摘要:
A waterborne polyurethane dispersion for the polyurethane foam of synthetic leather application, derived from (1) a prepolymer derived from the reaction of reactants comprising at least one aromatic isocyanate compound, an ethylene oxide-capped polyether triol, at least one polyether diol, and at least one polyester diol; (2) water; and (3) surfactant, is disclosed. The waterborne polyurethane dispersion can be used to prepare a synthetic leather product having superior wrinkle resistance, hand-feeling and peel strength. A synthetic leather article prepared with said waterborne polyurethane dispersion is also disclosed.
摘要:
An internally emulsified polyurethane dispersion, which is prepared by using a combined chain extender system of a hydrophilic amino siloxane compound and a polyetheramine compound, is provided. The internally emulsified polyurethane dispersion can be used to prepare a synthetic leather product having good anti-stickiness, wrinkle resistance, color fastness and superior mechanical properties. A laminated synthetic leather article prepared with said internally emulsified polyurethane dispersion as well a method for preparing the synthetic leather article are also provided.
摘要:
A foamed, opacifying element has a porous substrate composed of woven yarn strands composed of a thermoplastic polymer-coated multifilament core. It has a dry foamed composition on an opposing surface of the substrate, which includes: (a) 0.1-40 weight % of porous particles; (b) 10-80 weight %; (c) 0.2-50 weight % of one or more additives selected from the group consisting of dispersants, plasticizers, flame retardants, optical brighteners, thickeners, biocides, fungicides, tinting colorants, metal flakes, and inert inorganic or organic fillers; (d) less than 5 weight % of water; and (e) at least 0.002 weight % of an opacifying colorant different from all of the one or more additives of (c), which opacifying colorant absorbs electromagnetic radiation having a wavelength of 380-800 nm. The elements have a light-blocking value (LBV) of at least 4 and can have a bending stiffness that is greater than 0.15 milliNewtons-meter.
摘要:
A thermofusible sheet material which can be used as a fusible interlining in the textile industry, has a carrier layer made from a textile material to which a polyurethane foam coating is applied. The polyurethane foam has a pore structure in which more than 50% of the pores have a diameter, measured according to DIN ASTM E 1294, which is in the range of 5 to 30 μm.
摘要:
Foamable aqueous compositions can be foamed and applied to porous substrates to make light-blocking dry opacifying elements. Such compositions have 0.05-15 weight % of porous particles; at least 20 weight % of a binder; at least 0.0001 weight % of additives (including a surfactant); water; and at least 0.001 weight % of an opacifying colorant. Each porous particle includes a continuous polymeric phase and discrete pores; a mode particle size of 2-50 μm; and a porosity of 20-70 volume %. The continuous polymeric phase Tg is >80° C. and has a polymer viscosity of 80-500 centipoises at an ethyl acetate shear rate of 100 sec−1 at a concentration of 20 weight % at 25° C. The dry opacifying element light blocking value is at least 4 and has a luminous reflectance >40% as measured by the color space Y tristimulus value. The foamed aqueous composition has a foam density of 0.1-0.5 g/cm3.
摘要:
Foamable aqueous compositions can be foamed and applied to porous substrates to make light-blocking dry opacifying elements. Such compositions have 0.05-15 weight % of porous particles; at least 20 weight % of a binder; at least 0.0001 weight % of additives (including a surfactant); water; and at least 0.001 weight % of an opacifying colorant. Each porous particle includes a continuous polymeric phase and discrete pores; a mode particle size of 2-50 μm; and a porosity of 20-70 volume %. The continuous polymeric phase Tg is >80° C. and has a polymer viscosity of 80-500 centipoises at an ethyl acetate shear rate of 100 sec−1 at a concentration of 20 weight % at 25° C. The dry opacifying element light blocking value is at least 4 and has a luminous reflectance>40% as measured by the Y tristimulus value. The foamed aqueous composition has a foam density of 0.1-0.5 g/cm3.
摘要:
Textiles backed with a polyurethane cushion are produced by applying a layer of frothed polyurethane-forming mixture to a surface of the textile. The mixture contains both water and a physical blowing agent. The layer expands due to the action of the water and the physical blowing agent and cures to form an attached cushion having a density of 176 g/L or less.
摘要:
Described herein are methods of preparing PUD based, poromeric, synthetic leathers having improved embossing characteristics, the methods comprising: preparing a polyurethane prepolymer, wherein the prepolymer comprises at least one isocyanate resin, and at least two polyols; preparing a first mixture comprising the polyurethane prepolymer, water, a chain extender, and a first surfactant that comprises at least one surfactant; preparing a second mixture comprising the first mixture, a thickening agent, and a second surfactant the comprises at least one surfactant, frothing the second mixture and thereby forming a frothed second mixture; applying the frothed second mixture to a fabric and thereby forming a coated fabric; optionally adjusting the thickness of the frothed third mixture on the fabric; and drying the coated fabric.
摘要:
A two-liquid process for synthesizing polyurethane with high heat-resistance and high abrasion-resistance is disclosed, which utilizes a semi-reactive polymer A solution containing hydroxyl groups and a semi-reactive polymer B solution containing poly-isocyanate groups. The polymer A and B solution are mixed for performing a second reaction and then coated on a substrate by a coating machine, and the coating layer is cured to form a polyurethane film. The semi-reactive polymer A and B solution are pre-polymerized in advance. The required polyurethane resin expands on the semi-reactive polymer A and B with a whole range of new functionality and construction styles through polymerization to produce high heat-resistant and high abrasion-resistant polyurethane film through coating facility under the working temperature about 80° C. A fabric is coupled during coating step for polyurethane leather. The two-liquid process is without using solvent as carrier. The environmental problem of air and water pollution can be resolved.
摘要:
A task to be achieved by the invention is to provide a foamed sheet having excellent retention of foam, hand feeling, and peel strength. The present invention provides a foamed sheet which is formed from a water dispersion of a urethane resin (X), wherein the water dispersion has a urethane resin (X) content of 50 to 80% by mass, and the water dispersion contains no organic solvent. Further, the present invention provides a synthetic leather having at least a substrate (i) and a polyurethane layer (ii), wherein the polyurethane layer (ii) is formed from the above-mentioned foamed sheet. The foamed sheet preferably has a density of 200 to 1,000 kg/m3.