摘要:
A highly durable, high-strength thermal shield element is provided for the interior lining of the combustion chamber of a gas turbine. For this purpose, the thermal shield element comprises a base produced from a solidified cast ceramic material into which a plurality of reinforcing elements are integrated, to increase the tensile strength of the thermal shield element.
摘要:
The invention relates to moulded bodies having catalytic properties, obtained due to a method that comprises the following said steps: a) a moulded body is produced by means of a powder-based rapid-prototyping-method, b) said moulded body is optionally heat-treated, c) at least one catalytically active component is optionally applied to the moulded body, d) said moulded body is optionally subjected to another heat-treatment. The steps b, c) and/or d) can be performed several times. Said moulded bodies are used as reactor fittings in heterogeneously catalyzed chemical reactions.
摘要:
A highly durable, high-strength thermal shield element is provided for the interior lining of the combustion chamber of a gas turbine. For this purpose, the thermal shield element comprises a base produced from a solidified cast ceramic material into which a plurality of reinforcing elements are integrated, to increase the tensile strength of the thermal shield element.
摘要:
A material mixture for producing a fireproof material, including spinel and zirconium oxide and a coarse-grained fraction with a weight fraction of greater than 50% and a fine-grained fraction, wherein the coarse-grained fraction includes coarse grains with dimensions larger than 20 μm and the fine-grained fraction includes fine grains with dimensions smaller than 20 μm.
摘要:
Slip containing at least one aluminium oxide powder and at least one unstabilized zirconium dioxide powder, wherein a) the zirconium dioxide powder i) has a mean particle diameter of less than 300 nm, ii) shows only the monoclinic phase and the tetragonal phase in the X-ray diffraction pattern, with the proportion of tetragonal phase at room temperature being from 20 to 70%, and iii) is present in a proportion of from 2 to 20% by weight, based on the total amount of the slip, b) the aluminium oxide powder i) has a mean particle diameter of more than 300 nm and ii) is present in a proportion of from 80 to 98% by weight, based on the total amount of the slip, and c) the solids content, as the sum of aluminium oxide and zirconium dioxide, is from 50 to 85% by weight, based on the total amount of the slip.
摘要:
A highly durable, high-strength thermal shield element is provided for the interior lining of the combustion chamber of a gas turbine. For this purpose, the thermal shield element comprises a base produced from a solidified cast ceramic material into which a plurality of reinforcing elements are integrated, to increase the tensile strength of the thermal shield element.
摘要:
Shaped bodies having catalytic properties which can be obtained by a process comprising the steps: a) production of a shaped body by means of a powder-based rapid prototyping process, b) if appropriate, a heat treatment of the shaped body, c) if appropriate, application of at least one catalytically active component to the shaped body, d) if appropriate, a further heat treatment, where steps b), c) and/or d) can be carried out a number of times, are used as reactor internals in heterogeneously catalyzed chemical reactions.
摘要:
Disclosed is a molding compound for producing a fireproof lining, especially for a combustion chamber of a stationary gas turbine. Said molding compound is characterized particularly by the fact that the molding compound is formed from more than about 50 percent by weight of silicon carbide and less than about 50 percent by weight of aluminum silicate.
摘要:
Disclosed is a molding compound for producing a fireproof lining, especially for a combustion chamber of a stationary gas turbine. The molding compound is characterized particularly by the fact that the molding compound is formed from more than about 50 percent by weight of silicon carbide and less than about 50 percent by weight of aluminum silicate.
摘要:
Slip containing at least one aluminium oxide powder and at least one unstabilized zirconium dioxide powder, wherein a) the zirconium dioxide powder i) has a mean particle diameter of less than 300 nm, ii) shows only the monoclinic phase and the tetragonal phase in the X-ray diffraction pattern, with the proportion of tetragonal phase at room temperature being from 20 to 70%, and iii) is present in a proportion of from 2 to 20% by weight, based on the total amount of the slip, b) the aluminium oxide powder i) has a mean particle diameter of more than 300 nm and ii) is present in a proportion of from 80 to 98% by weight, based on the total amount of the slip, and c) the solids content, as the sum of aluminium oxide and zirconium dioxide, is from 50 to 85% by weight, based on the total amount of the slip.