摘要:
An aluminum sheet material for automobiles is herein disclosed, having an aluminum alloy composition: (i) comprising 3.5 to 5 wt % of Si, 0.3 to 1.5 wt % of Mg, 0.4 to 1.5 wt % of Zn, 0.4 to 1.5 wt % of Cu, 0.4 to 1.5 wt % of Fe, and 0.6 to 1 wt % of Mn, and one or more members selected from the group of 0.01 to 0.2 wt % of Cr, 0.01 to 0.2 wt % of Ti, 0.01 to 0.2 wt % of Zr, and 0.01 to 0.2 wt % of V, with the balance of aluminum and unavoidable impurities, or (ii) comprising between more than 2.6 wt % and 5 wt % of Si, 0.2 to 1.0 wt % of Mg, 0.2 to 1.5 wt % of Zn, 0.2 to 1.5 wt % of Cu, 0.2 to 1.5 wt % of Fe, and between 0.05 and less than 0.6 wt % of Mn, and one or more members selected from the group of 0.01 to 0.2 wt % of Cr, 0.01 to 0.2 wt % of Ti, 0.01 to 0.2 wt % of Zr, and 0.01 to 0.2 wt % of V, with the balance of aluminum and unavoidable impurities. It is possible to produce an aluminum sheet material for automobiles that has excellent mechanical strength and bending property as well as enhanced weldability, by making the recycling use of recycled aluminum materials.
摘要:
A method including preparing an aluminum scrap containing a total of about 0.3 to 2.0 wt % of Fe and Si; melting and then adjusting the material composition so as to attain an Mg content of about 3 to 10 wt % or a composition further containing at least one of the elements Cu, Mn, Cr, Zr and Ti, each in the amount of 0.02 to 0.5 wt %; subjecting the material to casting, hot rolling, cold rolling and continuous annealing to obtain an aluminum alloy sheet having a tensile strength of about 31 kgf/mm.sup.2 or more; and applying a lubricant surface coating to impart a coefficient of friction of not more than about 0.11.
摘要翻译:一种包括制备总计约0.3-2.0重量%的Fe和Si的铝屑的方法; 熔化,然后调整材料组成以获得约3至10重量%的Mg含量或进一步含有至少一种元素Cu,Mn,Cr,Zr和Ti的组成,其量为0.02至0.5 重量% 对该材料进行铸造,热轧,冷轧和连续退火,得到拉伸强度为约31kgf / mm 2以上的铝合金板; 并施加润滑剂表面涂层以赋予不大于约0.11的摩擦系数。
摘要:
An aluminum alloy brazing sheet having a core material of an aluminum alloy, and a filler material cladded on the core is disclosed. The core material is an aluminum alloy having about 0.05 to about 1.2 mass Si, about 0.05-about 1.0 mass % Fe, about 0.05-about 1.2 mass % Cu, and about 0.6-about 1.8 mass % Mn, balance Al and the inevitable impurities. The filler material includes an aluminum alloy having about 2.5-about 13.0 mass % Si. Also, there is provided a method of manufacturing such an aluminum alloy brazing sheet.
摘要:
An aluminum alloy brazing sheet having high strength comprising:a core alloy; an Al—Si-based filler alloy cladded on one side or both sides of the core alloy, wherein the core alloy is composed of an aluminum alloy containing 0.3-1.2% (mass %, the same applies the below) Si, 0.05-0.4% Fe, 0.3-1.2% Cu, 0.3-1.8% Mn, 0.05-0.6% Mg, and containing one or more elements selected from the group consisting of 0.02-0.3% Ti, 0.02-0.3% Zr, 0.02-0.3% Cr and 0.02-0.3% V, the balance of Al and unavoidable impurities; and wherein, after the aluminum alloy brazing sheet is subjected to brazing, the core alloy features a metallic structure in which a density of intermetallic compounds having a grain diameter of at least 0.1 μm is at most ten grains per μm2.
