Molybdenum Based Complex Oxide Catalyst, Its Preparation Method and Use
    4.
    发明申请
    Molybdenum Based Complex Oxide Catalyst, Its Preparation Method and Use 审中-公开
    钼基复合氧化物催化剂及其制备方法及用途

    公开(公告)号:US20160184805A1

    公开(公告)日:2016-06-30

    申请号:US14960946

    申请日:2015-12-07

    IPC分类号: B01J23/887 B01J37/00

    摘要: Disclosed are a molybdenum based composite oxide catalyst, its preparation method and use. The catalyst has the following general formula: BiMoxMyNzOa; wherein M is one of V, Cr, Mn, Fe, Co, Ni and Cu, or a mixture of two or more of V, Cr, Mn, Fe, Co, Ni and Cu in any ratio; N is one of Na, K, Cs, Ca and Ba, or a mixture of two or more of Na, K, Cs, Ca and Ba in any ratio; x=0.5˜20; y=0.05˜20; z=0.0˜15; a is a number satisfying the valance of each atom. The catalyst is prepared by the following method: firstly mixing a certain amount of the lead metal oxides according to the chemical proportion and then grinding the mixture with high-energy ball milling for a period of time to obtain the molybdenum based composite oxide catalyst. The catalyst exhibits excellent performance when using for preparation of butadiene by oxidative dehydrogenation of butene, and the preparation process is simple, controllable, and repeatable. Waste water or waste gas that is difficult to be treated is not produced during preparation.

    摘要翻译: 公开了一种钼基复合氧化物催化剂及其制备方法和用途。 催化剂具有以下通式:BiMoxMyNaOa; 其中M为V,Cr,Mn,Fe,Co,Ni和Cu中的一种,或V,Cr,Mn,Fe,Co,Ni和Cu中的两种或多种的任何比例的混合物; N是Na,K,Cs,Ca和Ba中的一种,或Na,K,Cs,Ca和Ba中的两种或多种的任何比例的混合物; x = 0.5〜20; y = 0.05〜20; z = 0.0〜15; a是满足每个原子价值的数。 催化剂通过以下方法制备:首先根据化学成分混合一定量的铅金属氧化物,然后用高能球磨研磨混合物一段时间,得到钼基复合氧化物催化剂。 当通过丁烯的氧化脱氢制备丁二烯时,催化剂表现出优异的性能,制备过程简单,可控,可重复。 在制备过程中不会产生难以处理的废水或废气。

    Heteropoly acid salt catalyst and its preparation method
    9.
    发明授权
    Heteropoly acid salt catalyst and its preparation method 有权
    杂多酸盐催化剂及其制备方法

    公开(公告)号:US09314772B2

    公开(公告)日:2016-04-19

    申请号:US14086368

    申请日:2013-11-21

    摘要: Disclosed are a catalyst and preparation method and use thereof. The catalyst has a constitution represented as the formula below, wherein, D represents at least one element selected from the group consisting of copper, magnesium, manganese, stibium and zinc; E represents at least one element selected from the group consisting of tungsten, silicon, nickel, palladium, ferrum and plumbum; Z is selected from the group consisting of SiC, MoO3, WO3, TiO2 and ZrO2; y/x=11.1-50:100; a=0.1-3; b=0.01-5; c=0.01-5; d=0.01-3; e=0.01-2; f is the proportion of oxygen atom balancing the valence. The method comprises: (i) formulating Solution A with molybdenum, phosphorus, and vanadium compounds; formulating Solution B with dissolve potassium compound and a D-containing compound; formulating Solution C with an E-containing compound; (ii) mix Solutions A, B and C under a temperature of −5-10° C.; (iii) pre-calcination (iv) adding graphite powder and the diluting heat-conductive agent, wherein the weight ratio between the diluting heat-conductive agent and the catalyst precursor (y/x) is 11.1-50%; and (v) calcination. x(Mo12PaKbVcDdEeOf)/yZ

    摘要翻译: 公开了催化剂及其制备方法和用途。 催化剂具有如下式所示的结构,其中,D表示选自铜,镁,锰,锑和锌中的至少一种元素; E表示选自钨,硅,镍,钯,铁和铅的至少一种元素; Z选自SiC,MoO 3,WO 3,TiO 2和ZrO 2; y / x = 11.1-50:100; a = 0.1-3; b = 0.01-5; c = 0.01-5; d = 0.01-3; e = 0.01-2; f是平衡价态的氧原子的比例。 该方法包括:(i)用钼,磷和钒化合物配制溶液A; 用溶解的钾化合物和含D化合物配制溶液B; 用含E化合物配制溶液C; (ii)在5-10℃的温度下混合溶液A,B和C. (iii)预煅烧(iv)添加石墨粉末和稀释导热剂,其中稀释导热剂和催化剂前体之间的重量比(y / x)为11.1-50%; 和(v)煅烧。 x(Mo12PaKbVcDdEef)/ yZ

    HETEROPOLY ACID SALT CATALYST AND ITS PREPARATION METHOD
    10.
    发明申请
    HETEROPOLY ACID SALT CATALYST AND ITS PREPARATION METHOD 有权
    异源酸盐催化剂及其制备方法

    公开(公告)号:US20140141964A1

    公开(公告)日:2014-05-22

    申请号:US14086368

    申请日:2013-11-21

    IPC分类号: B01J27/224

    摘要: Disclosed are a catalyst and preparation method and use thereof. The catalyst has a constitution represented as the formula below, wherein, D represents at least one element selected from the group consisting of copper, magnesium, manganese, stibium and zinc; E represents at least one element selected from the group consisting of tungsten, silicon, nickel, palladium, ferrum and plumbum; Z is selected from the group consisting of SiC, MoO3, WO3, TiO2 and ZrO2; y/x=11.1-50:100; a=0.1-3; b=0.01-5; c=0.01-5; d=0.01-3; e=0.01-2; f is the proportion of oxygen atom balancing the valence. The method comprises: (i) formulating Solution A with molybdenum, phosphorus, and vanadium compounds; formulating Solution B with dissolve potassium compound and a D-containing compound; formulating Solution C with an E-containing compound; (ii) mix Solutions A, B and C under a temperature of −5-10° C.; (iii) pre-calcination (iv) adding graphite powder and the diluting heat-conductive agent, wherein the weight ratio between the diluting heat-conductive agent and the catalyst precursor (y/x) is 11.1-50%; and (v) calcination. x(Mo12PaKbVcDdEeOf)/yZ

    摘要翻译: 公开了催化剂及其制备方法和用途。 催化剂具有如下式所示的结构,其中,D表示选自铜,镁,锰,锑和锌中的至少一种元素; E表示选自钨,硅,镍,钯,铁和铅的至少一种元素; Z选自SiC,MoO 3,WO 3,TiO 2和ZrO 2; y / x = 11.1-50:100; a = 0.1-3; b = 0.01-5; c = 0.01-5; d = 0.01-3; e = 0.01-2; f是平衡价态的氧原子的比例。 该方法包括:(i)用钼,磷和钒化合物配制溶液A; 用溶解的钾化合物和含D化合物配制溶液B; 用含E化合物配制溶液C; (ii)在5-10℃的温度下混合溶液A,B和C. (iii)预煅烧(iv)添加石墨粉末和稀释导热剂,其中稀释导热剂和催化剂前体之间的重量比(y / x)为11.1-50%; 和(v)煅烧。 x(Mo12PaKbVcDdEef)/ yZ