-
公开(公告)号:US20070066738A1
公开(公告)日:2007-03-22
申请号:US11228729
申请日:2005-09-16
IPC分类号: C08K3/22
CPC分类号: C09K21/14 , C08L81/06 , C08L83/10 , C08L2205/03 , Y10T428/31504 , C08L2666/14
摘要: Blends of polysulfones, polyethersulfones and polyphenylene ether sulfones with resorcinol based polyesters, or resorcinol based polyester carbonate polymers, and silicone copolymers have improved flame resistance. Peak heat release energy is reduced and the time to reach peak heat release is increased.
摘要翻译: 聚砜,聚醚砜和聚苯醚砜与间苯二酚基聚酯或间苯二酚基聚酯碳酸酯聚合物和硅氧烷共聚物的共混物具有改善的阻燃性。 峰值热释放能量减少,达到峰值热释放的时间增加。
-
公开(公告)号:US20070100088A1
公开(公告)日:2007-05-03
申请号:US11263493
申请日:2005-10-31
申请人: Robert Gallucci , William Kernick , Mark Sanner , Rajendra Singh
发明人: Robert Gallucci , William Kernick , Mark Sanner , Rajendra Singh
CPC分类号: C08L67/03 , C08L79/08 , C08L83/10 , C08L83/12 , C08L2666/14 , C08L83/00 , C08L2666/18
摘要: Blends of siloxane copolymers, notably siloxane polyimides, with polyaryl esters or polyaryl ester carbonates containing linkages derived from resorcinol, show improved flame resistance, as measured by two minute and peak heat release, compared to conventional polycarbonates. In some instances transparent flame retardant blends can also be prepared. The compositions show good melt processability, high impact strength and high elongation, and can be used to make various flame retardant articles including sheets and films.
摘要翻译: 与常规聚碳酸酯相比,硅氧烷共聚物,特别是硅氧烷聚酰亚胺与含有源自间苯二酚的连接的聚芳基酯或聚芳基酯碳酸酯的共混物显示改善的阻燃性,如通过两分钟和峰值热释放测量的。 在某些情况下,也可制备透明阻燃剂共混物。 该组合物显示出良好的熔融加工性,高冲击强度和高伸长率,并且可以用于制造各种阻燃制品,包括片材和薄膜。
-
公开(公告)号:US20070066737A1
公开(公告)日:2007-03-22
申请号:US11228728
申请日:2005-09-16
申请人: Robert Gallucci , William Kernick , Mark Sanner , Rajendra Singh
发明人: Robert Gallucci , William Kernick , Mark Sanner , Rajendra Singh
IPC分类号: C08K3/22
CPC分类号: C08L79/08 , C08L67/03 , C08L83/10 , C08L83/12 , C08L2205/02 , C08L2205/03 , C08L2666/18 , C08L2666/14 , C08L2666/20 , C08L83/00
摘要: Blends of polyimides, polyetherimides or polyetherimide sulfones with resorcinol based polyesters, or resorcinol based polyester carbonate polymers, and silicone copolymers, have improved flame resistance. Peak heat release energy is reduced and the time to reach peak heat release is increased. In some instances the flame retardant blends show high percent transmission with low haze. Addition of metal oxides may further improve flame resistance.
摘要翻译: 聚酰亚胺,聚醚酰亚胺或聚醚酰亚胺砜与间苯二酚基聚酯或间苯二酚基聚酯碳酸酯聚合物和硅氧烷共聚物的共混物具有改善的阻燃性。 峰值热释放能量减少,达到峰值热释放的时间增加。 在一些情况下,阻燃混合物显示高透射率,低雾度。 添加金属氧化物可进一步提高阻燃性。
-
公开(公告)号:US20070065615A1
公开(公告)日:2007-03-22
申请号:US11383639
申请日:2006-05-16
申请人: Roy Odle , Kapil Sheth , Michael Donovan , Mark Sanner , Rajendra Singh , Robert Gallucci
发明人: Roy Odle , Kapil Sheth , Michael Donovan , Mark Sanner , Rajendra Singh , Robert Gallucci
IPC分类号: B32B1/08
CPC分类号: C08L79/08 , B29K2079/085 , B29L2023/00 , C08K3/22 , C08L67/03 , C08L83/10 , C08L83/12 , C08L2205/02 , C08L2205/03 , F16L9/12 , H05K1/0346 , H05K1/0353 , Y10T428/139 , C08L2666/02 , C08L2666/14 , C08L2666/18 , C08L83/00 , C08L2666/20
摘要: The present invention is directed to a tubular article of manufacture in an annular or tubular shape having an outer diameter, an inner diameter and a length comprising one or more materials selected from the group consisting of: a) an immiscible blend of polymers comprising one or more polyetherimides, having more than one glass transition temperature wherein the polyetherimide has a glass transition temperature greater than 217° Celsius; b) a miscible blend of polymers, comprising one or more polyetherimides, having a single glass transition temperature greater than 180° Celsius; or, c) a single polyetherimide having a glass transition temperature of greater than 247° Celsius
