摘要:
A rubber composition containing 100 parts by weight of a diene-based rubber and 0.5 to 25 parts by weight of a heat expandable microcapsule composed of a thermoplastic resin particle having a substance enclosed therein, capable of vaporizing or expanding due to heat to thereby generate a gas, wherein a shell of the heat expandable microcapsule comprises a thermoplastic resin obtained by polymerization from, as a main component of a monomer, a nitrile-based monomer (I), a monomer (II) having an unsaturated double bond and carboxyl group in the molecule thereof, a monomer (III) having two or more polymerizable double bonds and, optionally, a copolymerizable monomer (IV) for adjusting the expansion characteristics, and a pneumatic tire using the same, whereby the tire weight is decreased and the ice traction thereof is improved.
摘要:
A rubber composition for a tire containing (i) 100 parts by weight of a diene-based rubber and (ii) 0.5 to 25 parts by weight of a heat-expandable microcapsule including a shell, and a substance capable of vaporizing or expanding under heating to thereby generate a gas and a nonpolar oil, both encapsulated in the shell,wherein the shell is made of a thermoplastic resin obtained by polymerization of a nitrile-based monomer (I), a monomer (II) having an unsaturated double bond and a carboxyl group in the molecule thereof, an optional monomer (III) having two or more polymerizable double bonds, and an optional copolymerizable monomer (IV) for adjusting the expansion properties.
摘要:
A rubber composition for a tire containing (i) 100 parts by weight of a diene-based rubber and (ii) 0.5 to 25 parts by weight of a heat-expandable microcapsule including a shell, and a substance capable of vaporizing or expanding under heating to thereby generate a gas and a nonpolar oil, both encapsulated in the shell, wherein the shell is made of a thermoplastic resin obtained by polymerization of a nitrile-based monomer (I), a monomer (II) having an unsaturated double bond and a carboxyl group in the molecule thereof, an optional monomer (III) having two or more polymerizable double bonds, and an optional copolymerizable monomer (IV) for adjusting the expansion properties.
摘要:
Thermo-expansive microcapsules comprising a shell of a polymer produced by polymerizing a mixture of monomers, which comprises (I) a nitrile monomer, (II) a monomer having an unsaturated double bond and carboxyl groups in a molecule, (III) a monomer having two or more of polymerizable double bonds in a molecule, and optionally, (IV) a monomer different from and copolymerizable with the monomers (I), (II) and (III) and a blowing agent encapsulated in the shell. The volume retention of the expanded microcapsules of the thermo-expansive microcapsules is 50% or more after loaded with 15 MPa.
摘要:
Thermo-expansive microcapsules comprising a shell of a polymer produced by polymerizing a mixture of monomers, which comprises (I) a nitrile monomer, (II) a monomer having an unsaturated double bond and carboxyl groups in a molecule, (III) a monomer having two or more of polymerizable double bonds in a molecule, and optionally, (IV) a monomer different from and copolymerizable with the monomers (I), (II) and (III) and a blowing agent encapsulated in the shell. The volume retention of the expanded microcapsules of the thermo-expansive microcapsules is 50% or more after loaded with 15 MPa.
摘要:
Heat-expandable microspheres include a shell of thermoplastic resin and core material encapsulated in the shell. The core material include a blowing agent having a boiling point not higher than the softening point of the thermoplastic resin and a gas migration inhibitor having a boiling point higher than the softening point of the thermoplastic resin. The ratio of the gas migration inhibitor to the core material is at least 1 weight percent and below 30 weight percent. The average particle size of the heat-expandable microspheres ranges from 1 to 100 micrometers.
摘要:
Heat-expandable microspheres include a shell of thermoplastic resin and core material encapsulated in the shell. The core material include a blowing agent having a boiling point not higher than the softening point of the thermoplastic resin and a gas migration inhibitor having a boiling point higher than the softening point of the thermoplastic resin. The ratio of the gas migration inhibitor to the core material is at least 1 weight percent and below 30 weight percent. The average particle size of the heat-expandable microspheres ranges from 1 to 100 micrometers.
摘要:
An electromechanical transducer includes a first electrode mounted on one of a substrate and a base film, an electromechanical transducer film mounted on the first electrode and made of a piezoelectric substance having a perovskite crystal structure, and a second electrode mounted on the electromechanical transducer film. The electromechanical transducer film includes a {100} plane preferentially oriented to be orthogonal to a thickness direction of the electromechanical transducer film and has a full width at half maximum corresponding to a {200} plane in an X-ray diffraction measurement curve in 2θ-ω scan that is measured by emitting an X-ray beam onto a surface of the electromechanical transducer film at an incident angle θ. The full width at half maximum is not greater than 10 degrees.
摘要:
The present invention provides a blood purifier which shows a decreased amount of hydrogen peroxide extracted from its selectively permeable separation membranes, and thus is highly reliable in its safety in use for hemecatharysis.The present invention relates to a blood purifier which comprises selectively permeable separation membranes as a main component and which is characterized in that the amount of hydrogen peroxide which is extracted from the selectively permeable separation membrane removed from the blood purifier after 3 months or longer has passed since the sterilization of the blood purifier by exposure to a radioactive ray and/or an electron ray is not larger than 10 ppm.
摘要:
A method that heat-expandable microspheres includes the use of a shell of thermoplastic resin and a non-fluorine blowing agent encapsulated therein having a boiling point not higher than the softening point of the thermoplastic resin. The method includes, a step of dispersing an oily mixture containing a polymerizable component, the blowing agent, and a polymerization initiator containing a peroxydicarbonate in an aqueous dispersing medium to polymerize the polymerizable component contained in the oily mixture. The resultant heat-expandable microsphres have a shell which is less apt to become thinner than its theoretical value, contain minimum amount of resin particle inside their shell, and have excellent heat-expanding performance.