Coated Glass Article
    1.
    发明申请
    Coated Glass Article 有权
    涂层玻璃制品

    公开(公告)号:US20110281109A1

    公开(公告)日:2011-11-17

    申请号:US13079129

    申请日:2011-04-04

    IPC分类号: B32B17/06

    摘要: A coated glass article, particularly for use as architectural glass, is gold in appearance. The coated glass article includes a glass substrate with an iron oxide coating deposited thereover, the iron oxide coating comprising primarily iron oxide in the form Fe2O3. The coated glass article has an a* value between about −5 and about 10, and a b* value between about 10 and about 40, for both transmitted and reflected light.

    摘要翻译: 特别用作建筑玻璃的涂层玻璃制品在外观上是金色的。 涂覆的玻璃制品包括其上沉积有氧化铁涂层的玻璃基底,氧化铁涂层主要包含Fe 2 O 3形式的氧化铁。 涂覆的玻璃制品对于透射和反射光具有约-5至约10的a *值和约10至约40的b *值。

    Nano-particle loaded metal oxide matrix coatings deposited via combustion deposition
    2.
    发明申请
    Nano-particle loaded metal oxide matrix coatings deposited via combustion deposition 有权
    通过燃烧沉积沉积的纳米颗粒负载金属氧化物基质涂层

    公开(公告)号:US20090233084A1

    公开(公告)日:2009-09-17

    申请号:US12076100

    申请日:2008-03-13

    IPC分类号: B05D1/12 B32B5/16 B32B17/06

    摘要: Certain example embodiments relate to coatings comprising nano-particle loaded metal oxide matrices deposited via combustion deposition. The matrix and the nano-particles comprising the coating may be of or include the same metal or a different metal. For example, the coating may include a silicon oxide matrix (e.g., SiO2, or other suitable stoichiometry) having silicon oxide (e.g., silica), titanium oxide (e.g., TiO2, titania, or other suitable stoichiometry), and/or other nano-particles embedded therein. In certain example embodiments, the coating may serve as an anti-reflective (AR) coating and, in certain example embodiments, a percent visible transmission gain of at least about 2.0%, and more preferably between about 3.0-3.5%, may be realized through the growth of a film on a first surface of the substrate. In certain example embodiments, the microstructure of the final deposited coating may resemble the microstructure of coatings produced by wet chemical (e.g., sol gel) techniques.

    摘要翻译: 某些示例性实施方案涉及包含通过燃烧沉积沉积的载有纳米颗粒的金属氧化物基质的涂层。 基质和包含该涂层的纳米颗粒可以是或包括相同的金属或不同的金属。 例如,涂层可以包括具有氧化硅(例如二氧化硅),氧化钛(例如,TiO 2,二氧化钛或其它合适的化学计量)的氧化硅基体(例如,SiO 2或其它合适的化学计量)和/或其它纳米 其中嵌入的颗粒。 在某些示例性实施例中,涂层可以用作抗反射(AR)涂层,并且在某些示例性实施例中,可以实现至少约2.0%,更优选在约3.0-3.5%之间的百分比可见透射增益 通过在衬底的第一表面上生长膜。 在某些示例性实施例中,最终沉积的涂层的微结构可类似于通过湿化学(例如,溶胶凝胶)技术产生的涂层的微结构。

    Curing Coatings on Glass Containers
    4.
    发明申请
    Curing Coatings on Glass Containers 有权
    玻璃容器上的固化涂料

    公开(公告)号:US20110226786A1

    公开(公告)日:2011-09-22

    申请号:US12727511

    申请日:2010-03-19

    IPC分类号: B65D1/40 B05D3/06

    摘要: A method of applying a coating to a glass container, which includes the steps of coating an exterior surface of the glass container with a thermally-curable coating material containing electrically-conductive nanoparticles, and exposing the coated container to radio frequency radiation such that absorption of the radio frequency radiation by the nanoparticles internally heats and cures the thermally-curable coating material on the exterior surface of the glass container to result in a cured coating on the glass container.

