Method for manufacturing high toughness sintered bodies
    13.
    发明授权
    Method for manufacturing high toughness sintered bodies 失效
    制造高韧性烧结体的方法

    公开(公告)号:US4626518A

    公开(公告)日:1986-12-02

    申请号:US610459

    申请日:1984-07-11

    摘要: A method for manufacture of a high toughness sintered body, characterized by sintering a shaped body of a mixed powder consisting essentially of from 40 to 70% by weight of a first component of powdered ZrO.sub.2 containing at least one stabilizer selected from the group consisting of Y.sub.2 O.sub.3, CaO, and MgO and having an average particle diameter of not more than 1.mu. and from 30 to 60% by weight of a second component of powdered .alpha.-Al.sub.2 O.sub.3 having an average particle diameter of not more than 1 .mu.m, which mixed powder may also contain not more than 3% by weight of SiO.sub.2, not more than 0.5% by weight of Fe.sub.2 O.sub.3, or not more than 0.5% by weight of TiO.sub.2 in a combined proportion of not more than 3% by weight at a temperature in the range of from 1400.degree. C. to 1600.degree. C. under normal pressure thereby producing a sintered body wherein at least 90% by weight of ZrO.sub.2 particles present therein are accounted for by tetragonal and cubic crystals, the ratio of said tetragonal crystals to said cubic crystals is at least 1:3, and the average crystal particle diameter of the entire sintered body is at least 3.mu..

    摘要翻译: 一种制造高韧性烧结体的方法,其特征在于,烧结混合粉末的成形体,所述混合粉末主要由40至70重量%的含有至少一种选自Y 2 O 3的稳定剂的粉末状ZrO 2的第一组分组成, CaO,MgO,平均粒径为1μm以下,平均粒径为1μm以下的粉末状α-Al2O3粉末的第二成分的平均粒径为1〜30重量%,混合粉末 还可以含有不超过3重量%的SiO 2,不超过0.5重量%的Fe 2 O 3,或不超过0.5重量%的TiO 2,其组合比例不超过3重量% 范围在常压下为1400℃至1600℃,从而生产烧结体,其中存在至少90重量%的存在于其中的ZrO 2颗粒为四方晶体和立方晶体,所述四方晶体与所述立方晶体的比率 结晶 Als至少为1:3,整个烧结体的平均晶粒直径至少为3微米。

    Data processing device and method for memory dump collection
    15.
    发明授权
    Data processing device and method for memory dump collection 有权
    数据处理设备和内存转储收集方法

    公开(公告)号:US08489933B2

    公开(公告)日:2013-07-16

    申请号:US13094071

    申请日:2011-04-26

    IPC分类号: G06F11/00

    CPC分类号: G06F11/0778

    摘要: A data processing device for memory dump collection, the data processing device includes: a processor to issue a first interrupt upon instructions to collect a memory dump being entered, to issue a second interrupt for running a program put in an address indicated by a reset vector upon the first interrupt being issued, and to record the memory dump in a storage unit in a process of running the program upon the second interrupt being issued.

    摘要翻译: 一种用于存储器转储收集的数据处理装置,所述数据处理装置包括:处理器,用于在收集正在输入的存储器转储的指令时发出第一中断,以发出第二中断,用于运行放置在由复位向量指示的地址中的程序 在发出第一个中断时,并且在发出第二个中断时运行程序的过程中将存储器转储记录在存储单元中。

    Method for forming coated film and intermediate coating material
    16.
    发明授权
    Method for forming coated film and intermediate coating material 有权
    涂膜和中间涂层材料的形成方法

    公开(公告)号:US06863929B2

    公开(公告)日:2005-03-08

    申请号:US10347270

    申请日:2003-01-21

    摘要: A method for forming a coated film comprising the steps of sequentially applying an intermediate coating material, a base coating material and a clear coating material on a substrate on which an electrodeposition coated film has been formed; and simultaneously curing the applied three layers by baking, wherein the intermediate coating material comprises: (a) 40 to 56% by weight of an urethane modified polyester resin, the urethane modified polyester resin being obtainable by polyaddition of: a hydroxyl group containing polyester resin which is obtainable by polycondensation of an acid ingredient including not less than 80% by mole of isophthalic acid with a polyhydric alcohol ingredient, with an aliphatic diisocyanate compound; (b) 10 to 30% by weight of a melamine resin; (c) 15 to 30% by weight of a blocked isocyanate compound; (d) 4 to 15% by weight of a nonaqueous dispersion resin having core-shell structure; and (e) 0.4 to 2 parts by weight of a flake-like pigment. The resulting layered coated film is superior in aesthetic appearance and chipping resistance even formed in the three-coating and one-baking method.

