公开(公告)号:US20220010097A1
公开(公告)日:2022-01-13
申请号:US17291367
申请日:2019-11-06
Applicant: DENKA COMPANY LIMITED
Inventor: Suguru ONUKI , Wataru NISHINO , Atsunori KONDO , Yuhei ISHIGAKI , Naoki KOBAYASHI
IPC: C08K5/38 , C08F236/12
Abstract: A chloroprene-unsaturated nitrile copolymer composition containing 100 parts by mass of a chloroprene-unsaturated nitrile copolymer having 3 to 20% by mass of a structural unit derived from an unsaturated nitrile monomer, and 0.05 to 2.0 parts by mass of a xanthogen compound.
-
公开(公告)号:US20210395422A1
公开(公告)日:2021-12-23
申请号:US17291347
申请日:2019-11-06
Applicant: DENKA COMPANY LIMITED
Inventor: Wataru NISHINO , Suguru ONUKI , Atsunori KONDO , Yuhei ISHIGAKI , Naoki KOBAYASHI
IPC: C08F236/18 , C08F220/44
Abstract: A chloroprene-unsaturated nitrile copolymer having 3 to 20% by mass of a structural unit derived from an unsaturated nitrile monomer, in which the chloroprene-unsaturated nitrile copolymer has a peak at 5.80 to 6.00 ppm in a 1H-NMR spectrum as measured in a deuterochloroform solvent, and a ratio (A/B) of a peak area (A) at 5.80 to 6.00 ppm and a peak area (B) at 4.05 to 6.20 ppm is 0.6/100 to 1.1/100.
-
公开(公告)号:US20240309197A1
公开(公告)日:2024-09-19
申请号:US18277869
申请日:2022-03-23
Applicant: DENKA COMPANY LIMITED
Inventor: Gaito KIYOFUJI , Seiya TOMIZAWA , Naoki KOBAYASHI
IPC: C08L47/00
CPC classification number: C08L47/00 , C08L2201/52
Abstract: A method for producing a chloroprene-based polymer composition including a polymerization step, wherein chloroprene, or chloroprene and a monomer copolymerizable with chloroprene are polymerized; and includes monomer and emulsifier addition steps, when a total amount of monomer used in the polymerization step is 100%, an initial addition amount of monomer at start of polymerization is X %; in the monomer addition step, when the initial addition amount of the monomer is 100%, a remaining monomer is added to the polymerization system from time when polymerization progresses and Y % of the monomer initially added converts, by reaching the polymerization completion conversion; in the emulsifier addition step, when the total amount of monomer used in the polymerization step is 100%, emulsifier is added from time when polymerization progresses and Z % of the monomer converts by reaching the polymerization completion conversion; and X, Y and Z satisfy following relationship, 1
-
公开(公告)号:US20230074040A1
公开(公告)日:2023-03-09
申请号:US17788994
申请日:2021-03-22
Applicant: DENKA COMPANY LIMITED
Inventor: Hideharu MORI , Wataru NISHINO , Yushi KUMAGAI , Yutaka SAITO , Naoki KOBAYASHI
IPC: C08F293/00 , C08K5/06
Abstract: A chloroprene-based block copolymer, a latex, a latex composition, and a rubber composition that can produce a product with excellent tensile properties and flexibility without the use of a vulcanizing agent or a vulcanizing accelerator having a chloroprene-based block copolymer, contains 5 to 30% by mass of a polymer block (A) and 70 to 95% by mass of a chloroprene-based polymer block (B), wherein the polymer block (A) is derived from a monomer, when the monomer is polymerized alone, a polymer with a glass transition temperature of 80° C. or higher can be obtained and the chloroprene-based polymer block (B) includes a chloroprene monomer unit and a polyfunctional monomer unit.
-
公开(公告)号:US20230055361A1
公开(公告)日:2023-02-23
申请号:US17788958
申请日:2021-03-22
Applicant: DENKA COMPANY LIMITED
Inventor: Yushi KUMAGAI , Wataru NISHINO , Yutaka SAITO , Naoki KOBAYASHI
IPC: C08F293/00 , C08K5/01
Abstract: A chloroprene-based block copolymer, a latex, a latex composition, and a rubber composition that can produce a product with excellent flexibility and tensile properties without the use of a vulcanizing agent or a vulcanizing accelerator. A chloroprene-based block copolymer, includes 5 to 30% by mass of a polymer block (A) and 70 to 95% by mass of a chloroprene-based polymer block (B), wherein: the polymer block (A) is derived from a monomer; when the monomer is polymerized alone, a polymer with a glass transition temperature of 80° C. or higher can be obtained; the chloroprene-based polymer block (B) includes a chloroprene monomer; and the chloroprene-based block copolymer has a toluene insoluble content of 20 to 100% by mass with respect to 100% by mass of the chloroprene-based block copolymer.
