Abstract:
A composite film including a base film including a polyimide or poly(imide-amide) copolymer and a coating layer including a copolymer represented by Chemical Formula 1 disposed on one surface of the base film: wherein, in the Chemical Formula 1, each substituent and variable is the same as described in the detailed description.
Abstract:
An optical filter includes a near-infrared absorbing layer including a first material, the first material being configured to absorb light in a first wavelength spectrum belonging to a near-infrared wavelength spectrum. The optical filter includes a compensation layer adjacent to the near-infrared absorbing layer, the compensation layer including a second material different from the first material. The optical filter includes a metamaterial structure spaced apart from the near-infrared absorbing layer via the compensation layer, the metamaterial structure being configured to absorb or reflect light in a second wavelength spectrum at least partially overlapped with the first wavelength spectrum.
Abstract:
A laminate includes a substrate, a self-healing layer on the substrate and having a thickness of greater than or equal to about 50 micrometers, a protective layer between the substrate and the self-healing layer, and a surface layer on the self-healing layer and having a thickness of about 20 nanometers to about 300 nanometers, wherein the self-healing layer has a first elastic modulus and the protective layer has a second elastic modulus, wherein the second elastic modulus is about 1.2 times to about 50 times greater than the first elastic modulus, and wherein the surface layer has a friction coefficient of less than or equal to about 1.
Abstract:
A combination structure includes a hybrid nanostructure array and a light-absorbing layer adjacent to the hybrid nanostructure array. The hybrid nanostructure array includes a plurality of hybrid nanostructures, each hybrid nanostructure includes a stack of a first nanostructure and a second nanostructure. The first nanostructure includes a first material. The second nanostructure includes a second material. The second material has a refractive index that is higher than a refractive index of the first material. The light-absorbing layer includes a near-infrared absorbing material configured to absorb light of at least a portion of a near-infrared wavelength spectrum.
Abstract:
A self-healing composition including, urethane (meth)acrylate having two (meth)acrylate groups, six or more urethane groups, and a substituted or unsubstituted polyhedral silsesquioxane.
Abstract:
A poly(imide-amide) copolymer, which is a product of a reaction between a diamine and a dianhydride, wherein the diamine comprises a diamine represented by Chemical Formula 1 and the dianhydride comprises a dianhydride represented by Chemical Formula 5: wherein, the variables in Chemical Formulae 1 and 5 are described in the specification.
Abstract:
A material for an optical film including a compound represented by Chemical Formula 1; a polymer including a repeating unit represented by Chemical Formula 10; a polymer including a repeating unit represented by Chemical Formula 20 and a repeating unit represented by Chemical Formula 21; an article prepared by using the polymer; and a display device including the article:
Abstract:
Disclosed are a combination structure including a nanostructure array including a plurality of nanostructures with a smaller dimension than the near-infrared wavelength are repeatedly arranged and a light absorption portion adjacent to the nanostructure array and including a near-infrared absorbing material configured to absorb light in at least a portion of near-infrared wavelength regions, an optical filter, an image sensor, a camera module, and an electronic device including the same.
Abstract:
A laminate includes a substrate, a self-healing layer on the substrate and having a thickness of greater than or equal to about 50 micrometers, a protective layer between the substrate and the self-healing layer, and a surface layer on the self-healing layer and having a thickness of about 20 nanometers to about 300 nanometers, wherein the self-healing layer has a first elastic modulus and the protective layer has a second elastic modulus, wherein the second elastic modulus is about 1.2 times to about 50 times greater than the first elastic modulus, and wherein the surface layer has a friction coefficient of less than or equal to about 1.
Abstract:
A composition for preparing a polyimide-inorganic composite material including: a polyamic acid represented by Chemical Formula 1, a polyimide represented by Chemical Formula 2, or a combination thereof; an inorganic particle precursor; and water, wherein the polyamic acid, the polyimide, or the combination thereof is a reaction product of a dicarboxylic acid anhydride and a diamine, wherein the mole ratio of the diamine to the dicarboxylic acid anhydride is greater than 0.93 and less than 0.95, and wherein the inorganic particle precursor is included in an amount to provide an inorganic particle in an amount of greater than or equal to about 30 weight % and less than or equal to about 60 weight % based the total weight of the polyimide-inorganic composite material prepared: wherein in Chemical Formulae 1, 2, and 3, groups and variable are defined in the specification.