摘要:
A thermoplastic molding composition having reduced gloss sensitivity and no unpleasant odor is produced from a graft copolymer and a thermoplastic polymer. The graft copolymer is produced from a soft elastomeric particulate graft base obtained by emulsion polymerization of a conjugated diene alone or with a small amount of a monoethylenically unsaturated monomer, using an inorganic radical generating substance and a limited amount of chain transfer agent, upon which is grafted a vinyl aromatic monomer and acrylonitrile and optionally another monoethylenically unsaturated monomer using an inorganic radical generating substance while the use of a chain transfer agent is excluded. The thermoplastic polymer is a copolymer of a vinyl aromatic monomer and acrylonitrile and optionally an additional monoethylenically unsaturated monomer. The thermoplastic molding composition has a low level of unpleasant odor coupled with reduced gloss sensitivity and good mechanical properties.
摘要:
A thermoplastic molding composition comprising A) 2.5 to 50 wt. % of a rubber modified styrenic resin; B) 50 to 97.5 wt. % of a polycarbonate resin; C) 0.001 to 1 wt. % of an inorganic boron compound; D) 0 to 25 wt. % of further polymer resins; and E) 0 to 45 wt. % additives, shows excellent thermal stability at high temperatures and impact resistance, and no thermal discolouration during processing.
摘要:
Molding compositions comprising at least one styrene polymer and comprising at least one zeolitic material of MFI structure type, a process for removal of styrene monomer from styrene polymer, and the use of at least one zeoltic material of MFI structure type for removal of styrene monomer from a molding composition comprising styrene polymer.
摘要:
Thermoplastic moulding composition (F), comprising: A) from 5 to 80% by weight of a graft polymer (A) having bimodal particle size distribution and a moisture content of 0 to 27% by weight, made, based on (A), a1) from 40 to 90% by weight of an elastomeric particulate graft base (a1), obtained by emulsion polymerization of based on (a1), a11) from 70 to 100% by weight of at least one conjugated diene, or of at least one C1-8-alkyl acrylate, or of mixtures of these, a12) from 0 to 30% by weight of at least one other monoethylenically unsaturated monomer and a13) from 0 to 10% by weight of at least one polyfunctional, cross linking monomer; a2) from 10 to 60% by weight of a graft a2), made, based on a2), a21) from 64 to 76% by weight of at least one vinyl aromatic monomer, a22) from 24 to 36% by weight of acrylonitrile, a23) from 0 to 30% by weight of at least one other monoethylenically unsaturated monomer, and a24) from 0 to 10% by weight of at least one polyfunctional, cross linking monomer; B) from 10 to 94% by weight of a thermoplastic polymer (B) having a viscosity number VN of from 50 to 120 ml/g, made, based on (B), b1) from 64 to 72% by weight of at least one vinyl aromatic monomer, b2) from 28 to 36% by weight of acrylonitrile, and b3) from 0 to 4% by weight of at least one other monoethylenically unsaturated monomer; whereby, the difference of the acrylonitrile content in component (B) and that in the graft shell a2) is minimal 2% by weight and maximal 6% by weight and optionally further components, have preferred optical appearance when coated with metal.
摘要:
A thermoplastic moulding composition with improved metal plating properties is provided. This thermoplastic moulding composition is produced from a graft copolymer (A) a thermoplastic polymer (B) and a thermoplastic polymer (C) that is not, or only to a limited amount miscible with the thermoplastic polymer (B). The thermoplastic polymer (C) contains from 1.2 to 3% by weight of at least one monoethylenically unsaturated monomer, like acrylic acid, methacrylic acid, or dicarboxylic acids, such as maleic acid and fumaric acid and their anhydrides, such as maleic anhydride. The vinyl aromatic content of component (C) is at least 5 units lower compared to that of component (B).The graft copolymer is produced from a soft elastomeric particulate graft base with a glass transition temperature below 0° C. obtained by emulsion polymerization of a conjugated diene alone or with a small amount of a monoethylenically unsaturated monomer or of at least one C1-8-alkyl acrylate, or of mixtures of these, upon which is grafted a vinyl aromatic monomer and acrylonitrile and optionally another monoethylenically unsaturated monomer.
摘要:
Thermoplastic moulding composition (F), comprising: A) from 5 to 80% by weight of a graft polymer (A) having bimodal particle size distribution and a moisture content of 0 to 27% by weight, made, based on (A), a1) from 40 to 90% by weight of an elastomeric particulate graft base (a1), obtained by emulsion polymerization of, based on (a1), a11) from 70 to 100% by weight of at least one conjugated diene, or of at least one C1-8-alkyl acrylate, or of mixtures of these, a12) from 0 to 30% by weight of at least one other monoethylenically unsaturated monomer and a13) from 0 to 10% by weight of at least one polyfunctional, cross linking monomer; a2) from 10 to 60% by weight of a graft a2), made, based on a2), a21) from 64 to 76% by weight of at least one vinyl aromatic monomer, a22) from 24 to 36% by weight of acrylonitrile, a23) from 0 to 30% by weight of at least one other monoethylenically unsaturated monomer, and a24) from 0 to 10% by weight of at least one polyfunctional, cross linking monomer; B) from 10 to 94% by weight of a thermoplastic polymer (B) having a viscosity number VN of from 50 to 120 ml/g, made, based on (B), b1) from 64 to 72% by weight of at least one vinyl aromatic monomer, b2) from 28 to 36% by weight of acrylonitrile, and b3) from 0 to 4% by weight of at least one other monoethylenically unsaturated monomer; whereby, the difference of the acrylonitrile content in component (B) and that in the graft shell a2) is minimal 2% by weight and maximal 6% by weight and optionally further components, have preferred optical appearance when coated with metal.