Abstract:
The present invention is to provide a metal particle dispersion which has low viscosity and excellent dispersibility and dispersion stability, and in which the precipitation of the metal particles is inhibited. Disclosed is a metal particle dispersion comprising metal particles, a dispersant and a solvent, wherein the metal particles contain one or more selected from the group consisting of gold, silver, copper, nickel, platinum, palladium, molybdenum, aluminum, antimony, tin, chromium, lanthanum, indium, gallium and germanium, and wherein the dispersant is a graft copolymer having at least one constitutional unit represented by the following general formula (I) and at least one constitutional unit represented by the following general formula (II), and in which at least part of nitrogen sites of the constitutional units represented by the general formula (I) each form a salt with at least one selected from the group consisting of a halogenated hydrocarbon, an acidic phosphorus compound represented by the following general formula (V), and a sulfonic acid compound represented by the following general formula (VI): (symbols shown in the general formulae (I), (II), (V) and (VI) are as described in the Description.)
Abstract:
To provide a sealing material sheet for a solar-cell module that has high productivity without performing crosslinking processing, and has a high tensile shear adhesion force at normal temperature at a high level in addition to heat resistance and molding characteristics. A sealing material sheet is a multi-layer sheet using a polyethylene-based resin as a base resin, a core layer has a density of 0.880 g/cm3 to 0.895 g/cm3 and a melting point of 70° C. or higher, a skin layer has a density of 0.880 g/cm3 to 0.910 g/cm3 and a melting point of 90° C. or lower and contains a silane-modified polyethylene-based resin, a weight average molecular weight of the silane-modified polyethylene-based resin contained in the skin layer 11 in terms of polystyrene is 70000 to 120000, and a polymerized silane amount of the skin layer in the whole resin component is 300 ppm to 2000 ppm.
Abstract:
The present invention is to provide a metal particle dispersion which has low viscosity and excellent dispersibility and dispersion stability, and in which the precipitation of the metal particles is inhibited. Disclosed is a metal particle dispersion comprising metal particles, a dispersant and a solvent, wherein the metal particles contain one or more selected from the group consisting of gold, silver, copper, nickel, platinum, palladium, molybdenum, aluminum, antimony, tin, chromium, lanthanum, indium, gallium and germanium, and wherein the dispersant is a graft copolymer having at least one constitutional unit represented by the following general formula (I) and at least one constitutional unit represented by the following general formula (II), and in which at least part of nitrogen sites of the constitutional units represented by the general formula (I) each form a salt with at least one selected from the group consisting of a halogenated hydrocarbon, an acidic phosphorus compound represented by the following general formula (V), and a sulfonic acid compound represented by the following general formula (VI): (symbols shown in the general formulae (I), (II), (V) and (VI) are as described in the Description.)
Abstract:
To provide a sealing material sheet for a solar-cell module that has high productivity without performing crosslinking processing, and has a high tensile shear adhesion force at normal temperature at a high level in addition to heat resistance and molding characteristics. A sealing material sheet is a multi-layer sheet using a polyethylene-based resin as a base resin, a core layer has a density of 0.880 g/cm3 to 0.895 g/cm3 and a melting point of 70° C. or higher, a skin layer has a density of 0.880 g/cm3 to 0.910 g/cm3 and a melting point of 90° C. or lower and contains a silane-modified polyethylene-based resin, a weight average molecular weight of the silane-modified polyethylene-based resin contained in the skin layer 11 in terms of polystyrene is 70000 to 120000, and a polymerized silane amount of the skin layer in the whole resin component is 300 ppm to 2000 ppm.
Abstract:
To provide a sealing material sheet for a solar-cell module that has high productivity, and can also suppress unevenness in thickness at the time of integration as a solar-cell module. There is provided a sealing material sheet 1 in which there are two inflection point temperatures that are temperatures only around which a change rate of the linear expansion coefficient locally increases, a first inflection point temperature at a low temperature side of two inflection point temperatures is within a range of 55° C. to 70° C., and a second inflection point at a high temperature side of the inflection point temperatures is within a range of 80° C. to 95° C.