Abstract:
The present invention relates to a phosphinated poly(2,6-dimethy phenylene oxide)oligomer, specifically an unsaturated group-containing phosphinated poly(2,6-dimethy phenylene oxide)oligomer, and processes for producing the same. A thermoset produced from the unsaturated group-containing phosphinated poly(2,6-dimethy phenylene oxide)oligomers according to the present invention exhibits flame retardancy and has a low dielectric constant and dissipation factor and a high glass transition temperature.
Abstract:
A preparation method of a polyurethane resin including the following steps is provided. A liquid polyamine compound is placed in a continuous reaction system, and the liquid polyamine compound is circulated in the continuous reaction system. A solid bis(cyclic carbonate) and a solid catalyst are placed in the continuous reaction system to mix the solid bis(cyclic carbonate), solid catalyst, and liquid polyamine compound to form a heterogeneous mixture. The heterogeneous mixture is heated in the continuous reaction system in a microwave manner, such that the heterogeneous mixture reacts to form a polyurethane resin.
Abstract:
The present invention relates to a phosphinated poly(2,6-dimethy phenylene oxide)oligomer, specifically an unsaturated group-containing phosphinated poly(2,6-dimethy phenylene oxide)oligomer, and processes for producing the same. A thermoset produced from the unsaturated group-containing phosphinated poly(2,6-dimethy phenylene oxide)oligomers according to the present invention exhibits flame retardancy and has a low dielectric constant and dissipation factor and a high glass transition temperature.
Abstract:
The subject invention is related to a process for the epoxidation of olefin with peroxide, comprising reacting peroxide with olefin in the presence a solvent, wherein the solvent has Hansen Solubility Parameters (HSPs) of δT,solvent and δH,solvent and the epoxide product has Hansen Solubility Parameters (HSPs) of δT,product and δH,product, and wherein: δT,product−6≦δT,solvent≦δT,product+6, and δH,product−6≦δH,solvent.
Abstract:
Provided are a liquid crystal polymer (LCP) film and a laminate comprising the same. The LCP film has a first surface and a second surface opposite each other, and a Kurtosis (Rku) of the first surface ranges from 3.0 to 60.0. With the Rku, the LCP film is able to improve the peel strength with a metal foil and ensure that a laminate comprising the same maintains the merit of low insertion loss.
Abstract:
An allyl-containing resin is provided. The allyl-containing resin comprises a repeating unit comprising a structural unit represented by the following formula (I): wherein, R1 to R3 in formula (I) are as defined in the specification; the Fourier transform infrared spectrum of the allyl-containing resin has a signal intensity “a” from 1650 cm−1 to 1630 cm−1 and a signal intensity “b” from 1620 cm−1 to 1560 cm−1, and 0
Abstract:
The instant disclosure relates to phosphorus-containing compounds that can be used to form flame retardant phosphorus-containing resins, and also can serve as a hardener for a flame retardant epoxy resin compositions. In particular, the phosphorus-containing compounds are modified with acyloxy groups (—O—(C═O)—R), as shown below. Incorporation of the acyloxy groups results in resins that are water resistant and exhibit improved dielectric properties.
Abstract:
A series of novel phosphorus-containing compounds having the following formula is provided: in which: R1-R4, A, Q and m are as defined in the specification. A process for the preparation of the compound of formula (I) is also provided. A polymer of formula (PA), and preparation process and use thereof are further provided. A polymer of formula (PI), and preparation process and use thereof are also provided.
Abstract:
Provided are a liquid crystal polymer (LCP) film and a laminate comprising the same. The LCP film has a first surface and a second surface opposite each other, and a ratio of a ten-point mean roughness relative to a maximum height (Rz/Ry) of the first surface is from 0.30 to 0.62. By controlling Rz/Ry of at least one surface of the LCP film, the peel strength of the LCP film stacked to a metal foil can be increased, and the laminate comprising the same can still maintain the merit of low insertion loss.
Abstract:
Provided are a liquid crystal polymer film (LCP film) and a laminate comprising the same. The LCP film has a first surface and a second surface opposite each other, and the first surface has an arithmetical mean height of a surface (Sa) less than 0.32 μm. The LCP film with proper Sa is suitable to be stacked with a metal foil, such that a laminate comprising the LCP film can have an advantage of low insertion loss.