-
公开(公告)号:US20230050436A1
公开(公告)日:2023-02-16
申请号:US17788950
申请日:2021-03-22
Applicant: DENKA COMPANY LIMITED
Inventor: Yushi KUMAGAI , Wataru NISHINO , Yutaka SAITO , Naoki KOBAYASHI
IPC: C08F293/00
Abstract: A chloroprene-based block copolymer latex, including a chloroprene-based block copolymer, wherein: the chloroprene-based block copolymer contains 5 to 30% by mass of a polymer block (A) and 70 to 95% by mass of a chloroprene-based polymer block (B); the polymer block (A) is derived from a monomer; when the monomer is polymerized alone, a polymer with a glass transition temperature of 80° C. or higher can be obtained; the chloroprene-based polymer block (B) includes a chloroprene monomer unit; and when the chloroprene-based block copolymer latex is molded by immersion molding to obtain a film and then the film is heat-treated at 130° C. for 30 minutes, a tensile strength at break measured in accordance with JIS K6251 of the film is 17 MPa or more is provided.
-
公开(公告)号:US20230025987A1
公开(公告)日:2023-01-26
申请号:US17788782
申请日:2021-03-22
Applicant: DENKA COMPANY LIMITED
Inventor: Yushi KUMAGAI , Wataru NISHINO , Yutaka SAITO , Naoki KOBAYASHI
IPC: C08F293/00 , C08J3/05
Abstract: An immersion-molded body, wherein: the immersion-molded body is obtained using a latex; the latex comprises a chloroprene-based block copolymer; the chloroprene-based block copolymer contains 5 to 30% by mass of a polymer block (A) and 70 to 95% by mass of a chloroprene-based polymer block (B); the polymer block (A) is derived from a monomer; when the monomer is polymerized alone, a polymer with a glass transition temperature of 80° C. or higher can be obtained; the chloroprene-based polymer block (B) includes a chloroprene monomer unit; and when the immersion-molded body is heat-treated at 130° C. for 30 minutes, a tensile strength at break of the heat-treated immersion-molded body measured in accordance with JIS K6251 is 17 MPa or more.
-
公开(公告)号:US20220396717A1
公开(公告)日:2022-12-15
申请号:US17623502
申请日:2020-08-11
Applicant: DENKA COMPANY LIMITED
Inventor: Manabu MIURA , Daisuke YOSHIMURA , Naoki KOBAYASHI , Atsunori KONDO
Abstract: An adhesive tape can reduce percussive sounds or friction sounds, can prevent contamination of a covered article due to contamination by dirt or dust or intrusion by water or oil, has durability against puncture or friction, and easily bends after binding a covered article. The adhesive tape having a substrate including 100 parts by mass of a polyvinyl chloride and, with respect to the 100 parts by mass of the polyvinyl chloride, 10-100 parts by mass of an elastomer and 10-100 parts by mass of a plasticizer, wherein the elastomer includes an acrylonitrile monomer unit and at least one monomer unit selected from the group made of a chloroprene monomer unit, a butadiene monomer unit, and an isoprene monomer unit and the adhesive tape has an attenuation value of 2 dB or greater in an acoustic absorption test.
-
公开(公告)号:US20180327576A1
公开(公告)日:2018-11-15
申请号:US15776029
申请日:2016-11-15
Applicant: DENKA COMPANY LIMITED
Inventor: Naoki KOBAYASHI , Yasushi ABE
CPC classification number: C08L11/00 , C08J3/226 , C08J2411/00 , C08K2003/222 , C08K2201/006 , C08L7/00 , C08L23/04 , C08L23/16 , C08L2205/03 , C08K3/22 , C08K5/101 , C08K3/04
Abstract: A rubber-based composition modifier includes 100 parts by mass of a mixed rubber component containing a chloroprene rubber and at least one copolymer selected from ethylene/α-olefin copolymers and ethylene/α-olefin/unconjugated polyene copolymers, 10 to 60 parts by mass of magnesium oxide, 3 to 30 parts by mass of a softener, and 30 to 120 parts by mass of acetylene black, wherein the mixed rubber component has a Mooney viscosity, as determined by the method specified in JIS K6300, of 60 to 180 at 100° C.; the magnesium oxide has a BET specific surface area, as determined by the one point method specified in JIS Z8830, of 20 to 150 m2/g; the softener contains a fatty acid ester-based plasticizer and an unsaturated fatty acid having a carbon number of 10 to 24 and containing an ester bond, a hydroxyl group, or both of them in part of the structure.
-
-
-
-
-
-
-
-