Nonradiative planar dielectric line and integrated circuit

    公开(公告)号:US5973580A

    公开(公告)日:1999-10-26

    申请号:US92290

    申请日:1998-06-05

    摘要: A nonradiative planar dielectric line exhibits low transmission losses and is easily connectable to electronic components. A first slot is provided between two electrodes on a first main surface of a dielectric plate. A second slot is provided between two electrodes on a second main surface of the dielectric plate. A first conductor is electrically connected to the electrodes on the first main surface and also covers the first slot. A second conductor is electrically connected to the electrodes on the second main surface and also covers the second slot. An integrated circuit using the above type of dielectric line is also provided. Thus, apparatuses using the above dielectric lines or integrated circuits are miniaturized.

    High-frequency amplifier integrated-circuit device
    93.
    发明授权
    High-frequency amplifier integrated-circuit device 失效
    高频放大器集成电路器件

    公开(公告)号:US5874859A

    公开(公告)日:1999-02-23

    申请号:US738022

    申请日:1996-10-25

    摘要: A high-frequency amplifying integrated-circuit device is provided in which variations of gain can be reduced and which can be manufactured at a low cost as compared with prior art devices. A high-frequency amplifying integrated-circuit device includes a semiconductor substrate; and a transistor which is formed on the semiconductor substrate and which has a plurality of first electrodes, a plurality of second electrodes, and at least one third electrode, a high-frequency signal input to the plurality of second electrodes being amplified by the transistor and output from the third electrode, wherein at least two first electrodes from among the plurality of first electrodes are each grounded via a capacitor, and the electrostatic capacitance values of the two capacitors are set at mutually different values.

    摘要翻译: 提供了一种高频放大集成电路器件,其中与现有技术器件相比,增益的变化可以降低并且可以以低成本制造。 高频放大集成电路器件包括半导体衬底; 以及晶体管,其形成在所述半导体基板上并且具有多个第一电极,多个第二电极以及至少一个第三电极,输入到所述多个第二电极的高频信号被所述晶体管放大;以及 从所述第三电极输出,其中,所述多个第一电极中的至少两个第一电极经由电容器接地,并且所述两个电容器的静电电容值被设定为相互不同的值。

    Method for producing superheavy oil emulsion fuel and fuel produced
thereby
    94.
    发明授权
    Method for producing superheavy oil emulsion fuel and fuel produced thereby 失效
    生产超重油乳化燃料的方法和由此生产的燃料

    公开(公告)号:US5851245A

    公开(公告)日:1998-12-22

    申请号:US863017

    申请日:1997-05-23

    IPC分类号: C10L1/32

    CPC分类号: C10L1/328

    摘要: A method for producing a superheavy oil emulsion fuel comprising the steps of (i) preparing a liquid mixture comprising a superheavy oil, water, one or more nonionic surfactants having an HLB (hydrophilic-lipophilic balance) of 13 to 19, and optionally one or more stabilizers, and then agitating the resulting liquid mixture with a high shear rate of 1000/sec to 60000/sec, to give an oil-in-water (O/W) type emulsion fuel having a superheavy oil concentration of from 74 to 82% by weight; and (ii) adding at least one of ionic dispersants, and optionally water, to the emulsion fuel obtained in step (i), and then blending and agitating the resulting liquid mixture with a shear rate of 10/sec to 10000/sec, to give an oil-in-water (O/W) type emulsion fuel having a superheavy oil concentration of from 68 to 79% by weight. In step (i), the nonionic surfactants are contained in an amount of from 0.1 to 0.8% by weight of the emulsion fuel obtained in step (i), and the stabilizers are contained in an amount of from 0.001 to 0.5% by weight of the emulsion fuel obtained in step (i). In step (ii), the ionic dispersants are contained in an amount of from 0.01 to 0.5% by weight of the emulsion fuel obtained in step (ii).

    摘要翻译: 一种制造超重油乳液燃料的方法,包括以下步骤:(i)制备包含超重油,水,一种或多种HLB(亲水 - 亲油平衡)为13至19的一种或多种非离子表面活性剂和任选的一种或多种 更多的稳定剂,然后以1000 /秒至60000 /秒的高剪切速率搅拌所得液体混合物,得到超重油浓度为74至82的油包水(O / W)型乳液燃料 重量% 和(ii)向步骤(i)中获得的乳液燃料中加入至少一种离子分散剂和任选的水,然后以10 /秒至10000 /秒的剪切速率将所得液体混合物共混并搅拌,至 得到超重油浓度为68〜79重量%的水包油型(O / W)型乳化燃料。 在步骤(i)中,非离子表面活性剂的含量为步骤(i)中获得的乳液燃料的0.1至0.8重量%,并且稳定剂的含量为0.001-0.5重量% 在步骤(i)中获得的乳液燃料。 在步骤(ii)中,离子分散剂的含量为步骤(ii)中获得的乳液燃料的0.01至0.5重量%。