摘要:
An aluminum alloy brazing sheet having high strength comprising:a core alloy; an Al—Si-based filler alloy cladded on one side or both sides of the core alloy, wherein the core alloy is composed of an aluminum alloy containing 0.3-1.2% (mass %, the same applies the below) Si, 0.05-0.4% Fe, 0.3-1.2% Cu, 0.3-1.8% Mn, 0.05-0.6% Mg, and containing one or more elements selected from the group consisting of 0.02-0.3% Ti, 0.02-0.3% Zr, 0.02-0.3% Cr and 0.02-0.3% V, the balance of Al and unavoidable impurities; and wherein, after the aluminum alloy brazing sheet is subjected to brazing, the core alloy features a metallic structure in which a density of intermetallic compounds having a grain diameter of at least 0.1 μm is at most ten grains per μm2.
摘要翻译:一种具有高强度的铝合金钎焊片,包括:芯合金; 在芯合金的一侧或两面上包覆的Al-Si系填充合金,其中,所述芯合金由含有0.3〜1.2%(质量%,以下相同)Si,0.05〜0.4 %Fe,0.3-1.2%Cu,0.3-1.8%Mn,0.05-0.6%Mg,并且含有一种或多种选自0.02-0.3%Ti,0.02-0.3%Zr,0.02-0.3%Cr 和0.02-0.3%V,余量为Al和不可避免的杂质; 在铝合金钎焊片进行钎焊之后,芯合金的特征在于,具有至少0.1μm的粒径的金属间化合物的密度至多为10个/ m 2的金属结构。
摘要:
Disclosed is an Al alloy for a welded construction having excellent welding characteristics, which Al alloy comprises 1.5 to 5 wt % of Si (hereinafter, wt % is referred to as %), 0.2 to 1.5% of Mg, 0.2 to 1.5% of Zn, 0.2 to 2% of Cu, 0.1 to 1.5% of Fe, and at least one member selected from the group consisting of 0.01 to 1.0% of Mn, 0.01 to 0.2% of Cr, 0.01 to 0.2% of Ti, 0.01 to 0.2% of Zr, and 0.01 to 0.2% of V, with the balance being Al and inevitable impurities. Also disclosed is a welded joint having this Al alloy base metal welded with an Al—Mg- or Al—Si-series filler metal.
摘要:
There is disclosed a method of producing an aluminum alloy for automotive parts, comprising adding a scrap of an aluminum wrought alloy or a pure aluminum ingot to an aluminum alloy casting scrap, melting the mixture to dilute impurities, and if necessary, adjusting elements of the resultant. According to the above method, aluminum alloy casting scraps, which contain large amounts of impurities and have been difficult to recycle into other articles until now, can be converted to an aluminum alloy material that is applicable as a wrought material usable as a higher-grade material.
摘要:
A method for manufacturing an aluminum alloy sheet for use in a body panel material, comprising: (a) casting a melted aluminum alloy containing Al, Mg, Fe, Mn, Cr, Ti and Zr, having a Mg content of 4 to 10 weight %, and having contents of Fe, Mn, Cr, Ti and Zr which are determined by a value f satisfying the following equation (I), and the balance being Al: 0.4 wt %.ltoreq.f.ltoreq.1.5 wt % (I), wherein, f=(Fe)+1.1 (Mn)+1.1 (Cr)+3 (Ti)+3 (Zr), wherein (Fe), (Mn), (Cr), (Ti), and (Zr) respectively represent the percentage content by weight of Fe, Mn, Cr, Ti and Zr, to form an ingot; (b) hot rolling the ingot to obtain a hot rolled sheet; (c) cold rolling the hot rolled sheet at a cold reduction R satisfying the following equation (II): -log(f-0.2)+8.ltoreq.R.ltoreq.-60 log (f-0.2)+50 (II) to obtain a cold rolled sheet; (d) subjecting the cold rolled sheet to a final annealing treatment including raising the temperature of the rolled sheet to 450.degree. to 550.degree. C. at a rate of 100.degree. C./minute or more, and maintaining the attained temperature for 300 seconds or less; and (e) cooling the annealed rolled sheet at a cooling rate of 100.degree. C./minute or more to obtain an aluminum alloy sheet having a grain size of 20 and 80 .mu.m.
摘要:
A process for producing high Mg content Al-Mg alloy sheet for press forming having a high tensile strength and formability. The maximum grain diameter of the alloy slab is less than 1000 .mu.m. The process consists of the steps of forming the slab, homogenizing, hot rolling, cold rolling and annealing. The composition of the alloy is disclosed as having the elements of Al, Mg, Be, B, Cu, Ti, Si as major components, the balance being inevitable impurities.