摘要翻译: 本发明涉及一种环形或管状形状的管状制品,其具有外径,内径和长度,其包括一种或多种选自以下的材料:a)聚合物的不混溶共混物,其包含一种或多种 更多的聚醚酰亚胺,具有多于一个玻璃化转变温度,其中聚醚酰亚胺的玻璃化转变温度大于217℃; b)可混合的聚合物混合物,其包含一种或多种具有大于180℃的单一玻璃化转变温度的聚醚酰亚胺; 或者c)玻璃化转变温度大于247℃的单一聚醚酰亚胺
-
公开(公告)号:US20070066740A1
公开(公告)日:2007-03-22
申请号:US11314542
申请日:2005-12-21
申请人: Roy Odle , Kopil Sheth , Michael Donovan , Mark Sanner , Rajendra Singh , Robert Gallucci
发明人: Roy Odle , Kopil Sheth , Michael Donovan , Mark Sanner , Rajendra Singh , Robert Gallucci
IPC分类号: C08K3/22
摘要: The present invention is directed to a tubular article of manufacture in an annular or tubular shape having an outer diameter, an inner diameter and a length comprising one or more materials selected from the group consisting of: a) an immiscible blend of polymers comprising one or more polyetherimides, having more than one glass transition temperature wherein the polyetherimide has a glass transition temperature greater than 217° Celsius; b) a miscible blend of polymers, comprising one or more polyetherimides, having a single glass transition temperature greater than 180° Celsius; or, c) a single polyetherimide having a glass transition temperature of greater than 247° Celsius.
摘要翻译: 本发明涉及一种环形或管状形状的管状制品,其具有外径,内径和长度,其包括一种或多种选自以下的材料:a)聚合物的不混溶共混物,其包含一种或多种 更多的聚醚酰亚胺,具有多于一个玻璃化转变温度,其中聚醚酰亚胺的玻璃化转变温度大于217℃; b)可混合的聚合物混合物,其包含一种或多种具有大于180℃的单一玻璃化转变温度的聚醚酰亚胺; 或者c)玻璃化转变温度大于247℃的单一聚醚酰亚胺。
-
公开(公告)号:US20070066741A1
公开(公告)日:2007-03-22
申请号:US11320350
申请日:2005-12-28
申请人: Michael Donovan , Robert Gallucci , Roy Odle , Mark Sanner , Kapil Sheth , Rajendra Singh
发明人: Michael Donovan , Robert Gallucci , Roy Odle , Mark Sanner , Kapil Sheth , Rajendra Singh
CPC分类号: H05K1/0346 , C08K3/22 , C08L67/03 , C08L79/08 , C08L83/10 , C08L83/12 , C08L2205/02 , C08L2205/03 , H05K1/0353 , H05K2201/0129 , C08L2666/18 , C08L2666/14 , C08L2666/20 , C08L83/00 , C08L2666/02
摘要: A composite material comprises an electrically conductive material disposed over at least a portion of a substrate wherein the substrate comprises either: a) an immiscible blend of polymers having more than one glass transition temperature and one of the polymers has a glass transition temperature greater than 180 degrees Celsius; b) a miscible blend of polymers having a single glass transition temperature greater than 217 degrees Celsius; or, c) a single virgin polymer having a glass transition temperature of greater than 247 degrees Celsius.
摘要翻译: 复合材料包括设置在基底的至少一部分上的导电材料,其中所述基底包括:a)具有多于一个玻璃化转变温度的聚合物的不混溶共混物,并且所述聚合物中的一种具有大于180的玻璃化转变温度 摄氏度 b)具有大于217摄氏度的单一玻璃化转变温度的可混合的聚合物混合物; 或者c)具有大于247摄氏度的玻璃化转变温度的单一的原始聚合物。
-
公开(公告)号:US20070197700A1
公开(公告)日:2007-08-23
申请号:US11358871
申请日:2006-02-21
申请人: Robert Gallucci , Mark Sanner , Rajendra Singh
发明人: Robert Gallucci , Mark Sanner , Rajendra Singh
IPC分类号: C08K5/00
CPC分类号: C08L69/005 , C08K5/16 , C08K5/20 , C08L67/00 , C08L67/03 , C08L79/08 , C08L2666/20 , C08L2666/18
摘要: Compositions made from a polyarylate or polyester carbonate containing greater than about 50 mole % resorcinol based ester linkages give miscible blends with polyimide resins, addition of alkyl amide compounds improves mold release and melt flow while maintaining transparency. The blends also have high refractive index and low haze.