    System for the recovery of ammonia escaping from an ammonia reduction
denitrator
    95.
    发明授权
    System for the recovery of ammonia escaping from an ammonia reduction denitrator 失效
    用于从氨还原脱硝机中逸出氨的回收系统

    公开(公告)号:US5770163A

    公开(公告)日:1998-06-23

    申请号:US638468

    申请日:1996-04-26

    摘要: For a system having a source of nitrogen oxide-containing gas, an ammonia reduction denitrator, and a leak ammonia recovery unit which adsorbs and removes ammonia escaping from said ammonia reduction denitrator, a method of removing adsorbed ammonia from said leak ammonia recovery unit and reusing the removed ammonia is provided which includes the steps of: introducing hot exhaust gas discharged from said nitrogen oxide-containing gas source into said leak ammonia recovery unit to desorb ammonia therefrom; after desorption of ammonia, cooling said heated leak ammonia recovery unit with cool air; and feeding ammonia carried away by said hot exhaust gas and said cool air to an upstream side of said ammonia reduction denitrator or to the source of nitrogen oxide-containing gas.

    摘要翻译: 对于具有含氮氧化物气体源的系统,氨还原脱硝机和吸附除氨从氨还原脱硝机排出的氨的泄漏氨回收装置,从所述泄漏氨回收装置中除去吸附氨的方法和再利用 提供去除的氨,其包括以下步骤:将从所述含氮氧化物的气体源排出的热废气引入所述泄漏氨回收单元以从其中解氨; 氨解氨后,用冷空气冷却加热的泄漏氨回收装置; 以及将由所述热废气和所述冷空气携带的氨供给到所述氨还原脱硝器的上游侧或含氮氧化物源的源。

    Preparation of a fermented milk drink
    96.
    发明授权
    Preparation of a fermented milk drink 失效
    制备发酵乳饮料

    公开(公告)号:US4260636A

    公开(公告)日:1981-04-07

    申请号:US880874

    申请日:1978-02-22

    IPC分类号: A23C9/123 A23C9/13 A23C9/12

    CPC分类号: A23C9/1307 A23C9/1238

    摘要: A fermented milk drink having a stable milky white appearance is prepared by adjusting the solids content and pH of a fermented milk to a solids-not-fat content of 0.5 to 2.5% and a pH of 3.00 to 3.45, heating the resultant adjusted fermented milk to a temperature above 60.degree. C. to dissolve milk protein therein, cooling the heated fermented milk and adjusting the pH to 3.5 to 3.8, and heating the fermented milk having a pH of 3.5 to 3.8 to a temperature above 60.degree. C. to cause re-formation of milk protein particles of relatively uniform small particle size to produce the fermented milk drink.

    摘要翻译: 通过将发酵乳的固体含量和pH调节至0.5-2.5%的固体 - 非脂肪含量和3.00-3.45的pH来制备具有稳定的乳白色外观的发酵乳饮料,加热所得调整后的发酵乳 温度高于60℃以溶解其中的乳蛋白,冷却加热的发酵乳并将pH调节至3.5至3.8,并将pH为3.5至3.8的发酵乳加热至高于60℃的温度以引起 重新形成相对均匀的小粒径的乳蛋白颗粒,以生产发酵乳饮料。

    Vehicle door handle system
    98.
    发明授权
    Vehicle door handle system 有权
    车门把手系统

    公开(公告)号:US09181733B2

    公开(公告)日:2015-11-10

    申请号:US12986357

    申请日:2011-01-07

    摘要: In a vehicle door handle system, a handle is pivotally supported by a base member, at least one portion of the base member being attached to an outer panel; and a lever member is pivotally supported by a spindle fixed to the base member and having an axis at a right angle to a plane extending along the outer panel, the lever member being interlocked and connected with a handle arm configured to pivot with the handle and the lever member being linked to a latch device. An attachment part which attaches the base member to the outer panel is disposed coaxially with the spindle. Accordingly, it is possible to attach the base member to the outer panel while avoiding the bulkiness of conventional systems.

