BASE MATERIAL FOR SOLAR CELL
    71.
    发明申请
    BASE MATERIAL FOR SOLAR CELL 审中-公开
    太阳能电池基材

    公开(公告)号:US20100326515A1

    公开(公告)日:2010-12-30

    申请号:US12865483

    申请日:2009-01-30

    IPC分类号: H01L31/04

    摘要: It is to provide a base material for a solar cell, constituted by a stretched film of a composition containing a thermoplastic crystalline resin and inert particles, in which the base material for a solar cell has, on at least one side, a surface that has a center plane average surface roughness Ra of 30 to 500 nm and an average interval between local crests S on the surface of 40 to 5,000 nm, by which the base material for a solar cell provided has a surface capable of providing a light trapping effect and is useful for producing a solar cell exhibiting an excellent photoelectric conversion efficiency upon using as a base material of a thin film solar cell.

    摘要翻译: 本发明提供一种太阳能电池用基材,其由含有热塑性结晶性树脂和惰性粒子的组合物的拉伸膜构成,其中太阳能电池用基材的至少一面具有至少一面, 中心平面平均表面粗糙度Ra为30〜500nm,表面上的局部峰值S之间的平均间隔为40〜5000nm,由此提供了太阳能电池用基材,具有能够提供遮光效果的表面, 对于制造在作为薄膜太阳能电池的基材使用时具有优异的光电转换效率的太阳能电池是有用的。

    Port structure in semiconductor processing system
    73.
    发明授权
    Port structure in semiconductor processing system 失效
    半导体处理系统中的端口结构

    公开(公告)号:US07279067B2

    公开(公告)日:2007-10-09

    申请号:US10503940

    申请日:2003-02-17

    摘要: In a port structure 16A in a semiconductor processing system 2, a door 20A is disposed in a port 12A defined by upright wall 52 and 54. A table 48 opposed to the port is disposed outside the system. Defined on the table is a mount region 76 for mounting an open type cassette 18A for a process subject substrate W. A hood 50 is disposed rotatable relative to the table. The hood defines in its closed position a closed space surrounding the mount region and port, the space having a size to receive the cassette. First ventholes 58 are formed in the upright walls and/or the door so as to introduce gas from within the system into the closed space in the hood. Second ventholes 72 are formed in the table so as to discharge the gas can be discharged out of the closed space.

    摘要翻译: 在半导体处理系统2中的端口结构16A中,门20A设置在由直立壁52和54限定的端口12A中。 与该端口相对的一个表48设置在系统外部。 在桌子上定义的是安装区域76,用于安装用于处理对象衬底W的打开型盒18A。罩50可相对于桌子旋转设置。 罩在其关闭位置限定围绕安装区域和端口的封闭空间,该空间具有用于容纳盒的尺寸。 第一通气孔58形成在直立壁和/或门中,以将来自系统内的气体引入罩内的封闭空间。 第二通气孔72形成在工作台中,以便排出气体可以排出封闭空间。

    Multilayered polyester film and process for producing the same
    74.
    发明申请
    Multilayered polyester film and process for producing the same 有权
    多层聚酯薄膜及其制造方法

    公开(公告)号:US20050123779A1

    公开(公告)日:2005-06-09

    申请号:US10505048

    申请日:2003-02-10

    IPC分类号: B29C55/02 B32B27/36 B32B37/15

    摘要: The present invention is a multilayer polyester film comprising a layer A and a layer B which are laminated alternately, the layer A constituting the outermost layer on both sides of the film, wherein (1) the layer A comprises a polyester A, and the layer B comprises a polyester B, (2) the melting point of the polyester A is higher than the melting point of the polyester B by at least 15° C., (3) the layer A is a layer having an oriented structure, and the layer B is a layer having a substantially unoriented structure, (4) the ratio (a/b) of the total thickness (a) of the layer A to the total thickness (b) of the layer B is 0.01 to 3, and (5) the in-plane tensile strength of the multilayer polyester film is 50 MPa or lower at a maximum, and the difference between its maximum value and minimum value is 20 MPa or smaller; and a method for producing the multilayer polyester film. According to the present invention, there is provided a film having excellent isotropy of in-plane tensile strength, excellent transparency, a low degree of thickness unevenness and excellent moldability.

    摘要翻译: 本发明是一种多层聚酯薄膜,其包括交替层压的层A和层B,层A构成膜两侧的最外层,其中(A)层A包含聚酯A,层 B包含聚酯B,(2)聚酯A的熔点比聚酯B的熔点高至少15℃,(3)层A是具有取向结构的层, 层B是具有基本上未取向结构的层,(4)层A的总厚度(a)与层B的总厚度(b)的比(a / b)为0.01〜3,( 5)多层聚酯膜的面内拉伸强度最大为50MPa以下,其最大值与最小值的差为20MPa以下; 以及多层聚酯膜的制造方法。 根据本发明,提供了具有优异的面内拉伸强度,优异的透明性,低的不均匀度,成型性优异的薄膜。

    Polyester film for use as an ink image receiving base film and ink
    75.
    发明授权
    Polyester film for use as an ink image receiving base film and ink 失效
    聚酯薄膜用作油墨图像接收基膜和油墨

    公开(公告)号:US06896941B1

    公开(公告)日:2005-05-24

    申请号:US09762145

    申请日:2000-05-12

    摘要: A white biaxially oriented polyester film for use as a base film for receiving an ink jet printer image and a base film for receiving an ink jet printer image which satisfy the following requirements (1) to (4): (1) the content of titanium oxide particles having an average particle diameter of 0.1 to 0.5 μm in the polyester film is 5 to 20 wt %; (2) the polyester film has an average glossiness of 65 to 95%; (3) the polyester film has an X-ray diffraction intensity ratio (F-1/F-2) represented by the following formal (1): 0.05≦F-1/F-2≦0.15 (1)  wherein (F-1) is an X-ray diffraction intensity on a plane (1{overscore (1)}0) parallel to the surface of the film and (F-2) is an X-ray diffraction intensity on a plane (100) parallel to the surface of the film; and (4) the polyester film has a static friction coefficient of 0.3 to 0.6. The base film for receiving an ink jet printer image of the present invention is excellent in adhesion, glossiness, opacifying properties and transportability.

