摘要:
A molding composition comprising an aggregate [Component (A)], a linear unsaturated polyester [Component (B)] and/or linear unsaturated polyester polyamide [Component (C)], and a radical generator [Component [D]), characterized in that each of Component (B) and Component (C) comprises a specific alkylene oxide adduct of bisphenol A in an amount of from 3 to 50 mol % based on the total amount of constituent monomers of each of Component (B) and Component (C) and a molded article obtained by molding the composition.
摘要:
A molding composition comprising (A) a fibrous material, (B) a nonlinear unsaturated polyester and/or (C) a nonlinear unsaturated polyester-polyamide, and (D) a radical generator, and a molded article obtained therefrom.
摘要:
The toner for electrophotography contains a binder resin, wherein the binder resin has a condensation polymerization-type resin for forming a matrix and an addition polymerization-type resin for forming a dispersed domain. The dispersed domain with a cross-sectional diameter of not more than 2 .mu.m has an areal proportion of not less than 90%, based on the total cross-sectional area of the dispersed domain. This toner is stable, which is capable of maintaining a suitable tribo electric charge, thereby providing a high image quality in which the formed images do not undergo deterioration even under severe environmental conditions. Moreover, in a fixing method using a heat roller; fixing at a low temperature can be performed without using an offset inhibiting liquid.
摘要:
The method of producing a binder resin has the steps of blending in advance (a) a starting material monomer mixture for two polymerization reaction types, (b) a compound which can react with both of starting material monomers for the two polymerization reaction types, and (c) a tricarboxylic or higher polycarboxylic acid or a derivative thereof, the two polymerization reaction types having independent reaction paths to each other in one reaction vessel; and concurrently carrying out the two polymerization reactions in one reaction vessel to give the binder resin. According to the present invention, the binder resin which has an excellent environmental stability in the tribo electric charge and the image quality, and also has good pulverizability and transparency can be produced. Moreover, in a fixing method using a heat roller, fixing at a low temperature can be performed without using an offset inhibiting liquid. By using such a binder resin, a toner for electrophotography and a developer having excellent performance can be obtained.
摘要:
A combination of powder coatings usable in a powder coating method for forming a coating film having visually homogeneous hue by mixing two or more powder coatings of which each color is different. In the combination of powder coatings, each of differences in triboelectric charges of two or more powder coatings is 5.0 μC/g or less. The coating method usable herein includes the step of applying onto a substrate to be coated two or more powder coatings of which each color is different, in which the triboelectric charges are controlled in the above given ranges.
摘要:
The thermosetting coating composition in a powdery form, includes (a) a binder resin prepared by the steps comprising preparing a starting material monomer mixture of two different polymerization reactions, each of the polymerization reaction being carried out in an independent reaction path, and then concurrently carrying out both of the two different polymerization reactions in one reaction vessel; (b) a colorant; and (c) a crosslinking agent. The coating film is prepared by curing the above thermosetting coating composition.
摘要:
The binder resin for producing a toner includes the following three resins (A) to (C): resin (A) having a softening point of 120.degree. C. or more and 170.degree. C. or less, a glass transition temperature of 58.degree. C. or more and less than 75.degree. C., and a weight percentage of components insoluble to chloroform at 25.degree. C. of 5% by weight or more and 50% by weight or less; resin (B) having a softening point of 90.degree. C. or more and 120.degree. C. or less, a glass transition temperature of 58.degree. C. or more and less than 75.degree. C., and a weight percentage of components insoluble to chloroform at 25.degree. C. of less than 5% by weight; and resin (C) having a softening point of 80.degree. C. or more and less than 110.degree. C., a glass transition temperature of 45.degree. C. or more and less than 58.degree. C., and a weight percentage of components insoluble to chloroform at 25.degree. C. of less than 5% by weight.
摘要:
The encapsulated toner for heat-and-pressure fixing including a heat-fusible core material containing at least a thermoplastic resin and a coloring agent and a shell comprising a hydrophilic resin formed thereon so as to cover the surface of the core material, wherein the core material contains a silicone oil having a kinematic viscosity of from 10 to 500 cSt at 25.degree. C., and wherein the encapsulated toner is obtainable by in situ polymerization method. Such an encapsulated toner can be produced by in situ polymerization method including the following steps (a)-(c): (a) dissolving an amorphous polyester in a mixture comprising a core material-constituting monomer, a polymerization initiator, a silicone oil, and a coloring agent; (b) dispersing the mixture obtained in step (a) in an aqueous dispersant, and localizing the amorphous polyester on the surface of droplets of a core-constituting material to give a polymerizable composition; and (c) polymerizing the polymerizable composition obtained in step (b) by in situ polymerization method to form a core material, wherein the core material is covered with a shell comprising the amorphous polyester, thereby giving an encapsulated toner.
摘要:
The encapsulated toner for heat-and-pressure fixing which includes a heat-fusible core material containing at least a thermoplastic resin and a coloring agent, and a shell formed thereon so as to cover the surface of the core material is produced by a process having the step of carrying out in situ polymerization using a thermoplastic resin as a main component of the shell to form a shell having a structure in which a part of the heat-fusible core material is incorporated therein, the thermoplastic resin having a mechanical loss tangent (tan .delta.) in the range of from 1.0 to 20.0 based on a dynamic viscoelasticity, when measured with a sine stress having an angular frequency of 25 rad/s at a temperature of from 80.degree. to 120.degree. C. By using the encapsulated toner, good offset resistance can be obtained in the resulting toner even when its fixing speed is slow. Also, the core material is likely to be released from the encapsulated toner upon fixing while retaining good blocking resistance and good shocking resistance.
摘要:
A molding composition comprises (A) an aggregate, at least one of (B) an unsaturated polyester and (C) an unsaturated polyester-polyamide, and (D) a radical generator comprising a peroxide represented by formula: R1OOC(CH3)2—R3—C(CH3)2OOR2 wherein R1 and R2, which may be the same or different, each represent an alkyl group having 3 to 10 carbon atoms or an arylalkyl group having 7 to 17 carbon atoms; and R3 represents an arylene group.