摘要:
A surface-treated copper foil includes a treated surface, where the peak extreme height (Sxp) of the treating surface is 0.4 to 3.0 μm. When the surface-treated copper foil is heated at a temperature of 200° C. for 1 hour, the ratio of the integrated intensity of diffraction peak of (111) plane to the sum of the integrated intensities of diffraction peaks of (111) plane, (200) plane, and (220) plane of the treating surface is at least 60%.
摘要:
A surface-treated copper foil including a treating surface, where the root mean square height (Sq) of the treating surface is in a range of 0.20 to 1.50 μm and the texture aspect ratio (Str) of the treating surface is not greater than 0.65. When the surface-treated copper foil is heated at a temperature of 200° C. for 1 hour, the ratio of the integrated intensity of (111) peak to the sum of the integrated intensities of (111) peak, (200) peak, and (220) peak of the treating surface is at least 60%.
摘要:
An electrodeposited copper foil includes a bulk copper foil. When a weight of the electrodeposited copper foil is increased to 105.0 wt % during a thermogravimetric analysis (TGA) performed on the electrodeposited copper foil at a heating rate of 5° C./min and an air flow rate of 95 mL/min, a heating temperature of the TGA is defined as T105.0 wt % and in a range of 550° C. to 750° C.
摘要:
Provided is an electrolytic copper foil. The electrolytic copper foil has a drum side and a deposited side, wherein ΔRz is less than 0.8 μm; the electrolytic copper foil has a transverse direction, wherein the electrolytic copper foil is divided into 10 test pieces with the same width and the same length, and each two adjacent ones of the 10 test pieces have a weight deviation therebetween, and a count of the weight deviation(s) greater than or equal to 1.5% is smaller than a count of the weight deviations smaller than 1.5%; wherein n represents any one of the test piece numbers from 1 to 9, and the weight deviation between each two adjacent ones of the 10 test pieces ( % ) = the weight of test piece ( n ) - the weight of test piece ( n + 1 ) the smaller weight in test piece ( n ) and test piece ( n + 1 ) × 100 % .
摘要:
The present disclosure relates to a copper foil which exhibits surprising anti-deformation properties (e.g., it is resistant to swelling, sagging, and wrinkling). Typically, the copper foil has (a) a shiny side with a surface roughness (Rz) in the range of 0.6 to 1.9 μm; (b) a matte side with a surface roughness (Rz) in the range of 0.6 to 1.9 μm; and (c) a lightness L* value of the matte side, based on the L*a*b* color system, in the range of 12 to 35. The disclosure further relates to an anode comprising an anode active material on an anode current collector, wherein the anode current collector includes the above-mentioned copper foil. The anodes are used in, for example, lithium ion secondary batteries.
摘要翻译:本公开涉及具有令人惊奇的抗变形性(例如,其耐溶胀,下垂和起皱)的铜箔。 通常,铜箔具有(a)光泽面,表面粗糙度(Rz)在0.6〜1.9μm的范围内; (b)表面粗糙度(Rz)为0.6〜1.9μm的无光面; 和(c)基于L * a * b *颜色系统的无光泽度的亮度L *值在12至35的范围内。本发明还涉及一种阳极,其包括在阳极电流上的阳极活性材料 集电体,其中所述阳极集电体包括上述铜箔。 阳极用于例如锂离子二次电池。
摘要:
An electrolytic copper foil includes a copper foil body; and a IIA-group metal adhered to a surface of the copper foil body, wherein a signal strength of the IIA group metal is greater than 0.1% based on a signal strength of copper element as 100% analyzed by a secondary ion mass spectrometer. The present invention also provides a method for cleaning copper foil and a cleaning fluid composition which is used in the cleaning method.
摘要:
Electrodeposited copper foils having adequate puncture strength to withstand both pressure application during consolidation with negative electrode active materials during manufacture, as well as expansion/contraction during repeated charge/discharging cycles when used in a rechargeable secondary battery are described. These copper foils find specific utility as current collectors in rechargeable secondary batteries, particularly in lithium secondary battery with high capacity. Methods of making the copper foils, methods of producing negative electrode for use in lithium secondary battery and lithium secondary battery of high capacity are also described.
摘要:
A package structure of a roll-shaped thin film includes a thin film roll and a buffer layer. The thin film roll includes a winding core and a thin film wound around the winding core, and the buffer layer is wound around an outer circumference of the thin film. An end portion of the buffer layer is covered with an inner surface of an end portion of the thin film, and the thickness of the buffer layer is in a range of 1-20 mm.
摘要:
Provided are an electrodeposited copper foil, an electrode comprising the same, and a lithium-ion secondary battery comprising the same. The electrodeposited copper foil has a drum side and a deposited side opposing the drum side, wherein at least one of the drum side and the deposited side exhibits a void volume value (Vv) in the range of 0.17 μm3/μm2 to 1.17 μm3/μm2; and an absolute value of a difference between a maximum height (Sz) of the drum side and a Sz of the deposited side is in the range of less than 0.60 μm.
摘要:
A package structure of a roll-shaped thin film includes a thin film roll and a buffer layer. The thin film roll includes a winding core and a thin film wound around the winding core, and the buffer layer is wound around an outer circumference of the thin film. An end portion of the buffer layer is covered with an inner surface of an end portion of the thin film, and the thickness of the buffer layer is in a range of 1-20 mm.