    摘要翻译: 一种将涂层施加到玻璃容器的方法,其包括以下步骤:用含有导电纳米颗粒的可热固化涂层材料涂覆玻璃容器的外表面,并将涂覆的容器暴露于射频辐射,使得吸收 纳米颗粒的射频辐射内部加热并固化玻璃容器的外表面上的可热固化的涂层材料,从而在玻璃容器上形成固化的涂层。

    Surface-assisted combustion deposition deposited coatings, and/or methods of making the same
    5.
    发明申请
    Surface-assisted combustion deposition deposited coatings, and/or methods of making the same 审中-公开
    表面辅助燃烧沉积沉积涂层,和/或制备它们的方法

    公开(公告)号:US20090311423A1

    公开(公告)日:2009-12-17

    申请号:US12213008

    申请日:2008-06-12

    IPC分类号: B05D1/00

    摘要: Certain example embodiments relate to surface-assisted combustion deposition deposited coatings (e.g., metal oxide coatings) formed on glass substrates, and/or methods of making the same. In certain example embodiments, a wet-applied (e.g., sol-gel applied) pre-treatment coating increases a number of nucleation sites on or proximate to the at least one surface of the substrate to be coated, and/or increases a number of binding sites or forms a binding medium on the at least one surface of the substrate to be coated. A combustion deposition deposited growth is formed thereon. The pre-treatment coating may facilitate the combustion deposition depositing of coatings.

    摘要翻译: 某些示例性实施方案涉及形成在玻璃基材上的表面辅助燃烧沉积沉积涂层(例如,金属氧化物涂层)和/或其制备方法。 在某些示例性实施例中,湿施加(例如,施加溶胶 - 凝胶)的预处理涂层增加了待涂覆的基底的至少一个表面上或附近的多个成核位点,和/或增加多个 结合位点或在待涂覆的基底的至少一个表面上形成结合介质。 在其上形成燃烧沉积生长。 预处理涂层可以有助于涂层的燃烧沉积沉积。

    Alkaline earth fluoride coatings deposited via combustion deposition
    6.
    发明申请
    Alkaline earth fluoride coatings deposited via combustion deposition 审中-公开
    通过燃烧沉积沉积的碱土氟化物涂层

    公开(公告)号:US20090274930A1

    公开(公告)日:2009-11-05

    申请号:US12149396

    申请日:2008-04-30

    IPC分类号: B05D5/00 B05D1/00 B32B33/00

    摘要: Certain example embodiments of this invention relate to the combustion deposition depositing of alkaline earth fluoride inclusive coatings on substrates from a metal inclusive organic precursor and a fluorinating reagent, or from a single-source precursor. In certain example embodiments, the fluorinating reagent may be an organic source or an inorganic source. In certain example embodiments, the alkaline earth fluoride inclusive coating may be a magnesium fluoride (e.g., MgF2 or other suitable stoichiometry) inclusive coating, although other Group 2 metals may be used in place of magnesium. In certain example embodiments, the alkaline earth fluoride inclusive coating may be an anti-reflective (AR) coating.

    摘要翻译: 本发明的某些示例性实施方案涉及从包含金属的有机前体和氟化试剂或来自单源前体的底物上沉积含碱土金属氟化物的涂层的燃烧沉积。 在某些示例性实施方案中,氟化试剂可以是有机源或无机源。 在某些示例性实施方案中,包含碱土金属氟化物的涂层可以是氟化镁(例如,MgF 2或其它合适的化学计量)的包覆涂层,尽管可以使用其它第二族金属来代替镁。 在某些示例性实施方案中,含碱土氟化物的涂层可以是抗反射(AR)涂层。

    Scratch-and etch-resistant coated glass article, and method of making same
    8.
    发明申请
    Scratch-and etch-resistant coated glass article, and method of making same 有权
    刮擦和耐蚀刻涂层玻璃制品及其制备方法

