摘要:
The present invention provides a grain-oriented electrical steel sheet product having a superior corrosion resistance, annealing resistance, film tension, and the like in insulating treatment based on a phosphate not containing chromium and a treatment agent for the same, so provides grain-oriented electrical steel sheet having an insulating film not containing chromium characterized by the insulating film containing a phosphate and one or more compounds selected from inorganic compounds of Fe, Ni, Co, Cu, Sr, and Mo in an amount, as metal elements, of 0.06 to 2.10 moles per mole of phosphate, and an insulating film agent of the same.
摘要:
The present invention is a grain-oriented electrical steel sheet characterized in that Bi is present at 0.01 to less than 1,000 ppm in terms of mass at the interface of the substrate steel and the primary film of the grain-oriented electrical steel sheet. The grain-oriented electrical steel sheet is produced by any of the processes of: before decarburization annealing, applying preliminary annealing for 1 to 20 sec. at 700° C. or higher and controlling an atmosphere in the temperature range; controlling the maximum attaining temperature B (° C.) before final cold rolling so that the maximum attaining temperature B may satisfy the expression, −10×ln(A)+1,100≦B≦10×ln(A)+1,220, in accordance with a Bi content A (ppm) and at the same time heating the steel sheet cold rolled to the final thickness to 700° C. or higher within 10 sec. or at a heating rate of 100° C./sec. or more before decarburization annealing, or immediately thereafter applying preliminary annealing for 1 to 20 sec. at 700° C. or higher; or controlling a TiO2 amount B added in relation to MgO of 100 as parts by weight and an MgO coating amount C (g/m2) so that the expression, A0.8≦B×C≦400, may be satisfied in accordance with the Bi content A (ppm).
摘要:
The present invention is a grain-oriented electrical steel sheet characterized in that Bi is present at 0.01 to less than 1,000 ppm in terms of mass at the interface of the substrate steel and the primary film of the grain-oriented electrical steel sheet. The grain-oriented electrical steel sheet is produced by any of the processes of: before decarburization annealing, applying preliminary annealing for 1 to 20 sec. at 700° C. or higher and controlling an atmosphere in the temperature range; controlling the maximum attaining temperature B (° C.) before final cold rolling so that the maximum attaining temperature B may satisfy the expression, −10×ln(A)+1,100≦B≦10×ln(A)+1,220, in accordance with a Bi content A (ppm) and at the same time heating the steel sheet cold rolled to the final thickness to 700° C. or higher within 10 sec. or at a heating rate of 100° C./sec. or more before decarburization annealing, or immediately thereafter applying preliminary annealing for 1 to 20 sec. at 700° C. or higher; or controlling a TiO2 amount B added in relation to MgO of 100 as parts by weight and an MgO coating amount C (g/m2) so that the expression, A0.8≦B×C≦400, may be satisfied in accordance with the Bi content A (ppm).
摘要翻译:本发明是一种方向性电磁钢板,其特征在于,所述Bi在基板钢与晶粒取向电工钢板的一次膜的界面处的质量比为0.01〜小于1,000ppm。 晶粒取向电工钢板通过以下任一方法制造:在脱碳退火之前,进行1〜20秒的预退火。 在700℃以上,控制温度范围内的气氛; 控制最终冷轧前的最大达到温度B(℃),使得最大达到温度B可以满足以下表达式:-10×ln(A)+1,100 <= B <= 10×ln(A)+1,220,根据 Bi含量A(ppm),同时在10秒内将钢板冷轧至最终厚度至700℃以上。 或加热速率为100℃/秒。 或更多的脱碳退火之前,或者之后立即进行1〜20秒的预退火。 在700℃以上; 或控制相对于MgO为100重量份的TiO 2 B量和MgO涂布量C(g / m 2 O 2),使得表达式A 根据Bi含量A(ppm)可以满足0.8≤BxC≤400。
摘要:
The present invention is a grain-oriented electrical steel sheet characterized in that Bi is present at 0.01 to less than 1,000 ppm in terms of mass at the interface of the substrate steel and the primary film of the grain-oriented electrical steel sheet. The grain-oriented electrical steel sheet is produced by any of the processes of: before decarburization annealing, applying preliminary annealing for 1 to 20 sec. at 700° C. or higher and controlling an atmosphere in the temperature range; controlling the maximum attaining temperature B (° C.) before final cold rolling so that the maximum attaining temperature B may satisfy the expression, −10×ln(A)+1,100≦B≦10×ln(A)+1,220, in accordance with a Bi content A (ppm) and at the same time heating the steel sheet cold rolled to the final thickness to 700° C. or higher within 10 sec. or at a heating rate of 100° C./sec. or more before decarburization annealing, or immediately thereafter applying preliminary annealing for 1 to 20 sec. at 700° C. or higher; or controlling a TiO2 amount B added in relation to MgO of 100 as parts by weight and an MgO coating amount C (g/m2) so that the expression, A0.8≦B×C≦400, may be satisfied in accordance with the Bi content A (ppm).
