摘要:
The present invention relates to a paper or paperboard substrate having barrier properties which substrate comprises a first fiber based layer, a second layer comprising microfibrillated cellulose and a third layer comprising a polymer. The invention further relates to a process for the production of said substrate and a package formed of said substrate.
摘要:
A process for producing microfibrillated cellulose comprises providing a slurry comprising cellulosic fibers, treating the slurry with an enzyme, mechanically treating the slurry so that the fibers are disintegrated wherein the mechanical treatment and the treatment with the enzyme is performed simultaneously in a single treatment step. In this way it is possible to produce microfibrillated cellulose (MFC) in an improved and energy efficient way. A microfibrillated cellulose is produced according to the process.
摘要:
The present invention relates to a process for the production of a paper or paperboard comprising at least two plies wherein microfibrillated cellulose is added to the surface of a first ply and the other ply is attached to the first ply so that the microfibrillated cellulose located in between the plies. The invention further relates to a paper or board produced according to the method.
摘要:
The invention relates to a polymer-coated, heat-sealable liquid packaging board that resists solvents, such as strong alcoholic drinks, to a method of manufacturing the same and to a drinking cup made of the same. In the invention, resistance to solvents is achieved by lowering the raw edge penetration to the board. For this, the fibre base of the board contains at least 1.3 kg of hydrophobic size containing alkyl ketene dimer (AKD) per 1 tonne of dry matter, and at least 1.0 kg of wet-strength size per 1 tonne of dry matter, the density of the fibre base is 630-800 kg/m3 and the amount of heat-sealable polymer in the top layer is higher than the Bristow wheel roughness volume of the uncoated fibre base and/or at least 14 g/m2. When manufacturing the board, the AKD size, the length of the carbon chain of which is preferably at least C18, and the wet-strength size, such as polyamidoamine epichlorohydrin resin (PAAE), are added into the stock on the wire of the paper or board machine or before the same. At the same time, the pH of the tail water is adjusted so as to be alkaline, preferably to a value of over 9, whereby the pH of the water extract of the obtained board is in the order of about 7 or more. The drinking cup made of the board resists an ethanol solution of 30% by weight at 23° C. for at least 1 h.
摘要翻译:本发明涉及一种聚合物涂覆的,可热封的液体包装板,其耐受诸如强酒精饮料的溶剂,其制造方法和由其制成的饮杯。 在本发明中,通过降低对板的原始边缘渗透来实现对溶剂的耐受性。 为此,该板的纤维基含有每1吨干物质至少1.3kg含有烷基烯酮二聚体(AKD)的疏水性尺寸,并且每1吨干物质含有至少1.0kg的湿强度,密度 的纤维基数为630-800kg / m 3,顶层中的可热封聚合物的量高于未涂布的纤维基材的Bristow轮粗糙度体积和/或至少14g / m 2。 当制造板时,将AKD尺寸,其碳链长度优选至少为C18,以及湿强度尺寸(例如聚酰胺胺表氯醇树脂(PAAE))加入纸上的原料中 或板机或之前。 同时,将尾水的pH调节为碱性,优选为9以上,由此所得板的水提取物的pH为约7以上。 由该板制成的饮用杯子在23℃下抵抗30重量%的乙醇溶液至少1小时。
摘要:
The present invention relates to a container made from fiber based board wherein the container comprises a sleeve and a bottom, said bottom comprises polymer coated board, at least one side of said sleeve is uncoated and the sleeve is formed by sealing two edges of the sleeve together along a side seam. The invention further relates to a method for producing said container.
摘要:
The invention relates to a package intended for thermal treatment comprising a fibre-based packaging material treated with a hydrophobic size and comprising one or more layers for reduced water penetration outside and/or inside the fibre substrate. The package of the invention is characterised by the fibre substrate being treated with a combination of a wet-strength size, a hydrophobic size and an aluminium and/or calcium compound for increased heat resistance of the packaging material, and in that the ratio of hydrophobic size to the aluminium and/or calcium compound is 1:1-1:10.
摘要:
The invention relates to a package intended for thermal treatment comprising a fiber-based packaging material treated with a hydrophobic size and comprising one or more layers for reduced water penetration outside and/or inside the fiber substrate. The package of the invention is characterized by the fiber substrate being treated with a combination of a wet-strength size, a hydrophobic size and an aluminum and/or calcium compound for increased heat resistance of the packaging material, and in that the ratio of hydrophobic size to the aluminium and/or calcium compound is 1:1-1:10.
摘要:
The invention relates to a high quality paperboard comprising at least two plies, a first ply having good surface properties and strength, and a second ply for providing the paperboard with bulk wherein the second ply comprises hardwood CTMP. This paperboard has an internal strength and a bending resistance that is comparable with conventional high quality paperboard based on softwood CTMP. The invention also relates to products manufactured of the paperboard.
摘要:
The invention relates to a method in the wet end of a web forming process. In the method, at least one electrode pair (102, 103) is placed in the wet end. The electrode pair (102, 103) is supplied with a current/voltage from a power source (100), so that an electric field is set up between the electrode pair (102, 103), causing the material particles in the pulp suspension in the wet end to be electrically charged in a desired manner and to move in a desired manner in the pulp suspension in the wet end. The current/voltage of the power source (100) is controlled by means of a measuring and control unit (101) so as to cause the material particles in the pulp suspension to be electrically charged and to move in a desired manner, thus allowing the retention, formation and orientation of the material particles in the pulp suspension to be substantially improved.
摘要:
Polymer-coated, heat-sealable liquid packaging board that resists solvents (e.g. strong alcoholic drinks), method of manufacturing board, and drinking cup made of board. Resistance to solvents is achieved by lowering raw edge penetration into the board. The fiber base of the board contains at least 1.3 kg of hydrophobic size containing alkyl ketene dimer and at least 1.0 kg of wet-strength size per 1 ton of dry matter. Fiber base density is 630-800 kg/m3. The amount of heat-sealable polymer in the top layer is higher than the Bristow wheel roughness volume of the uncoated fiber base and/or at least 14 g/m2. When manufacturing the board, the alkyl ketene dimer size and a wet-strength size are added into the stock. The pH of the tail water is adjusted so as to be alkaline (about 7 or more).
摘要翻译:聚合物涂覆的,可热封的液体包装板,其抵抗溶剂(例如强酒精饮料),制造板的方法和由板制成的饮杯。 通过降低原料边缘渗透到板中来实现耐溶剂性。 板的纤维基底含有至少1.3kg含有烷基烯酮二聚体的疏水性尺寸,每1吨干物质含有至少1.0kg的湿强度尺寸。 纤维基础密度为630-800公斤/立方米。 顶层中的可热封聚合物的量高于未涂布纤维基材的布里斯托轮粗糙度体积和/或至少14g / m 2。 当制造板时,将烷基烯酮二聚体尺寸和湿强度尺寸加入到原料中。 尾水的pH调节为碱性(约7以上)。