    摘要翻译: 在车门把手系统中,把手由基座枢转地支撑,所述基座构件的至少一部分附接到外板; 并且杆构件由固定到所述基座构件的心轴枢转地支撑,并且具有与沿着所述外板延伸的平面成直角的轴线,所述杆构件互锁并与手柄臂连接,所述手柄臂构造成与所述手柄枢转, 杠杆构件连接到闩锁装置。 将基座部件附接到外板的安装部件与主轴同轴设置。 因此,可以避免常规系统的蓬松性而将基座部件附接到外板。

    Si-killed steel wire rod and spring excellent in fatigue properties
    99.
    发明授权
    Si-killed steel wire rod and spring excellent in fatigue properties 有权
    Si杀死钢丝绳和弹簧疲劳性能优异

    公开(公告)号:US09062361B2

    公开(公告)日:2015-06-23

    申请号:US12520993

    申请日:2007-12-03

    摘要: A Si-killed steel wire rod for obtaining a spring excellent in fatigue properties and a spring excellent in fatigue properties obtained from the steel wire rod are provided.The Si-killed steel wire rod of the present invention contains Sr: 0.03-20 ppm (means “mass ppm”, hereinafter the same), Al: 1-30 ppm and Si: 0.2-4% (means “mass %”, hereinafter the same) respectively, and contains Mg and/or Ca by a range of 0.5-30 ppm in total.Also, in the Si-killed steel wire rod of the present invention, oxide-based inclusions present in the wire rod contain SiO2: 30-90%, Al2O3: 2-50%, MgO: 35% or below (not inclusive of 0%), CaO: 50% or below (not inclusive of 0%), MnO: 20% or below (not inclusive of 0%) and SrO: 0.2-15% respectively, and total content of (CaO+MgO) is 3% or above.A spring excellent in fatigue properties can be obtained by forming the spring from such steel wire rod.

    摘要翻译: 提供了一种用于获得疲劳特性优异的弹簧和由钢丝棒获得的疲劳特性优异的弹簧的Si镇静钢线材。 本发明的Si镇静钢线材含有Sr:0.03〜20ppm(以下相同的质量ppm),Al:1-30ppm,Si:0.2〜4%(意指“质量%”, 以下相同),并且含有总共0.5-30ppm范围的Mg和/或Ca。 此外,在本发明的Si镇静钢线材中,线材中存在的氧化物系夹杂物含有SiO 2:30〜90%,Al 2 O 3:2-50%,MgO:35%以下(不包括0 %),CaO:50%以下(不包括0%),MnO:20%以下(不包括0%)和SrO:0.2〜15%,(CaO + MgO)的总含量为3 %或以上。 通过从这种钢丝线形成弹簧可以获得疲劳性能优异的弹簧。

    SI-KILLED STEEL WIRE ROD AND SPRING EXCELLENT IN FATIGUE PROPERTIES
    100.
    发明申请
    SI-KILLED STEEL WIRE ROD AND SPRING EXCELLENT IN FATIGUE PROPERTIES 有权
    SI-KILLED钢丝绳和弹簧在疲劳性能方面优秀

    公开(公告)号:US20100098577A1

    公开(公告)日:2010-04-22

    申请号:US12520993

    申请日:2007-12-03

    摘要: A Si-killed steel wire rod for obtaining a spring excellent in fatigue properties and a spring excellent in fatigue properties obtained from the steel wire rod are provided.The Si-killed steel wire rod of the present invention contains Sr: 0.03-20 ppm (means “mass ppm”, hereinafter the same), Al: 1-30 ppm and Si: 0.2-4% (means “mass %”, hereinafter the same) respectively, and contains Mg and/or Ca by a range of 0.5-30 ppm in total.Also, in the Si-killed steel wire rod of the present invention, oxide-based inclusions present in the wire rod contain SiO2: 30-90%, Al2O3: 2-50%, MgO: 35% or below (not inclusive of 0%), CaO: 50% or below (not inclusive of 0%), MnO: 20% or below (not inclusive of 0%) and SrO: 0.2-15% respectively, and total content of (CaO+MgO) is 3% or above.A spring excellent in fatigue properties can be obtained by forming the spring from such steel wire rod.

    摘要翻译: 提供了一种用于获得疲劳特性优异的弹簧和由钢丝棒获得的疲劳特性优异的弹簧的Si镇静钢线材。 本发明的Si镇静钢线材含有Sr:0.03〜20ppm(以下相同的质量ppm),Al:1-30ppm,Si:0.2〜4%(意指“质量%”, 以下相同),并且含有总共0.5-30ppm范围的Mg和/或Ca。 此外,在本发明的Si镇静钢线材中,线材中存在的氧化物系夹杂物含有SiO 2:30〜90%,Al 2 O 3:2-50%,MgO:35%以下(不包括0 %),CaO:50%以下(不包括0%),MnO:20%以下(不包括0%)和SrO:0.2〜15%,(CaO + MgO)的总含量为3 %或以上。 通过从这种钢丝线形成弹簧可以获得疲劳性能优异的弹簧。