摘要:
An electrical steel sheet (10) is provided with a base iron (1) and an insulating film (2) formed on a surface of the base iron (1). The insulating film (2) contains: a first component: 100 parts by mass, the first component containing: a metal phosphate: 100 parts by mass; and one kind selected from a group consisting of an acrylic resin, an epoxy resin and a polyester resin which have an average particle size of 0.05 μm to 0.50 μm, or a mixture or copolymer of two or three kinds selected from the group: 1 part by mass to 50 parts by mass; and a second component composed of dispersion or powder of a fluorine resin having an average particle size of 0.05 μm to 0.35 μm: 0.5 parts by mass to 10 parts by mass.
摘要:
An insulating coating film obtained by mixing 0.5 parts by mass to 10 parts by mass of a copolymer of a fluoroolefin and an ethylenically unsaturated compound when converted into a solid content with 100 parts by mass in solid content of a mixture composed of a metal phosphate and a specific organic resin or a mixture composed of colloidal silica and a specific organic resin is designed to be provided on a surface of an electrical steel sheet, and in this manner, it is possible to obtain an electrical steel sheet having good corrosion resistance under a wet environment and having good properties related to the insulating coating film such as a space factor and adhesiveness.
摘要:
The invention relates to a timepiece which has a resin substrate, rotors, and wheel trains, and relates to a wheel train apparatus which has a resin substrate, bearing members, gear wheel, and the like. The invention is constituted by a timepiece comprising; a gear wheel, and a substrate which supports a shaft of a rotor and/or a shaft of the gear wheel, the substrate being formed from a filled resin. Alternatively the invention is constituted by a wheel train apparatus comprising: a gear wheel; a substrate which supports one shaft section of the gear wheel, and a bridge which rotatably supports an other shaft section of the gear wheel, the substrate and the bridge being formed from a filled resin.
摘要:
The invention relates to a timepiece which has a resin substrate, rotors, and wheel trains, and relates to a wheel train apparatus which has a resin substrate, bearing members, gear wheel, and the like. The invention is constituted by a timepiece comprising; a gear wheel, and a substrate which supports a shaft of a rotor and/or a shaft of the gear wheel, the substrate being formed from a filled resin. Alternatively the invention is constituted by a wheel train apparatus comprising: a gear wheel; a substrate which supports one shaft section of the gear wheel, and a bridge which rotatably supports an other shaft section of the gear wheel, the substrate and the bridge being formed from a filled resin.
摘要:
Escalator apparatus of the invention is of the type that has a step whose step board can be raised to provide a surface for carrying a wheelchair. In order to realize conveyance of a large size wheelchair or handcart without changing the installation space for the escalator, the escalator apparatus of the invention is structured such that the step boards of a plurality of adjacent steps are movable upwardly and downwardly.
摘要:
A non-contact power supply system is provided in which current phases of induction lines are matched. According to the output current of a power supply unit (21) and the power consumption of induction lines (19), a lead time corresponding to a phase difference between the output currents of the induction lines is determined. A signal for driving transistors (52) is advanced ahead of a drive synchronization signal (β) according to the lead time.