Abstract:
The invention provides a composition comprising the following components: A) an anhydride and/or carboxylic acid functionalized ethylene/alpha-olefin interpolymer having the following properties: i) a melt viscosity (177 C) less than, or equal to, 50,000 cP, ii) a density from 0.855 to 0.900 g/cc; B) a tackifier selected from the following: a) a hydrocarbon tackifier that has a cloud point (DACP) temperature greater than, or equal to, 20 C, b) a rosin ester tackifier with an acid number of less than 25, c) a terpene tackifier, or d) a combination thereof.
Abstract:
A process to form an olefin-based polymer, said process comprising at least the following steps: a) polymerizing a reaction mixture comprising an olefin, in at least one reactor, in a solution polymerization, to form a polymer solution; b) feeding at least a portion of the polymer solution through at least one devolatilizer, to form the olefin-based polymer, in melt form; c) feeding at least a portion of the olefin-based polymer, in melt, form through a heat exchanger, and then into a pastillation apparatus to form polymer particles.
Abstract:
A stretch-modified elastomeric multilayer film comprising a core layer comprising a first ethylene-α-olefin block copolymer, wherein the first ethylene-α-olefin block copolymer comprises at least 50 mol. % ethylene, has a melt index (I2) from 0.5 g/10 min to 5 g/10 min, and has a density of 0.850 g/cc to 0.890 g/cc, and at least one outer layer independently comprising a second ethylene-α-olefin block copolymer and from 2.5 to 30 wt. % of an antiblock agent, wherein the second ethylene-α-olefin block copolymer comprises at least 50 mol. % ethylene, has a melt index (I2) from 0.5 g/10 min to 25 g/10 min, and has a density of 0.850 g/cc to 0.890 g/cc, wherein the density of the first ethylene-α-olefin block copolymer is equal to or greater than the density of the second ethylene-α-olefin block copolymer.
Abstract:
A stretch-modified elastomeric multilayer film comprising a core layer comprising a first ethylene-α-olefin block copolymer, wherein the first ethylene-α-olefin block copolymer comprises at least 50 mol. % ethylene, has a melt index (12) from 0.5 g/10 min to 5 g/10 min, and has a density of 0.850 g/cc to 0.890 g/cc, and at least one outer layer independently comprising a second ethylene-α-olefin block copolymer and from 2.5 to 30 wt. % of an antiblock agent, wherein the second ethylene-α-olefin block copolymer comprises at least 50 mol. % ethylene, has a melt index (12) from 0.5 g/10 min to 25 g/10 min, and has a density of 0.850 g/cc to 0.890 g/cc, wherein the density of the first ethylene-α-olefin block copolymer is equal to or greater than the density of the second ethylene-α-olefin block copolymer.