    公开(公告)号:US20100075157A1

    公开(公告)日:2010-03-25

    申请号:US12232616

    申请日:2008-09-19

    IPC分类号: B32B17/06 C23C14/08

    CPC分类号: C03C17/3441 C03C17/3452

    摘要: A scratch resistant coated article is provided which is also resistant to attacks by at least some fluorine-inclusive etchant(s) for at least a period of time. In certain example embodiments, an anti-etch layer(s) is provided on a glass substrate in order to protect the glass substrate from attacks by fluorine-inclusive etchant(s), a scratch resistant layer of or including DLC is provided over the anti-layer(s), and a seed layer is provided between the anti-layer(s) and the scratch resistant layer so as to facilitate the adhesion of the scratch resistant layer while also helping to protect the anti-layer(s). Optionally, a base layer(s) or underlayer(s) may be under at least the anti-etch layer(s).

    摘要翻译: 提供了耐刮擦的涂层制品,其还耐受至少一些含氟蚀刻剂至少一段时间的攻击。 在某些示例性实施例中,在玻璃基板上提供防蚀刻层以保护玻璃基板免受含氟蚀刻剂的攻击,抗反射层或包含DLC的抗划伤层 层,并且在抗层和抗划伤层之间设置种子层,以便于耐划伤层的粘附,同时也有助于保护抗层。 任选地,基底层或底层可以在至少一层或多层抗蚀刻层之下。

    Deposition of Ruthenium Oxide Coatings on a Substrate
    9.
    发明申请
    Deposition of Ruthenium Oxide Coatings on a Substrate 审中-公开
    氧化钌涂层在基材上的沉积

    公开(公告)号:US20090311500A1

    公开(公告)日:2009-12-17

    申请号:US12085211

    申请日:2006-11-21

    IPC分类号: B32B17/06 C23C16/40

    摘要: A CVD process is defined for producing a ruthenium dioxide or ruthenium metal like coating on an article. The article is preferably for use as an architectural glazing, and preferably has low emissivity and solar control properties. The method includes providing a heated glass substrate having a surface on which the coating is to be deposited. A ruthenium containing precursor, an oxygen containing compound, and optionally water vapor, in conjunction with an inert carrier gas, are directed toward and along the surface to be coated and the ruthenium containing precursor and the oxygen containing compound are reacted at or near the surface of the glass substrate to form a ruthenium dioxide coating.

    摘要翻译: 定义CVD工艺用于在制品上制备二氧化钌或钌金属如涂层。 该制品优选用作建筑玻璃,并且优选具有低发射率和太阳能控制性能。 该方法包括提供具有其上要沉积涂层的表面的加热玻璃基板。 将包含钌的前体,含氧化合物和任选的水蒸气与惰性载气结合,指向并沿着待涂覆的表面,并且含钌前体和含氧化合物在表面或附近反应 的玻璃基板以形成二氧化钌涂层。

    Composite coatings comprising hollow and/or shell like metal oxide particles deposited via combustion deposition
    10.
    发明申请
    Composite coatings comprising hollow and/or shell like metal oxide particles deposited via combustion deposition 审中-公开
    复合涂层包括通过燃烧沉积沉积的中空和/或壳状金属氧化物颗粒

    公开(公告)号:US20090233105A1

    公开(公告)日:2009-09-17

    申请号:US12149460

    申请日:2008-05-01

    IPC分类号: C23C16/06 B32B17/06 B32B15/04

    摘要: Certain example embodiments relate to the combustion deposition depositing of coatings comprising metal oxide matrices loaded with hollow metal oxide particles. The hollow metal oxide particles may be produced by combusting an emulsion including an aqueous phase and an oil phase, and an optional surfactant. The aqueous and/or oil phase may include a first metal oxide precursor. A second metal oxide precursor may be combusted in addition to the emulsion to produce a dense binder layer, acting as a “glue” to hold the hollow particles together. The matrix and the hollow particles comprising the coating may be of or include the same metal or a different metal. In certain example embodiments, the microstructure of the final deposited coating may resemble the microstructure of coatings produced by wet chemical (e.g., sol gel) techniques.