摘要:
Pyrogenically produced aluminum oxide, in which the BET specific surface area is greater than 115 m2/g and the Sears index is over 8 ml/2 g and the dibutyl phthalate absorption as a powder measured with a 16 g weighed portion is not measurable, is produced by means of flame oxidation or preferably flame hydrolysis, whereby a vaporizable aluminum compound is used as starting material. The aluminum oxide can be used as an ink-absorbing substance in inkjet media and also as a filler, as a substrate, as a catalytically active substance, as a starting material for the production of dispersions, as a polishing material (CMP applications), as a ceramic raw material, in the electronics industry, in the cosmetics industry, as an additive in the silicone and rubber industry, to adjust the rheology of liquid systems, as a heat stabilizer, in the paint industry.
摘要:
A pyrogenic process is used to prepare alkali-doped silica particles. Particles produced by this process exhibit homogeneous doping, reduced agglomeration, greater stability and higher removal rates. Aqueous dispersions containing alkali-doped pyrogenic silica with average particle size less than 100 nm are used for polishing surfaces (CMP).
摘要:
Pyrogenically prepared silica doped with silver or silver oxide is prepared by feeding an aerosol into a flame such as is used for the preparation of pyrogenic silica, mixing the aerosol homogeneously with gas mixture before the reaction, then allowing the aerosol/gas mixture to react in a flame. The resulting pyrogenic silicas doped with silver or silver oxide are separated from the gas stream. The pyrogenic silica doped with silver or silver oxide by means of an aerosol can be used as a bactericidal filler.
摘要:
Stable, pourable silicon dioxide dispersion, in which the average, number-related aggregate diameter of the silicon dioxide particles in dispersion is less than 200 nm, and which comprises at least 35 wt. % of a silicon dioxide powder, 3 to 35 wt. % of at least one polyol, 20 to 60 wt. % of water, 0 to 10 wt. % of an additive and a substance having an alkaline action in an amount such that a pH of 10
摘要:
Pyrogenically produced silicon dioxide doped with aluminum oxide by means of an aerosol is produced by introducing an aqueous aerosol of an aluminum salt into the flame of a pyrogenic silica producing flame hydrolysis method or a flame oxidation method. The silicon dioxide doped with Al2O3 by means of an aerosol may inter alia be used in the production of inkjet paper or inkjet films.
摘要:
Silicon-titanium mixed oxide powder, dispersion thereof and titanium-containing zeolite prepared therefrom Pyrogenic silicon-titanium mixed oxide powder, having a BET surface area of 200 to 400 m2/g, a silicon dioxide content of 97.0±1.5% by weight, a titanium dioxide content of 3.5±1.0% by weight, the sum of silicon dioxide content and titanium dioxide content being greater than 99.7% by weight.Dispersion comprising this powder.Process for the preparation of a titanium-containing zeolite starting from powder or dispersion.
摘要:
Alkali metal oxide-metal oxide mixed oxide powder in the form of aggregates of pore-free primary particles, comprising from 0.005 to 5% by weight of at least one alkali metal oxide, which has a BET surface area of from 100 to 350 m/g, has a specific DBP number, expressed as DBP number per square metre of specific surface area, greater than or equal to that of a powder which has only the metal oxide component, has the alkali metal oxide distributed in the core and on the surface of the primary particles. Silicone rubber comprising the alkali metal oxide-metal oxide mixed oxide powder.
摘要:
Carbon black with an OAN, measured on the beaded carbon black, of less than 120 ml/100 g. A process for the preparation of the carbon black is described, wherein a salt solution is converted into an aerosol and this is then introduced into the carbon black formation zone. The carbon black can be used in inks, paints, lacquers, printing inks and ink-jet inks, and for coloring plastics.
摘要:
Moldings based on pyrogenically produced mixed oxide having the following physicochemical parameters: External diameter 0.8-25 mm BET surface area 5-400 m2/g Pore Volume 0.2-1.8 ml/g Fracture strength 5 to 350 N Composition At least two oxides selected from the group SiO2, Al2O3, TiO 2 and ZrO2 in any desired combination but with the exception of SiO2/Al2O3 mixed oxides, in which > 75 wt. % of SiO2 is present. Other constituents
摘要:
The present invention relates to an aqueous dispersion containing a silicon dioxide powder coated with cerium oxide. In addition, the present invention provides a method of producing an aqueous dispersion containing a silicon dioxide powder coated with cerium oxide and methods of using this aqueous dispersion for chemical-mechanical polishing.