公开(公告)号:US20240375359A1
公开(公告)日:2024-11-14
申请号:US18287378
申请日:2022-05-20
Applicant: Polyplastics Co., Ltd.
Inventor: Takato Isomura , Koki Nagai , Kazuya Goshima , Hiroki Fukatsu
IPC: B29C65/00 , B29C65/16 , B29K67/00 , B29K105/00
Abstract: A laser transmissive resin composition is disclosed with high laser transmissiveness, good color development, and in which color transfer does not occur and a molded article using the same. The laser transmissive resin composition (I) includes, with respect to 100 parts by mass of a polyester-based resin (A), 0.005-5.0 parts by mass of an organic pigment (B) including at least a benzimidazolone-based yellow pigment (b1), wherein a 1 mm thick molded article of the resin composition (I) has a CIE L* value of 25 or less and a 940 nm laser transmittance of 40% or greater.
-
公开(公告)号:US11891504B2
公开(公告)日:2024-02-06
申请号:US18030582
申请日:2021-09-10
Applicant: Polyplastics Co., Ltd.
Inventor: Yuuki Kanda , Tomohiro Monma , Hiroki Arai
CPC classification number: C08L59/00 , C08K3/04 , C08K5/005 , C08K7/18 , C08K2201/003
Abstract: A polyacetal resin composition contains a polyacetal copolymer (A) in an amount of 100 parts by mass, the polyacetal copolymer resin having a hemiformal terminal group amount of 0.8 mmol/kg or less, an antioxidant (B) in an amount of 0.5 to 3.0 parts by mass, at least one of zinc oxide or magnesium oxide (C) having an average particle diameter of 5 μm or less in an amount of more than 2.0 parts by mass and 12 parts by mass or less, carbon black (D) having a BET specific surface area of 300 to 400 m2/g in an amount of 5.0 to 16 parts by mass, and polyalkylene glycol (E) in an amount of 0.5 to 3.0 parts by mass.
-
公开(公告)号:US20230242762A1
公开(公告)日:2023-08-03
申请号:US18014774
申请日:2021-06-22
Applicant: POLYPLASTICS CO., LTD.
Inventor: Hidekazu IDEI , Katsuhei OHNISHI
CPC classification number: C08L81/02 , B29C45/0001 , B29C45/0005 , C08K3/041 , C08K7/14 , B29K2081/04
Abstract: Provided is a method of suppressing burrs that occur during injection-molding of a polyarylene sulfide resin composition, including: adding at least 0.01 to 5 parts by mass of a carbon nanostructure to 100 parts by mass of a polyarylene sulfide resin and melt-kneading at least the carbon nanostructure and the polyarylene sulfide resin.
-
公开(公告)号:US11661511B2
公开(公告)日:2023-05-30
申请号:US17593231
申请日:2020-03-10
Applicant: Polyplastics Co., Ltd.
Inventor: Akihiro Tamaoka , Hatsuhiko Harashina , Tomohiro Monma
IPC: C08L59/00 , C08K5/098 , C08K5/25 , C08K5/3445
CPC classification number: C08L59/00 , C08K5/098 , C08K5/25 , C08K5/3445 , C08L2201/08 , C08L2203/30
Abstract: A method for producing a polyacetal resin composition which allows for suppression of formaldehyde generation from a molded article to an extremely low level, and stable suppression of mold deposits during molding. The polyacetal resin composition contains: 100 parts by mass of a polyacetal polymer (A); 0.01 to 0.50 parts by mass of an aliphatic carboxylic acid hydrazide (B); 0.001 to 0.50 parts by mass of a hydantoin compound having two hydrazinocarbonylalkyl groups (C); and 0.001 to 0.30 parts by mass of an alkaline earth metal salt of aliphatic carboxylic acid (D), wherein the total amount of the components (B) and (C) with respect to 100 parts by mass of the polyacetal polymer (A) is 0.03 to 0.55 parts by mass, and the polyacetal polymer (A) is a polyacetal copolymer obtained by copolymerizing trioxane as a principal monomer (a) with a cyclic ether having at least one carbon-carbon bond as a comonomer (b) using a heteropolyacid represented by general formula (1) as a polymerization catalyst (c) to obtain a reaction product, and subsequently adding a carbonate of an alkali metal element or alkaline earth metal element (d) to the reaction product to deactivate the polymerization catalyst (c).
-
公开(公告)号:US20230041838A1
公开(公告)日:2023-02-09
申请号:US17783326
申请日:2020-12-16
Applicant: Polyplastics Co., Ltd.
Inventor: Takato Isomura , Kazuya Goshima , Kouichi Sakata
IPC: B29C65/16
Abstract: Problem: To provide a molded article for laser welding which has excellent visible light transmittance and laser transmittance and in which variation in laser transmittance is suppressed, and an agent for suppressing variation in laser transmittance of a molded article for laser welding.
