摘要:
A liquid-crystalline polyester production method with a shortened reaction time and improved productivity per unit time by using an organic basic compound containing one nitrogen atom in a molecule is achieved by a liquid-crystalline polyester production method comprising carrying out acylation reaction and/or ester-exchange in the presence of an organic basic compound containing one nitrogen atom in one molecule and satisfying the following inequality (1): 0
摘要:
A liquid-crystalline polyester production method with a shortened reaction time and improved productivity per unit time by using an organic basic compound containing one nitrogen atom in a molecule is achieved by a liquid-crystalline polyester production method comprising carrying out acylation reaction and/or ester-exchange in the presence of an organic basic compound containing one nitrogen atom in one molecule and satisfying the following inequality (1): 0
摘要:
Provided is a laminated porous film comprising a laminate of a heat-resistant porous layer containing a liquid crystalline polyester and a shutdown layer containing a thermoplastic resin.
摘要:
A process for producing a porous film containing a liquid crystal polyester comprising the following steps (a), (b) and (c) in this order: (a) dispersing 1 to 1,500 parts by weight of a filler, based on 100 parts by weight of a liquid crystal polyester, in a solution in which 100 parts by weight of the liquid crystal polyester is dissolved in a solvent to produce a slurry coating liquid; (b) coating the coating liquid on at least one side of a substrate to form a coating film; and (c) removing the solvent from the coating film, immersing the film in a solvent which does not dissolve the liquid crystal polyester, and drying the film to form a porous film containing a liquid crystal polyester.
摘要:
A liquid-crystalline polymer composition with less warpage not only in molding but also in a high temperature treatment conducted after molding is provided. The liquid-crystalline polymer comprises (i) 30 to 95% by weight of a first liquid-crystalline polymer having a deflection temperature under load of 200° C. or higher and (ii) 5 to 70% by weight of a second liquid-crystalline polymer having a deflection temperature under load lower than that of the first liquid-crystalline polymer, a melting point from 270° C. to lower than 400° C. and a flow-beginning temperature of 270° C. or higher.
摘要:
An aromatic polyester film comprising a polymer having a repeating unit such as a unit derived from 4-hydroxy-carboxyphenyl is provided. The film is excellent in heat resistance and solvent resistance and can be obtained by a deposition polymerization method.
摘要:
An aromatic liquid-crystalline polyester having a small dielectric loss in a wide frequency region is provided. An aromatic liquid-crystalline polyester is provided that can manufacture a film having a small volume expansion by heating. An aromatic liquid-crystalline polyester substantially comprising a repeating structural unit originating in 2-hydroxy-6-naphthoic acid 30 to 80 mol %, a repeating structural unit originating in aromatic diol 35 to 10 mol %, and a repeating structural unit originating in aromatic dicarboxylic acid 35 to 10 mol %.
摘要:
Provided is a laminated porous film comprising a laminate of a heat-resistant porous layer containing a heat-resistant resin and a shutdown layer containing a thermoplastic resin, wherein the film has a free chlorine content of 1×102 ppm by weight or less.
摘要:
A liquid-crystalline polyester solution composition comprises an aprotic solvent and liquid-crystalline polyester. The liquid-crystalline polyester includes at least one of repeating unit selected from the group consisting of a repeating unit derived from aromatic diamine, a repeating unit derived from aromatic amine having a hydroxyl group and a repeating unit derived from aromatic amino acid, in from 10 to 35 mol % in the liquid-crystalline polyester.
摘要:
A liquid-crystalline polymer composition with less warpage not only in molding but also in a high temperature treatment conducted after molding is provided. The liquid-crystalline polymer comprises (i) 30 to 95% by weight of a first liquid-crystalline polymer having a deflection temperature under load of 200° C. or higher and (ii) 5 to 70% by weight of a second liquid-crystalline polymer having a deflection temperature under load lower than that of the first liquid-crystalline polymer, a melting point from 270° C. to lower than 400° C. and a flow-beginning temperature of 270° C. or higher.