Magnetic recording medium and method of manufacturing a magnetic recording medium
    81.
    发明授权
    Magnetic recording medium and method of manufacturing a magnetic recording medium 失效
    磁记录媒体及其制造方法

    公开(公告)号:US07241518B2

    公开(公告)日:2007-07-10

    申请号:US10488983

    申请日:2003-07-14

    申请人: Satoshi Sato

    发明人: Satoshi Sato

    IPC分类号: G11B5/706 B05D5/10

    摘要: It is a magnetic recording medium for which favorable values for all of reproduced output, noise level and error rate can be obtained, and which is also superior in terms of storage stability. A magnetic recording medium (10), which has a configuration in which a magnetic layer (3) comprised of a maghemite thin film containing cobalt is formed on a tape-shaped substrate (1) comprised of aromatic polyimide, and in which the substrate (1) is 3 to 10 μm in thickness, and 5 to 30 nm in its ten-point average roughness (SRz) of the surface on which the magnetic layer (3) is formed, and the magnetic layer (3) is 10 to 50 nm in thickness, 0.1 to 3.0 nm in center plane average thickness (SRa), and 2,000 to 4,000 Oe (158,000 to 316,000 A/m) in in-plane coercivity, is made.

    摘要翻译: 它是一种磁记录介质,可以获得所有再现输出,噪声电平和误差率的有利值,并且在存储稳定性方面也是优异的。 一种磁记录介质(10),其具有在由芳香族聚酰亚胺构成的带状基板(1)上形成由含有钴的磁赤铁矿薄膜构成的磁性层(3)的构造,并且其中基板 1)的厚度为3〜10μm,形成有磁性层(3)的表面的十点平均粗糙度(SRz)为5〜30nm,磁性层(3)为10〜50 的厚度,中心面平均厚度(SRa)为0.1〜3.0nm,面内矫顽力为2,000〜4000e(158,000〜316,000A / m)。

    Method of producing silicon monocrystal
    84.
    发明授权
    Method of producing silicon monocrystal 有权
    硅单晶的生产方法

    公开(公告)号:US07195669B2

    公开(公告)日:2007-03-27

    申请号:US10521035

    申请日:2003-07-07

    IPC分类号: C30B25/12

    摘要: A silicon single crystal rod (24) is pulled from a silicon melt (13) made molten by a heater (17), and a change in diameter of the silicon single crystal rod every predetermined time is fed back to a pulling speed of the silicon single crystal rod and a temperature of the heater, thereby controlling a diameter of the silicon single crystal rod. A PID control in which a PID constant is changed on a plurality of stages is applied to a method which controls the pulling speed of the silicon single crystal rod so that the silicon single crystal rod has a target diameter and a method which controls a heater temperature so that the silicon single crystal rod has the target temperature. A set pulling speed for the silicon single crystal rod is set so that V/G becomes constant, and an actual pulling speed is accurately controlled so as to match with the set pulling speed, thereby suppressing a fluctuation in diameter of the single crystal rod.

    摘要翻译: 从由加热器(17)熔化的硅熔体(13)拉出硅单晶棒(24),并且每隔预定时间将硅单晶棒的直径变化反馈到硅的拉伸速度 单晶棒和加热器的温度,从而控制硅单晶棒的直径。 将控制多个级上的PID常数的PID控制应用于控制硅单晶棒的拉拔速度的方法,使得硅单晶棒具有目标直径,以及控制加热器温度的方法 使硅单晶棒具有目标温度。 设定硅单晶棒的设定拉拔速度使得V / G变得恒定,并且实际的拉拔速度被精确地控制以与设定的牵引速度相匹配,从而抑制单晶棒的直径的波动。

    Cholesterol detection reagent
    87.
    发明申请
    Cholesterol detection reagent 审中-公开
    胆固醇检测试剂

    公开(公告)号:US20060110781A1

    公开(公告)日:2006-05-25

    申请号:US10516072

    申请日:2003-05-30

    IPC分类号: C12Q1/00 C12Q1/60

    CPC分类号: G01N33/92

    摘要: An object of the present invention is to provide a novel cholesterol detection reagent comprising a substance which can specifically binds to cholesterol to detect it, and a method for detecting cholesterol using the reagent. The present invention provides a cholesterol detection reagent comprising a polyethylene glycol cholesteryl ether which may be labeled.

    摘要翻译: 本发明的目的是提供一种胆固醇检测试剂,其包含能够特异性结合胆固醇进行检测的物质,以及使用该试剂检测胆固醇的方法。 本发明提供一种胆固醇检测试剂,其包含可标记的聚乙二醇胆固醇醚。

    Modular jack
    88.
    发明授权

    公开(公告)号:US06645000B2

    公开(公告)日:2003-11-11

    申请号:US10147861

    申请日:2002-05-20

    IPC分类号: H01R300

    摘要: The modular jack (21) comprises a housing (22) having side walls (30), a plurality of cavities (27, 28) provided at a front side of the housing (22), into which mating modular plugs are inserted, at least one groove (33, 34) provided in one of the side walls (30), and at least one LED (24, 25) fitted into the groove (33, 34) and accommodated in the side walls (30). Accordingly, the fixing work for LEDs (24, 25) is simplified and the manufacturing cost is minimized.

    Magnetic recording medium
    89.
    发明授权
    Magnetic recording medium 失效
    磁记录介质

    公开(公告)号:US06203884B1

    公开(公告)日:2001-03-20

    申请号:US09211003

    申请日:1998-12-15

    IPC分类号: G11B5733

    摘要: The present invention provides a metal thin film type magnetic recording medium including a non-magnetic substrate made from a polyamide film whose surface configuration is controlled so as to obtain an optimal fine configuration of a magnetic layer surface, enabling to simultaneously obtain a preferable electro-magnetic conversion characteristic and preferable running characteristic. The non-magnetic substrate is made from an aromatic polyamide film formed in such a manner that fine protrusions having an average height of 5 to 50 nm are formed in a range of 103 to 105 thousand pieces/mm2 on a surface where a ferromagnetic metal thin film is to be formed.

    摘要翻译: 本发明提供一种金属薄膜型磁记录介质,其包括由聚酰胺薄膜制成的非磁性基材,其表面形状被控制以获得磁性层表面的最佳精细构型,能够同时获得优选的电 - 磁转换特性和优选的行走特性。非磁性基材由芳族聚酰胺薄膜制成,其形成方式是使平均高度为5〜50nm的微细突起形成在103〜105000张/ mm 2的范围内 在要形成铁磁金属薄膜的表面上。

    Method of tightening a bolt with an optimum time
    90.
    发明授权
    Method of tightening a bolt with an optimum time 失效
    以最佳时间拧紧螺栓的方法

    公开(公告)号:US5650574A

    公开(公告)日:1997-07-22

    申请号:US671553

    申请日:1996-06-27

    摘要: A method of tightening a bolt in an optimum time length does not require an additional program for controlling speed once optimum internal parameters have been determined through several learning cycles. A target torque is first preset and the nut runner is subjected to several learning cycles so that the nut runner automatically determines such internal parameters as to stop the motor immediately after the target torque is reached, requiring a minimum time for tightening the bolt.

    摘要翻译: 在最佳时间长度内拧紧螺栓的方法,一旦通过几个学习周期确定最佳内部参数,就不需要用于控制速度的附加程序。 首先预设目标扭矩,并且螺母扳手经受若干学​​习循环,使得螺母扳手自动确定这样的内部参数,以在达到目标扭矩之后立即停止马达,需要最小时间来拧紧螺栓。