摘要翻译: 含有大于约50摩尔%间苯二酚基酯键的多芳基化合物或聚酯碳酸酯的组合物可与聚酰亚胺树脂混合混合,加入烷基酰胺化合物可改善脱模和熔体流动同时保持透明度。 混合物也具有高折射率和低雾度。
-
公开(公告)号:US20070066739A1
公开(公告)日:2007-03-22
申请号:US11272982
申请日:2005-11-14
申请人: Roy Odle , Kapil Sheth , Michael Donovan , Mark Sanner , Rajendra Singh , Robert Gallucci
发明人: Roy Odle , Kapil Sheth , Michael Donovan , Mark Sanner , Rajendra Singh , Robert Gallucci
IPC分类号: C08K3/22
CPC分类号: C08J7/047 , C08G77/42 , C08K3/22 , C08L67/03 , C08L79/08 , C08L2205/02 , C08L2666/02 , C08L2666/20
摘要: The present invention relates generally to the field of articles of manufacture in the form of a shaped article comprising a blend of polymers wherein all, or some of, one or more surfaces of the shaped article is coated with a covering material, wherein the covering material has a different composition than the shaped article, and, wherein the shaped article comprises either: a) an immiscible blend of polymers having more than one glass transition temperature and one of the polymers has a glass transition temperature greater than 180° Celsius; b) a miscible blend of polymers having a single glass transition temperature greater than 217° Celsius; or, c) a single virgin polymer having a glass transition temperature of greater than 247° Celsius. The present invention is also directed to light source reflectors comprising a polymer according to a), b) or c) above.
摘要翻译: 本发明一般涉及成形制品形式的领域,其包括聚合物的共混物,其中成型制品的一个或多个表面的一个或多个表面涂覆有覆盖材料,其中覆盖材料 具有与成形制品不同的组成,并且其中成形制品包括:a)具有多于一个玻璃化转变温度的聚合物的不混溶共混物,并且所述聚合物之一具有大于180℃的玻璃化转变温度; b)具有大于217℃的单一玻璃化转变温度的可混合的聚合物混合物; 或者c)玻璃化转变温度大于247℃的单一的原始聚合物。 本发明还涉及包含根据上述a),b)或c)的聚合物的光源反射器。
-
公开(公告)号:US20050288406A1
公开(公告)日:2005-12-29
申请号:US10878954
申请日:2004-06-28
申请人: Robert Gallucci , Mark Sanner , Paul Sybert
发明人: Robert Gallucci , Mark Sanner , Paul Sybert
IPC分类号: C08K5/00 , C08K5/5313 , C08K5/5333 , C08L67/02 , C08L67/03 , C08L69/00 , C08L79/08 , C08K5/49
CPC分类号: C08L69/005 , C08K5/0066 , C08K5/5313 , C08K5/5333 , C08L67/02 , C08L67/03 , C08L79/08 , C08L2666/20 , C08L2666/18
摘要: Compositions made from a polyarylate or polyester carbonate containing greater than about 50 mole % resorcinol based ester linkages give miscible blends with polyimide resins. The blends of polyimides and resorcinol based polyesters or resorcinol based polyester carbonates also give miscible blends when combined with other aryl alky polyester resins.
摘要翻译: 由含有大于约50摩尔%间苯二酚基酯键的多芳基化合物或聚酯碳酸酯制成的组合物可与聚酰亚胺树脂混合。 当与其他芳基烷基聚酯树脂结合时,聚酰亚胺和间苯二酚基聚酯或间苯二酚基聚酯碳酸酯的共混物也提供可混溶的共混物。
-
公开(公告)号:US20060078751A9
公开(公告)日:2006-04-13
申请号:US10869231
申请日:2004-06-15
CPC分类号: C08K5/42 , H05K1/0373 , H05K1/0393 , H05K2201/0129 , H05K2203/122 , Y10T428/31681 , Y10T428/31721 , C08L81/06 , C08L79/08
摘要: A film can comprise greater than or equal to about 95 wt % thermoplastic resin and about 0.001 wt % to about 5.0 wt % sulfonate salt, based on a total weight of the film, and have a UL-94 rating of VTM-0, wherein the thermoplastic resin is selected from the group consisting of polyimide, polysulfone, and copolymers, reaction products, and combinations comprising at least one of the foregoing thermoplastic resins.
摘要翻译: 基于膜的总重量,膜可以包含大于或等于约95重量%的热塑性树脂和约0.001重量%至约5.0重量%的磺酸盐,并且具有VT-0的UL-94等级,其中 热塑性树脂选自聚酰亚胺,聚砜,共聚物,反应产物和包含至少一种前述热塑性树脂的组合。
-
-
-
-
-
-
-
-
-