Abstract:
Provided are drill stem assemblies with ultra-low friction coatings for subterraneous drilling operations. In one form, the coated drill stem assemblies for subterraneous rotary drilling operations include a body assembly with an exposed outer surface including a drill string coupled to a bottom hole assembly, a coiled tubing coupled to a bottom hole assembly, or a casing string coupled to a bottom hole assembly and an ultra-low friction coating on at least a portion of the exposed outer surface of the body assembly, hardbanding on at least a portion of the exposed outer surface of the body assembly, an ultra-low friction coating on at least a portion of the hardbanding, wherein the ultra-low friction coating comprises one or more ultra-low friction layers, and one or more buttering layers interposed between the hardbanding and the ultra-low friction coating. The coated drill stem assemblies disclosed herein provide for reduced friction, vibration (stick-slip and torsional), abrasion, and wear during straight hole or directional drilling to allow for improved rates of penetration and enable ultra-extended reach drilling with existing top drives.
Abstract:
Provided are drill stem assemblies with ultra-low friction coatings for subterraneous drilling operations. In one form, the coated drill stem assemblies for subterraneous rotary drilling operations include a body assembly with an exposed outer surface including a drill string coupled to a bottom hole assembly, a coiled tubing coupled to a bottom hole assembly, or a casing string coupled to a bottom hole assembly and an ultra-low friction coating on at least a portion of the exposed outer surface of the body assembly, hardbanding on at least a portion of the exposed outer surface of the body assembly, an ultra-low friction coating on at least a portion of the hardbanding, wherein the ultra-low friction coating comprises one or more ultra-low friction layers, and one or more buttering layers interposed between the hardbanding and the ultra-low friction coating. The coated drill stem assemblies disclosed herein provide for reduced friction, vibration (stick-slip and torsional), abrasion, and wear during straight hole or directional drilling to allow for improved rates of penetration and enable ultra-extended reach drilling with existing top drives.
Abstract:
Provided are precipitation hardened high strength nickel based alloy welds that yield improved properties and performance in joining high strength metals. The advantageous weldments include two or more segments of ferrous or non- ferrous components, and fusion welds, friction stir welds, electron beam welds, laser beam welds, or a combination thereof bonding adjacent segments of the components together, wherein the welds comprise a precipitation hardened nickel based alloy weld metal composition including greater than or equal to 1.4 wt% of combined aluminum and titanium based on the total weight of the nickel based alloy weld metal composition. Also provided are methods for forming the welds from the nickel based alloy weld compositions, wherein the precipitation hardening occurs in the as-welded condition. The nickel based welds do not require a separate heat treatment step after welding to produce advantageous strength properties.
Abstract:
A cermet composition represented by the formula (PQ)(RS)X comprising: a ceramic phase (PQ) , a binder phase (RS) and X wherein X is at least one member selected from the group consisting of an oxide dispersoid E, an intermetallic compound F and a derivative compound G wherein said ceramic phase (PQ) is dispersed in the binder phase (RS) as particles of diameter in the range of about 0.5 to 3000 microns, and said X is dispersed in the binder phase (RS) as particles in the size range of about 1 nm to 400 nm.
Abstract:
Cermets, particularly composition gradient cermets can be prepared starting with suitable bulk metal alloys by a reactive heat treatment process involving a reactive environment selected from the group consisting of reactive carbon, reactive nitrogen, reactive boron, reactive oxygen and mixtures thereof.
Abstract:
Weld metals and methods for welding ferritic steels are provided. The weld metals have high strength and high ductile tearing resistance and are suitable for use in strain based pipelines. The weld metal contains retained austenite and has a cellular microstructure with cell walls containing lath martensite and cell interiors containing degenerate upper bainite. The weld metals are comprised of between 0.02 and 0.12 wt% carbon, between 7.50 and 14.50 wt% nickel, not greater than about 1.00 wt% manganese, not greater than about 0.30 wt% silicon, not greater than about 150 ppm oxygen, not greater than about 100 ppm sulfur, not greater than about 75 ppm phosphorus, and the balance essentially iron. Other elements may be added to enhance the properties of the weld metal. The weld metals are applied using a power source with current waveform control which produces a smooth, controlled welding arc and weld pool in the absence of C0 2 or oxygen in the shielding gas.
Abstract:
Provided are coated petrochemical and chemical industry devices and methods of making and using such coated devices. In one form, the coated petrochemical and chemical industry device includes a petrochemical and chemical industry device including one or more bodies, and a coating on at least a portion of the one or more bodies, wherein the coating is chosen from an amorphous alloy, a heat-treated electroless or electro plated based nickel-phosphorous composite with a phosphorous content greater than 12 wt%, graphite, MoS 2 , WS 2 , a fullerene based composite, a boride based cermet, a quasicrystalline material, a diamond based material, diamond-like-carbon (DLC), boron nitride, and combinations thereof. The coated petrochemical and chemical industry devices may provide for reduced friction, wear, corrosion and other properties required for superior performance.
Abstract:
Provided are strain hardened high strength nickel based alloy welds that yield improved properties and performance in joining high strength metals. The advantageous weldments include two or more segments of ferrous or non-ferrous components, and fusion welds, friction stir welds, electron beam welds, laser beam welds, or a combination thereof bonding adjacent segments of the components together, wherein the welds comprise a strain hardened nickel based alloy weld metal composition including greater than or equal to 10 wt% Mo based on the total weight of the nickel based alloy weld metal composition. Also provided are methods for forming the welds from the nickel based alloy weld compositions. The strain hardened high strength nickel based alloy welds are useful in the oil, gas and petrochemical industry in applications for natural gas transportation and storage, oil and gas well completion and production, and oil and gas refinery and chemical plants.
Abstract:
A cermet composition represented by the formula (PQ)(RS) comprising : a ceramic phase (PQ) and binder phase (RS) wherein, P is at least one metal selected from the group consisting of Group IV, Group V, Group VI elements, Q is boride, R is selected from the group consisting of Fe, Ni, Co, Mn and mixtures thereof, S comprises at least one element selected from Cr, Al, Si and Y.
Abstract:
A cermet composition and method for its manufacture represented by the formula (PQ) (RS ) comprising: a ceramic phase (PQ) and a binder phase (RS ) wherein, P is a metal selected from the group consisting of Al, Si, Mg, Ca, Y, Fe, Mn, Group IV, Group V, Group VI elements, and mixtures thereof, Q is oxide, R is a base metal selected from the group consisting of Fe, Ni Co, Mn and mixtures thereof, S consists essentially of at least one element selected from Cr, Al and Si and at least one reactive wetting element selected from the group consisting of Ti, Zr, Hf, Ta, Sc, Y, La, and Ce.