    摘要翻译: 用于接收喷墨打印机图像的基膜的白色双轴取向聚酯膜和满足以下要求(1)至(4)的用于接收喷墨打印机图像的基膜:(1)钛的含量 聚酯膜中平均粒径为0.1〜0.5μm的氧化物粒子为5〜20重量% (2)聚酯膜的平均光泽度为65〜95%。 (3)聚酯膜具有由以下形式(1)表示的X射线衍射强度比(F-1 / F-2):<?in-line-formula description =“In-line Formulas”end =“ (F-1)=((F-1))为(F-1) 平面上的平面(1(超(10))和(F-2)平面上的X射线衍射强度是平行于膜表面的平面(100)上的X射线衍射强度;以及 (4)聚酯薄膜的静摩擦系数为0.3〜0.6,本发明的喷墨打印机图像用接收基底膜的粘合性,光泽性,遮光性,输送性优异。

    White laminated polyester film for metallic plate lamination work
    76.
    发明授权
    White laminated polyester film for metallic plate lamination work 失效
    白色层压聚酯薄膜,用于金属板层压工作

    公开(公告)号:US06420010B1

    公开(公告)日:2002-07-16

    申请号:US09077837

    申请日:1998-06-04

    IPC分类号: B32B530

    摘要: The invented film comprises a layer A composed of a copolyester A, a layer B composed of a copolyester B, and a layer C composed of copolyester C. Layer A is laminated to one side of the layer B. Layer C is laminated to the other side of Layer B. Copolyester A contains 0-15 wt % of rutile titanium oxide (average particle diameter 0.1-0.5 &mgr;m). Copolyester B contains 10-50 wt % of the rutile titanium oxide. Copolyester C contains 0-15 wt % of the rutile titanium oxide. Each of Copolyester A, B, and C has a melting point of 210-245° C. The intrinsic viscosity (&eegr;A) of the polymer part of copolyester A, the intrinsic viscosity (&eegr;B) of the polymer part of copolyester B, and the intrinsic viscosity (&eegr;C) of the polymer part of copolyester C satisfy the following relationship. 0.46≦&eegr;B≦0.66, |&eegr;A-&eegr;B|

    摘要翻译: 本发明的薄膜包括由共聚酯A,由共聚聚酯B构成的层B和由共聚聚酯C组成的层C构成的层A.层A层叠在层B的一侧。层C层压到另一层 B层。共聚酯A含有0-15重量%的金红石型氧化钛(平均粒径0.1-0.5μm)。 共聚酯B含有10-50重量%的金红石氧化钛。 共聚酯C含有0-15重量%的金红石氧化钛。 共聚酯A,B和C的共聚物的熔点为210-245℃。共聚酯A的聚合物部分的特性粘度(ηaA),共聚酯B的聚合物部分的特性粘度(etaB) 共聚聚酯C的聚合物部分的特性粘度(η)满足以下关系。 0.46 <= etaB = 0.66,| etaA-etaB | <0.15,| etaC-etaB | <0.15和| etaA-etaC | <0.15。 整个层叠膜的表观密度(rho)与计算出的密度(rho0)的比例满足以下公式:0.75 <= rho / rho0 <= 1.00。 计算出的密度(rho0)由各共聚酯的聚合物部分的密度,金红石型氧化钛的密度,各层的厚度,各共聚酯中的金红石型氧化钛的浓度以及共聚酯层的数量来计算。

    Developing solution for silver halide photographic material and method
for processing silver halide photographic material by using the same
    79.
    发明授权
    Developing solution for silver halide photographic material and method for processing silver halide photographic material by using the same 失效
    用于卤化银照相材料的显影液和使用该卤化银照相材料的卤化银照相材料的处理方法

    公开(公告)号:US6013423A

    公开(公告)日:2000-01-11

    申请号:US193641

    申请日:1994-02-07

    IPC分类号: G03C5/29

    CPC分类号: G03C5/29

    摘要: A developing solution for silver halide photographic material contains a six-membered heterocyclic compound having two nitrogen atoms as the constituent atoms of the six-membered ring and mercapto group, hydroxyl group and at least one substituent group other than hydrogen atom and a five-membered heterocyclic compound having two to three nitrogen atoms as the constituent atoms of the five-membered ring and at least one mercapto group. There is also disclosed a method for processing a silver halide photographic material with said developing solution.

    摘要翻译: 用于卤化银照相材料的显影液含有六元杂环化合物,其具有两个氮原子作为六元环和巯基,羟基和至少一个除氢原子以外的取代基的组成原子,并且五元 具有2至3个氮原子的杂环化合物作为五元环的组成原子和至少一个巯基。 还公开了一种用所述显影液处理卤化银照相材料的方法。