摘要:
A membrane for use in an X-ray mask composed of a compound comprising at least three kinds of elements of boron (B), silicon (Si) and nitrogen (N) in which the content of silicon in the compound is at least 15 atomic percent, but less than 100 atomic percent, and the atomic ratio of Si/(B+Si) in the compound is at least 0.2, but less than one. The membrane is synthesized from source gases including at least the foregoing three kinds of elements by chemical reaction under such conditions that the ratio of nitrogen to boron plus silicon is at least one in the source gases and thereby depositing a film of the compound onto a substrate. Since the membrane thus prepared has a high transmittance in the visible region and X-ray and their residual stress can be readily controlled by adjusting the conditions for the formation of the membrane, it is suitable for the preparation of X-ray masks.
摘要:
Boron nitride containing titanium nitride in an amount of 0.05 to 10 wt. % which is produced at a relatively low temperature, utilizing a chemical vapor deposition technique. In the deposition process, boron, titanium and nitrogen source gases are introduced into an evacuated reactor together with a carrier and/or diluent gas and contacted with a heated substrate previously mounted in the reactor, whereby boron nitride with titanium nitride is deposited onto the substrate. The deposit thus obtained has a high density, a significantly improved heat-shielding ability, a high degree of anisotropy with respect to thermal diffusivity and a high chemical stability. By using such anisotropic boron nitride with BN ceramics, very useful BN type composite ceramics can be produced.
摘要:
An aluminum-based alloy having the general formula Al.sub.x L.sub.y M.sub.z (wherein L is Mn or Cr; M is Ni, Co, and/or Cu; and x, y, and z, representing a composition ratio in atomic percentages, satisfy the relationships x+y+z=100, 75.ltoreq.x.ltoreq.95, 2.ltoreq.y.ltoreq.15, and 0.5.ltoreq.z.ltoreq.10) having a metallographic structure comprising a quasi-crystalline phase possesses high strength and high rigidity. In order to enhance the ductility and toughness of the aluminum-based alloy, the atomic percentage of M may be further limited to 0.5.ltoreq.z.ltoreq.4, and more preferably to 0.5.ltoreq.z.ltoreq.3. The aluminum-based alloy is useful as a structural material for aircraft, vehicles and ships, and for engine parts; as material for sashes, roofing materials, and exterior materials for use in construction; or as materials for use in marine equipment, nuclear reactors, and the like.
摘要:
Hard magnetic materials of the present invention contain at least one element of Fe, Co and Ni as a main component, at least one element M of Zr, Nb, Ta and Hf, at least one rare earth element R and B. The texture of the materials has at least 70% of fine crystalline phase having an average grain size of 100 nm or less, and the residue having an amorphous phase, the fine crystalline phase mainly composed of bcc-Fe or bcc-Fe compound, Fe--B compound and/or R.sub.2 Fe.sub.14 B.sub.1.
摘要:
An Fe-based soft magnetic alloy having a high saturated magnetic flux density and having a composition represented by formula (I) below: (Fe.sub.1-a Q.sub.a).sub.b B.sub.x T.sub.y T'.sub.z (I) wherein Q represents at least one element selected from the group consisting of Co and Ni; T represents at least one element selected from the group consisting of Ti, Zr, Hf, V, Nb, Ta, Mo and W, with Zr and/or Hf being always included; T' represents at least one element selected from the group consisting of Cu, Ag, Au, Ni, Pd and Pt; a, b, x, y and z are real numbers satisfying relationships below: 0.ltoreq.a.ltoreq.0.05, 0.ltoreq.b.ltoreq.93 atomic %, 0.5.ltoreq.x.ltoreq.16 atomic %, 4.ltoreq.y.ltoreq.10 atomic %, 0.ltoreq.z.ltoreq.4.5 atomic % provided that when 0
摘要翻译:具有高饱和磁通密度且具有由下式(I)表示的组成的Fe基软磁合金:(Fe1-aQa)bBxTyT'z(I)其中Q表示选自以下的至少一种元素: Co和Ni; T表示选自Ti,Zr,Hf,V,Nb,Ta,Mo和W中的至少一种元素,其中始终包括Zr和/或Hf; T'表示选自Cu,Ag,Au,Ni,Pd和Pt中的至少一种元素; a,b,x,y和z是满足以下关系的实数:0 = a = 0.05,0
摘要:
A noise filter includes an annular magnetic core made of a soft magnetic alloy ribbon mainly made of Fe and containing B and at least one element selected from a group consisting of Ti, Zr, Hf, Nb, Ta, Mo and W, at least 50% of the soft magnetic alloy structure being composed of body-centered cubic structured fine grains having an average grain size of 30 nm or below, a casing for accommodating the magnetic core and having an insulating plate, a pair of coils separated from each other by the insulating plate, and an electronic circuit for connecting a core element made up of the magnetic core, the casing and the coils.
