POLYETHERIMIDE POLYCARBONATE BLENDS
    3.
    发明申请
    POLYETHERIMIDE POLYCARBONATE BLENDS 有权
    聚酰亚胺聚碳酸酯混合物

    公开(公告)号:US20130261202A1

    公开(公告)日:2013-10-03

    申请号:US13795210

    申请日:2013-03-12

    Abstract: The disclosure relates to compositions exhibiting a UV resistance of ΔE ranging from more than 0 to less than or equal to 10 units after exposure to ultraviolet light for 300 hours, per ASTM D-4459 protocol. The compositions can include at least 15 wt. % of a polyetherimide; at least 35 wt. % of a polycarbonate; a polyetherimide siloxane; and optionally, at least one UV stabilizer. The disclosure also relates to methods of shaping such compositions and articles produced from such compositions.

    Abstract translation: 本公开涉及根据ASTM D-4459方案,在暴露于紫外线300小时之后,显示出DeltaE的抗紫外线性范围为大于0至小于或等于10单位的组合物。 组合物可以包含至少15wt。 %的聚醚酰亚胺; 至少35重量% %的聚碳酸酯; 聚醚酰亚胺硅氧烷; 和任选的至少一种UV稳定剂。 本公开还涉及成形由这种组合物制备的这种组合物和制品的方法。

    Blends of polysulfones and polyphenylene sulfide resins
    4.
    发明授权
    Blends of polysulfones and polyphenylene sulfide resins 有权
    聚砜和聚苯硫醚树脂的共混物

    公开(公告)号:US08859651B2

    公开(公告)日:2014-10-14

    申请号:US13791673

    申请日:2013-03-08

    Abstract: Compositions including a blend of a) a polysulfone (PSU); b) a polyphenylene sulfide (PPS); and, c) a polyetherimide and epoxy. The polyetherimide and epoxy can be present in an amount effective to act as a compatibilizer for the polysulfone (PSU) and polyphenylene sulfide (PPS).Various embodiments relate to a method of compatibilizing a blend of polysulfone (PSU) and polyphenylene sulfide (PPS). The method can include a) melt mixing a polysulfone (PSU) and a polyetherimide; and b) melt mixing a polyphenylene sulfide (PPS) and an epoxy. Step a) and b) can be carried out by one of sequential mixing and simultaneous mixing.

    Abstract translation: 组合物,包括a)聚砜(PSU)的混合物; b)聚苯硫醚(PPS); 和c)聚醚酰亚胺和环氧树脂。 聚醚酰亚胺和环氧树脂可以有效地用作聚砜(PSU)和聚苯硫醚(PPS)的增容剂。 各种实施方案涉及使聚砜(PSU)和聚苯硫醚(PPS)的共混物相容化的方法。 该方法可以包括:a)熔融混合聚砜(PSU)和聚醚酰亚胺; 和b)熔融混合聚苯硫醚(PPS)和环氧树脂。 步骤a)和b)可以通过顺序混合和同时混合中的一种进行。

    BLENDS OF POLYSULFONES AND POLYPHENYLENE SULFIDE RESINS
    5.
    发明申请
    BLENDS OF POLYSULFONES AND POLYPHENYLENE SULFIDE RESINS 有权
    聚苯乙烯和聚苯乙烯树脂的混合物

    公开(公告)号:US20140194580A1

    公开(公告)日:2014-07-10

    申请号:US13791673

    申请日:2013-03-08

    Abstract: Compositions including a blend of a) a polysulfone (PSU); b) a polyphenylene sulfide (PPS); and, c) a polyetherimide and epoxy. The polyetherimide and epoxy can be present in an amount effective to act as a compatibilizer for the polysulfone (PSU) and polyphenylene sulfide (PPS).Various embodiments relate to a method of compatibilizing a blend of polysulfone (PSU) and polyphenylene sulfide (PPS). The method can include a) melt mixing a polysulfone (PSU) and a polyetherimide; and b) melt mixing a polyphenylene sulfide (PPS) and an epoxy. Step a) and b) can be carried out by one of sequential mixing and simultaneous mixing.

    Abstract translation: 组合物,包括a)聚砜(PSU)的混合物; b)聚苯硫醚(PPS); 和c)聚醚酰亚胺和环氧树脂。 聚醚酰亚胺和环氧树脂可以有效地用作聚砜(PSU)和聚苯硫醚(PPS)的增容剂。 各种实施方案涉及使聚砜(PSU)和聚苯硫醚(PPS)的共混物相容化的方法。 该方法可以包括:a)熔融混合聚砜(PSU)和聚醚酰亚胺; 和b)熔融混合聚苯硫醚(PPS)和环氧树脂。 步骤a)和b)可以通过顺序混合和同时混合中的一种进行。

    FIBER REINFORCED POLYARYLETHERKETONE RESIN COMPOSITIONS
    6.
    发明申请
    FIBER REINFORCED POLYARYLETHERKETONE RESIN COMPOSITIONS 审中-公开
    纤维增强聚烯烃酮树脂组合物

    公开(公告)号:US20150087767A1

    公开(公告)日:2015-03-26

    申请号:US14034125

    申请日:2013-09-23

    Abstract: Disclosed herein are methods and fiber reinforced thermoplastic composition comprising: a polyaryletherketone (PAEK) component; a polyimide component, wherein the polyimide component comprises a blend of at least a first polyimide (PI) having glass transition temperature of at least 300° C. and a second polyimide (PI) having glass transition temperature less than the glass transition temperature of the first polyimide; and a reinforcement fiber component. The resulting fiber reinforced thermoplastic compositions exhibit improved mechanical performance.

    Abstract translation: 本文公开了方法和纤维增强的热塑性组合物,其包含:聚芳醚酮(PAEK)组分; 聚酰亚胺组分,其中所述聚酰亚胺组分包含至少具有至少300℃的玻璃化转变温度的第一聚酰亚胺(PI)和玻璃化转变温度低于玻璃化转变温度的第二聚酰亚胺(PI)的共混物, 第一聚酰亚胺; 和增强纤维部件。 所得到的纤维增强热塑性组合物显示出改进的机械性能。

    Polyetherimide polycarbonate blends
    7.
    发明授权
    Polyetherimide polycarbonate blends 有权
    聚醚酰亚胺聚碳酸酯共混物

    公开(公告)号:US08921438B2

    公开(公告)日:2014-12-30

    申请号:US13795210

    申请日:2013-03-12

    Abstract: The disclosure relates to compositions exhibiting a UV resistance of ΔE ranging from more than 0 to less than or equal to 10 units after exposure to ultraviolet light for 300 hours, per ASTM D-4459 protocol. The compositions can include at least 15 wt. % of a polyetherimide; at least 35 wt. % of a polycarbonate; a polyetherimide siloxane; and optionally, at least one UV stabilizer. The disclosure also relates to methods of shaping such compositions and articles produced from such compositions.

    Abstract translation: 本公开涉及根据ASTM D-4459方案,在暴露于紫外线300小时之后,其抗紫外线性≥D≤E的组合物的范围为大于0至小于或等于10单位。 组合物可以包含至少15wt。 %的聚醚酰亚胺; 至少35重量% %的聚碳酸酯; 聚醚酰亚胺硅氧烷; 和任选的至少一种UV稳定剂。 本公开还涉及成形由这种组合物制备的这种组合物和制品的方法。