    摘要: A process for making a colored composite pavement structure comprising silylated glass aggregate particles and a polymeric binder composition is disclosed. Systems and methods are also disclosed for providing a colored composite material that cures into a pavement structure. In one embodiment, a colorant concentrate is provided by combining an inorganic colorant with a portion of a first component of a polymeric binder composition. The colorant concentrate can then be combined with the first and second components of the polymeric binder composition to provide a colored polymeric binder composition. The colored polymeric binder composition may then be applied to silylated glass aggregate particles to provide a colored composite material that cures into a pavement structure.

    摘要翻译: 公开了一种制备包含硅烷化玻璃聚集体颗粒和聚合物粘合剂组合物的着色复合路面结构的方法。 还公开了用于提供固化到路面结构中的着色复合材料的系统和方法。 在一个实施方案中,通过将无机着色剂与聚合物粘合剂组合物的第一组分的一部分组合来提供着色剂浓缩物。 然后可以将着色剂浓缩物与聚合物粘合剂组合物的第一和第二组分组合以提供着色聚合粘合剂组合物。 然后将着色的聚合物粘合剂组合物施用于甲硅烷基化的玻璃聚集体颗粒,以提供固化到路面结构中的着色复合材料。

    Asphalt shingle recycling system
    5.
    发明申请
    Asphalt shingle recycling system 有权
    沥青瓦回收系统

    公开(公告)号:US20110266381A1

    公开(公告)日:2011-11-03

    申请号:US13065025

    申请日:2011-03-11

    申请人: Thomas B. Harmon

    发明人: Thomas B. Harmon

    IPC分类号: B02C11/08

    摘要: The asphalt roofing material is delivered into a treatment chamber of a processor. Hot oil is passed through a jacket surrounding the treatment chamber. Heated asphalt forms a hot solid and/or a liquefied slurry. The hot solid and/or the liquefied slurry is then removed from the treatment chamber. The asphalt roofing material in the treatment chamber can be agitated to promote mixing. The asphalt is heated to a temperature in the range from 200 degrees Fahrenheit to 650 degrees Fahrenheit within the treatment chamber. The solid and/or liquefied slurry is milled after it has been removed from the treatment chamber. The solid and/or the liquefied slurry is cooled after it exits the treatment chamber, preferably to a temperature in the range of approximately 90 degrees Fahrenheit to 110 degrees Fahrenheit. The hot solid and/or the liquefied slurry is passed through a hammer mill after the hot solid and/or the liquefied slurry exits the treatment chamber to reduce the particle size of the solid particles.

    摘要翻译: 沥青屋顶材料被输送到处理器的处理室中。 热油通过围绕处理室的护套。 加热沥青形成热固体和/或液化浆料。 然后将热固体和/或液化的浆液从处理室中取出。 可以搅拌处理室中的沥青屋面材料以促进混合。 将沥青加热至处理室内从华氏200度至华氏650度的温度。 固体和/或液化浆料在从处理室中取出后被研磨。 固体和/或液化的浆料在其离开处理室之后被冷却,优选在约华氏温度至华氏110度的温度范围内。 热固体和/或液化浆料在热固体和/或液化浆料离开处理室之后通过锤磨机,以减小固体颗粒的粒度。

    Asphalt shingle recycling system and method
    6.
    发明授权
    Asphalt shingle recycling system and method 有权
    沥青瓦回收系统及方法

    公开(公告)号:US07913940B2

    公开(公告)日:2011-03-29

    申请号:US12381192

    申请日:2009-03-09

    申请人: Thomas B. Harmon

    发明人: Thomas B. Harmon

    IPC分类号: B02C19/00

    摘要: The asphalt roofing material is delivered into a treatment chamber of a processor. Hot oil is passed through a jacket surrounding the treatment chamber. Heated asphalt forms a hot solid and/or a liquefied slurry. The hot solid and/or the liquefied slurry is then removed from the treatment chamber. The asphalt roofing material in the treatment chamber can be agitated to promote mixing. The asphalt is heated to a temperature in the range from 200 degrees Fahrenheit to 650 degrees Fahrenheit within the treatment chamber. The solid and/or liquefied slurry is milled after it has been removed from the treatment chamber. The solid and/or the liquefied slurry is cooled after it exits the treatment chamber, preferably to a temperature in the range of approximately 90 degrees Fahrenheit to 110 degrees Fahrenheit. The hot solid and/or the liquefied slurry is passed through a hammer mill after the hot solid and/or the liquefied slurry exits the treatment chamber to reduce the particle size of the solid particles.