摘要:
Ultrafine whiskery or columnar ceramic particles, a method for producing the ultrafine particles, and a sintered article obtained by sintering the ultrafine ceramic particles are disclosed. The ultrafine ceramic particles are produced by thermally melting a matrix alloy of a composition of Al--M.sup.1, wherein M.sup.1 stands for at least one metallic element selected from the group consisting of Cr, Co, and Fe, or Al--M.sup.1 --M.sup.2, wherein M.sup.2 stands for at least one metallic element selected from the group consisting of Au, Cu, Dy, Er, Ga, Ge, Gd, Hf, Ho, Lu, Mn, Mo, Nb, Nd, Ni, Pr, Re, Sb, Sc, Si, Sn, Ta, Tb, Ti, Tm, V, W, Y, Zn, or Zr, in a nitriding atmosphere containing nitrogen and causing the vaporized raw material to react with the nitrogen in the atmosphere. By this method, ultrafine composite particles or a mixture comprising ultrafine whiskery or columnar aluminum nitride particles and ultrafine particles of the metal, the intermetallic compound of the metal with aluminum, and the nitride ceramic of the metal are produced. The ultrafine particles thus obtained find extensive utility as sintering materials and dispersion materials, for example.
摘要:
The present invention relates to a method of stably manufacturing a Fe-base soft magnetic alloy having steps of subjecting an amorphous alloy mainly composed of Fe to heat treatment in which the amorphous alloy is heated to 400.degree. to 750.degree. C. at a heating rate of 1.0.degree. C./minute or higher so that at least 50% or more of the structure of the amorphous alloy is made of fine crystalline grains formed into a body-centered cubic structure and having an average grain size of crystal of 30 nm or smaller as to have a high magnetic permeability and saturation magnetic flux density.
摘要:
The present invention provides a sacrificial electrode material which consists of a single phase amorphous structure or a structure consisting of an amorphous phase and a crystalline solid solution phase and provides electrochemical corrosion protection to metallic articles exposed to an aqueous electrolytic solution. The electrode material is prepared by rapidly quenching a magnesium-based alloy material from the liquid phase or vapor phase thereof, the magnesium-based alloy material consisting the general formula: Mg.sub.bal X1.sub.a X2.sub.b or Mg.sub.bal X1.sub.a, wherein X1 is at least one element selected from the group consisting of Al, Zn, Ga, Ca and In; X2 is at least one element selected from the group consisting of Mm (misch metal), Y and rare earth metal elements; a and b are, in atomic percentages, 5.0.ltoreq.a.ltoreq.35.0 and 3.0.ltoreq.b.ltoreq.25.0, respectively. The magnesium-based alloy material may further contain one or more transition metal elements in their total contents not exceeding 1.0 atomic %.
摘要:
Deposition of a hard film of Ti-Si-N composite material on a substrate is carried out by using a source of evaporation possessing a composition of Ti.sub.a Si.sub.b (wherein "a" and "b" stand for atomic percentages respectively falling in the ranges of 75 at % .ltoreq.a.ltoreq.85 at % and 15 at %.ltoreq.b.ltoreq.25 at %, providing a+b=100 at %). Deposition is effected by a sputtering process or ion plating process in an atmosphere of an inert gas containing a nitrogen-containing reaction gas while controlling the feed rate of the reaction gas into a chamber in such a manner that the partial pressure of nitrogen is kept constant or varied continuously or stepwise. By this method there can be obtained a film having fine TiN crystalline particles uniformly dispersed in the matrix phase of Ti-Si amorphous metal or a film of functionally gradient structure in which the ratio of fine TiN crystalline particles dispersed in the matrix phase increases continuously or stepwise in the direction of thickness of the film.
摘要翻译:通过使用具有TiaSib组成的蒸发源(其中“a”和“b”表示分别落在75的范围内的原子百分比),将Ti-Si-N复合材料的硬膜沉积在基底上 at% = a = 85 at%和15 at% = b = 25 at%,提供+ b = 100 at%)。 在含有含氮反应气体的惰性气体的气氛中通过溅射法或离子镀法进行沉积,同时将反应气体的进料速率控制在室内,使得氮的分压保持恒定 或连续或逐步变化。 通过该方法可以获得均匀分散在Ti-Si非晶态金属的基体相中的细TiN结晶粒子的膜或其中分散在基体相中的细TiN结晶粒子的比例连续增加的功能梯度结构的膜,或 在膜的厚度方向上逐步地。