    摘要翻译: 一种形成涂膜的方法,包括以下步骤:在其上形成有电沉积涂膜的基材上顺次涂布中间涂料,基涂料和透明涂料; 同时通过烘烤固化所施加的三层,其中中间涂层材料包括:(a)40至56重量%的氨基甲酸酯改性聚酯树脂,所述聚氨酯改性聚酯树脂可通过以下方式加成获得:含羟基的聚酯树脂 其可以通过使含有不少于80摩尔%的间苯二甲酸与多元醇成分的酸成分与脂肪族二异氰酸酯化合物缩聚而得到; (b)10〜30重量%的三聚氰胺树脂; (c)15〜30重量%的封端异氰酸酯化合物; (d)4〜15重量%的具有核 - 壳结构的非水分散体树脂; 和(e)0.4〜2重量份的片状颜料。 所得到的层状涂膜在三层涂布和一次烘烤方法中甚至形成的美观性和耐崩裂性优异。

    Assembly process apparatus
    17.
    发明授权
    Assembly process apparatus 有权
    装配工艺装置

    公开(公告)号:US06256868B1

    公开(公告)日:2001-07-10

    申请号:US09292332

    申请日:1999-04-15

    IPC分类号: B23P2100

    摘要: An assembly process apparatus includes an assembly robot for assembling parts to a workpiece which is a main body, a part supply apparatus for supplying parts to the workpiece, a work pallet for supplying workpieces to an assembly station of the assembly robot, and a tool pallet for supplying assembly process modules interchangeable with respect to the assembly robot. The part supply apparatus is made up of a plurality of part supply modules interchangeable with respect to the assembly robot. With the assembly process apparatus as one unit, it is constructed to assemble parts one unit only or with a plurality of units combined. Accordingly, an assembly process apparatus achieves excellent productivity with which it is possible to expand or cut line equipments easily according to production volume, and it is possible to achieve utilization of surplus assembly robots.

    摘要翻译: 组装工艺装置包括:组装机器人,用于将零件组装到作为主体的工件上,用于向工件供应零件的零件供应装置,用于将工件供给到组装机器人的组装工位的工件托盘,以及工具托盘 用于提供相对于组装机器人可互换的组装过程模块。 零件供应装置由相对于组装机器人可互换的多个部件供应模块组成。 以组装处理装置作为一个单元,它被构造为仅组装一个单元或者组合多个单元。 因此,组装处理装置实现了优异的生产率,通过该生产率可以根据生产量容易地扩大或切割生产线,并且可以实现多余的组装机器人的利用。

    TiC-base/SiC whisker composite ceramic cutting tools
    19.
    发明授权
    TiC-base/SiC whisker composite ceramic cutting tools 失效
    TiC基/ SiC晶须复合陶瓷切割工具

    公开(公告)号:US5439854A

    公开(公告)日:1995-08-08

    申请号:US131571

    申请日:1993-10-04

    IPC分类号: C04B35/56 C22C29/10

    摘要: A ceramic cutting tool formed of a TiC-based sintered body contains 40 wt % or more of TiC, and 5 to 40 wt % of SiC whisker uniformly dispersed in the sintered body. The SiC whisker has a diameter of 0.2-1.5 .mu.m and a length of 1-20 .mu.m. The sintered body may contain up to 40 wt % of Al.sub.2 O.sub.3, and further sintering aids. Up to 40% by weight of the TiC may be substituted with at least one of Ti, nitrides, oxides and borides of Ti, and solid-solutions of these nitrides, oxides and borides of Ti to form a TiC-base composition. The TiC base composition may be represented by the formula (Ti.sub.a M.sub.b) (C.sub.c N.sub.d O.sub.e B.sub.f).sub.g, in which M denotes at least one transition metal element of Groups IVa, Va and VIa according to the International Periodic Table, except Ti; and a+b=1, 0

    摘要翻译: 由TiC系烧结体形成的陶瓷切削工具包含40重量%以上的TiC和5〜40重量%的均匀分散在烧结体中的SiC晶须。 SiC晶须的直径为0.2-1.5μm,长度为1-20μm。 该烧结体可含有至多40重量%的Al 2 O 3,以及其它烧结助剂。 高达40重量%的TiC可以被Ti的Ti,氮化物,氧化物和硼化物中的至少一种,Ti的这些氮化物,氧化物和硼化物的固溶体代替,以形成TiC基组合物。 TiC基础组合物可以由式(TiaMb)(CcNdOeBf)g表示,其中M表示除了Ti之外,根据国际周期表的至少一种IVa,Va和VIa族的过渡金属元素; 和a + b = 1,0,0

    Diamond-coated bodies and process for preparation thereof
    20.
    发明授权
    Diamond-coated bodies and process for preparation thereof 失效
    金刚石涂层体及其制备方法

    公开(公告)号:US5334453A

    公开(公告)日:1994-08-02

    申请号:US905199

    申请日:1992-06-26

    摘要: A diamond-coated body is prepared by coating a diamond film on the surface of a sintered body by means of vapor phase synthesis, the sintered body being so prepared by subjecting a sintered body prepared from ceramics based on silicon nitride to heat treatment at the temperature of 1,400.degree. C. to 1,700.degree. C. as to give a crystalline intergranular phase. The resulting diamond-coated body has excellent adhesion between the diamond film and the substrate and it is appropriately employed for cutting tools and so on because, when applied to the cutting tools, they can be used for cutting for a long period of time.

    摘要翻译: 通过气相合成在烧结体的表面上涂布金刚石膜来制备金刚石涂层体,该烧结体通过将由氮化硅制成的陶瓷制成的烧结体在温度下进行热处理 1400℃至1700℃,以产生结晶晶间相。 所得到的金刚石涂层体在金刚石膜和基材之间具有优异的粘合性,并且适用于切削工具等,因为当应用于切削工具时,它们可以长时间地切割。