene content of 10 to 25% by weight, and(b) a Mooney viscosity value (ML.sub.1+4, at 100.degree. C.) of 5 to 20,(E) not more than 15% by weight of a talc that(a) has an average diameter D50 of from 1.0 to 3.0 .mu.m, and(b) does not contain a particle having a diameter of 10 .mu.m or more,wherein the component (B) is rubber reinforced by lamellae of components (C) and (D).
摘要:
A modified polyolefin-polyester graft copolymer includes (a) 10-90 parts by weight of a polyester having an intrinsic viscosity [.eta.] of 0.30-1.20 and an end carboxyl group content of 15-200 milliequivalent/kg, and (b) 90-10 parts by weight of a modified polyolefin having 0.2-5 mol % of an epoxy group or carboxyl group content and a weight-average molecular weight of 8,000-140,000.A thermoplastic resin composition includes (a) 5-95 weight % of an aromatic polycarbonate, (b) 95-5 weight % of a polyolefin, and (c) 1-30 parts by weight, per 100 parts by weight of (a)+(b), of the graft copolymer.
摘要:
A resin composition for an automobile bumper comprising components (A), (B), and (C) described below:(A) 45 to 74% by weight of a crystalline ethylene-propylene block copolymer having (a) a flexural modulus of 15,000 kg/cm.sup.2 or more, (b) an ethylene content of 5 to 20% by weight, (c) an intrinsic viscosity (decalin, 135.degree. C.) of a portion soluble in p-xylene at room temperature of 3 or more, (d) a melt flow index (MI) of 21 to 70 g/10 min., and (e) a content of a portion insoluble in boiling n-heptane of 97% by weight or more;(B) 21 to 35% by weight of elastomer selected from the group consisting of components (I), (II) and (III) and having a weight ratio of (I) : [(I)+(II)+(III)] of from 0.5 to 1.0, (a) said component (1) being an amorphous ethylene-butene copolymer having a butene content of 10 to 25% by weight and a Mooney viscosity value, (ML.sub.1+4, 100.degree. C.) of 5 to 20, (b) said component (II) being an amorphous ethylene-propylene copolymer having an ethylene content of 70 to 90% by weight and a Mooney viscosity value (ML.sub.1+4, 100.degree. C.) of 5 to 40, and (c) said component (III) being a hydrogenated block copolymer consisting of 10 to 40% by weight of an aromatic vinyl polymer block X and 60 to 90% by weight of a conjugate diene polymer block Y, having a structure of said block components being X-Y or X-(Y-X).sub.n , wherein n is 1 or 2, 90 mol% or more of said block Y being hydrogenated and the melt flow index (MI) of the hydrogenated block copolymer being 5 g/10 min. (230.degree. C., 2.16 kg) or more, and;(C) 5 to 10% by weight of talc having a combustion loss of 7% by weight or less, containing no particles having a diameter of 10 .mu.m or more and having an average particle diameter D.sub.50 of 1.0 to 3.0 .mu.m.
摘要:
A polypropylene resin composition for use in automotive inner and outer trims, comprising 50 to 85% by weight of a crystalline polypropylene (A) having an MFR (230° C.) of 7 to 70 g/10 min, 2 to 16% by weight of a hydrogenated block copolymer (B) obtained by hydrogenating at a hydrogenation ratio of at least 90% an aromatic vinyl/conjugated diene block copolymer which contains an aromatic vinyl block polymer unit in an amount of 22% by weight or less and has an MFR (230° C.) of at least 5 g/10 min, and 5 to 25% by weight of an inorganic filler (G) having an average particle size of 0.1 to 3 &mgr;m as essential components. This composition may contain, as optional components, another hydrogenated block copolymer (C), an aromatic hydrocarbon copolymer (D), a crystalline polyethylene (E) and a soft ethylene/&agr;-olefin copolymer (F). This composition is excellent in heat resistance, rigidity and impact resistance and can provide a molding having beautiful appearance.