Solution: A molded article for laser welding comprising a polybutylene terephthalate resin composition containing 100 parts by mass of (A) a polybutylene terephthalate resin, (B) a polycarbonate resin in which the melt viscosity at 300° C. and a shear rate of 1000 sec−1 is 0.20 kPa·s or greater, and 1 part by mass or greater and 10 parts by mass or less of (C) an epoxy-based compound, the molded article having a thickness at a welded part of 1.3 mm or greater, and an agent for suppressing variation in laser transmittance of a molded article for laser welding, the agent containing an epoxy-based compound.-
公开(公告)号:US20220388208A1
公开(公告)日:2022-12-08
申请号:US17763419
申请日:2020-09-16
Applicant: Polyplastics Co., Ltd.
Inventor: Takashi FUJITA , Hiroki ARAI
Abstract: A casing member for an in-vehicle camera, obtained by injection molding a resin composition that comprises 100 to 300 parts by mass of a total of a fibrous inorganic filler and a non-fibrous inorganic filler to 100 parts by mass of a polyarylene sulfide resin and has a content of an elastomer of 10% by mass or less, and satisfying the following conditions (A) and (B). (A) When a molded product of a predetermined shape is injection molded using the resin composition under predetermined conditions, an absolute value of (shrinkage rate in a direction perpendicular to a flow direction)−(shrinkage rate in the flow direction) is 0.5% or less. (B) A water absorption rate of a molded product of a predetermined shape that is injection molded using the resin composition under predetermined conditions is 0.3% or less when subjected to a predetermined hot water immersion test.
-
公开(公告)号:US11326053B2
公开(公告)日:2022-05-10
申请号:US16981861
申请日:2019-03-20
Applicant: POLYPLASTICS CO., LTD.
Inventor: Kazuya Goshima , Itsuki Saito
Abstract: The present invention addresses the problem of enhancing the fluidity of a polybutylene terephthalate resin composition that uses a halogenated benzyl acrylate-based flame retardant as a flame retardant while maintaining properties such as excellent mechanical strength that a polybutylene terephthalate-based resin possesses. The problem is solved by adding a protic compound to the polybutylene terephthalate resin composition that uses a halogenated benzyl acrylate-based flame retardant as a flame retardant.
-
公开(公告)号:US20210354353A1
公开(公告)日:2021-11-18
申请号:US17309370
申请日:2020-01-16
Applicant: Polyplastics Co., Ltd.
Inventor: Akihiro MOCHIZUKI , Kohshi MIOKI
Abstract: A resin molded article that has a high bond strength in a composite molded article in which a first molded article and a second molded article are integrated, and that has a stable and uniform bond strength of a composite molded article between shots of the molded article. The composite molded article includes a grooved first resin molded article containing at least a resin, a glass fiber, and a laser absorption material, and having grooves that expose the glass fiber; and a second molded article adjacently disposed on the grooved surface of the first resin molded article. In the first resin molded article, the glass fiber is added in an amount of 12-45 mass % with respect to the total mass of the resin composition that constitutes the resin molded article, the laser absorption material is added in an amount of 0.25-10 mass % with respect to the total mass of the resin composition, and the glass fiber and the laser absorption material are blended within specific blending ranges.
-
公开(公告)号:US11142637B2
公开(公告)日:2021-10-12
申请号:US16082052
申请日:2017-02-06
Applicant: Polyplastics Co., Ltd.
Inventor: Hatsuhiko Harashina , Hirokazu Katsuchi
Abstract: A polyacetal resin composition which exhibits resistance to hot water, and contains 100 parts by mass of a polyacetal resin, 1 to 100 parts by mass, inclusive, of glass fibers subjected to a surface treatment with a blocked isocyanate compound and an aminosilane coupling agent, and 0.001 to 1.0 parts by mass, inclusive, of boric acid.
-
公开(公告)号:US10683413B2
公开(公告)日:2020-06-16
申请号:US15510381
申请日:2015-06-11
Applicant: Polyplastics Co., Ltd.
Inventor: Akihide Shimoda
Abstract: A polyoxymethylene (POM) resin composition which is used for a resin molded article having an excellent sliding characteristic and wear resistance property and also having an excellent surface property and peeling resistance property. This POM resin composition contains: (A) 100 parts by mass of a POM resin; (B) 0.01-1 parts by mass of a hindered phenolic antioxidant; (C) 0.05-1 parts by mass inclusive of a nitrogen-containing compound; (D) 0.5-10 parts by mass of a modified olefin polymer which is an olefin polymer that has been modified by an unsaturated carboxylic acid or the like; (E) 0.01-5 parts by mass of an alkylene glycol polymer that has a primary or secondary amino group and a number average molecular weight of 400-500,000; (F) 0.1-20 parts by mass of calcium carbonate which has a BET specific surface area of 15 m2/g or less, has a mean particle size of 50-200 nm or less, is surface-untreated, and is substantially cubic; (G) 0.1-10 parts by mass of a partial ester of a divalent to tetravalent alcohol; and (H) 0.1-10 parts by mass of an α-olefin oligomer.
-
-
-
-
-
-
-
-
-