    摘要翻译: 沥青屋顶材料被输送到处理器的处理室中。 热油通过围绕处理室的护套。 加热沥青形成热固体和/或液化浆料。 然后将热固体和/或液化的浆液从处理室中取出。 可以搅拌处理室中的沥青屋面材料以促进混合。 将沥青加热至处理室内从华氏200度至华氏650度的温度。 固体和/或液化的浆料在从处理室中取出后被研磨。 固体和/或液化的浆料在其离开处理室之后被冷却,优选在约华氏温度至华氏110度的温度范围内。 热固体和/或液化浆料在热固体和/或液化浆料离开处理室之后通过锤磨机,以减小固体颗粒的粒度。

    Method and apparatus for the batchwise production of paving mixes
containing mineral aggregate and bituminous binder
    9.
    发明授权
    Method and apparatus for the batchwise production of paving mixes containing mineral aggregate and bituminous binder 失效
    分批生产含有矿物骨料和沥青粘合剂的铺路混合料的方法和装置

    公开(公告)号:US4793711A

    公开(公告)日:1988-12-27

    申请号:US856438

    申请日:1986-04-22

    申请人: Karl G. Ohlson

    发明人: Karl G. Ohlson

    摘要: In such batchwise production of a paving mix of mineral particles and bituminous binder, in which a coarse-grained portion of the mineral aggregate batch is first introduced in measured quantity into a container and then discharged through a discharge opening in the container, controlled by a discharge door into an asphalt mixer where the coarse-grained portion of the mineral aggregate batch is mixed with a batch of binder, whereupon the remaining, fine-grained portion of the mineral aggregate batch is introduced in measured quantity into the container and then discharged through the discharge opening into the mixer the time needed to discharge the fine-grained portion of the mineral material batch is controlled.

    摘要翻译: 在这种间歇式生产矿物颗粒和沥青粘合剂的铺路混合物中,其中矿物骨料批料的粗粒部分首先以测量的量引入容器中,然后通过容器中的排放口排出,由 排出门进入沥青混合器,其中矿物骨料批料的粗粒部分与一批粘合剂混合,然后将剩余的细粒部分的矿物骨料批料以测量的量引入容器中,然后通过 进入混合器的排出口控制排出矿物料批料的细粒部分所需的时间。

    Method and apparatus for the batchwise production of paving mixes
containing mineral aggregate and bituminous binder
    10.
    发明授权
    Method and apparatus for the batchwise production of paving mixes containing mineral aggregate and bituminous binder 失效
    分批生产含有矿物骨料和沥青粘合剂的铺路混合料的方法和装置

    公开(公告)号:US4468125A

    公开(公告)日:1984-08-28

    申请号:US285228

    申请日:1981-07-20

    申请人: Karl G. Ohlson

    发明人: Karl G. Ohlson

    摘要: In such batchwise production of a paving mix of mineral particles and bituminous binder, in which a coarse-grained portion of the mineral aggregate batch is first introduced in measured quantity into a container and then discharged through a discharge opening in the container, controlled by a discharge door into an asphalt mixer where the coarse-grained portion of the mineral aggregate batch is mixed with a batch of binder, whereupon the remaining, fine-grained portion of the mineral aggregate batch is introduced in measured quantity into the container and then discharged through the discharge opening into the mixer the time needed to discharge the fine-grained portion of the mineral material batch is controlled.

    摘要翻译: 在这种间歇式生产矿物颗粒和沥青粘合剂的铺路混合物中,其中矿物骨料批料的粗粒部分首先以测量的量引入容器中,然后通过容器中的排放口排出,由 排出门进入沥青混合器,其中矿物骨料批料的粗粒部分与一批粘合剂混合,然后将剩余的细粒部分的矿物骨料批料以测量的量引入容器中,然后通过 进入混合器的排出口控制排出矿物料批料的细粒部分所需的时间。