摘要:
A method is disclosed for improving the uniformity and durability of a pyrolytically deposited metal oxide film on glass by cooling the coating solution and/or the atomizing air prior to the application of the coating composition to the hot glass surface.
摘要:
A metal reactant, dissolved in a volatile solvent, is sprayed into converging reactive carrier gas streams, is vaporized and is carried past a heater for ultimate discharge against a heated substrate whereupon the metal reactant and a portion of the reactive gas streams react to form an adherent coating on the substrate.
摘要:
This invention relates to a two layers or more anti-static film coating deposited on a substrate. Selected layers of the films may have anti-static and/or electromagnetic properties. In one embodiment, the film farthest from the substrate has an index of refraction lower than the underlying film. In another embodiment, the surface of the film is roughened to provide a graded index of refraction.
摘要:
A method is disclosed for depositing a coating from a gaseous stream of a powder coating reactant, wherein the carrier gas is supplied at a high volume rate (at least 100 cubic ft./min) and low pressure (not greater than one psi).
摘要:
An apparatus for coating a glass ribbon has an exhaust on each side of a coating unit at different distances therefrom. With this arrangement, portions of the ribbon upstream and downstream of the coating unit are exposed to coating vapors from the coating unit for different periods of time. A coating mixture includes tin containing precursors and a silicon containing precursor. The silicon containing precursor has the structural formula ##STR1## where R.sub.1 is a group which does not have an oxygen available to form a peroxide, R.sub.2 is a functional group giving the silicon containing precursor the ability to be easily converted to silicon oxide coating, R.sub.3 is a bridging group to provide for multiple silicon atoms and R.sub.4 completes the bonding on the foundation silicon atom. An accelerant e.g. a phosphorus containing precursor may be used with the metal containing precursors to increase the deposition rate of the coating. The coating deposited on the glass has regions of continuously varying weight percent of silicon oxide and tin oxide as the distance from the glass-coating interface increases, with the surface of the coating farthest from the glass-coating interface being predominantly tin oxide. The regions within the coating provide the coating with different indices of refraction to eliminate iridescence resulting from increased thickness of the tin oxide at the outer coating surface and to provide the coated glass article with a neutral color. When phosphorus is used as the accelerant, the percent of crystallinity is reduced and approaches O, thereby reducing or eliminating the coating haze.
摘要:
The durability of a transparent pyrolytic spray applied coating is improved by providing a spray solution of metal acetylacetonates having different particle size distribution. More particularly, the particle size distribution of each of the metal acetylacetonates is a function of its melting temperature, and optionally of its melting temperature and solubility.
摘要:
A metal oxide coating is applied to a hot glass surface by contacting the surface with a mixture of carrier air, vaporized solvent and a vaporized metal containing reactant. The mixture is directed against the glass through an elongated, converging slot-nozzle, the interior surfaces of which have an increasing radius of curvature towards the exit end, nozzle at a Reynolds number exceeding 2500 with the nozzle-to-glass spacing at least 1.25 times the characteristic dimension of the nozzle.
摘要:
A coating apparatus includes non-orthogonal coater geometry to improve coatings on a glass ribbon, and to improve yields of such coatings. The apparatus includes a first arrangement to move the ribbon along a first imaginary straight line through a coating zone provided in a glass forming chamber. The coater has a coating nozzle and an exhaust slot, each have a longitudinal axis. The coating nozzle directs coating vapors toward the coating zone, and the exhaust slot removes vapors from the coating zone. A second arrangement mounts the coater in spaced relation to the path with the coating nozzle and the exhaust slot facing the coating zone. A second imaginary straight line is normal to the longitudinal axis of the coating nozzle, and the first imaginary line and the second imaginary line subtend an angle in the range of greater than zero degrees to 90 degrees.
摘要:
A coating apparatus includes non-orthogonal coater geometry to improve coatings on a glass ribbon, and to improve yields of such coatings. The apparatus includes a first arrangement to move the ribbon along a first imaginary straight line through a coating zone provided in a glass forming chamber. The coater has a coating nozzle and an exhaust slot, each have a longitudinal axis. The coating nozzle directs coating vapors toward the coating zone, and the exhaust slot removes vapors from the coating zone. A second arrangement mounts the coater in spaced relation to the path with the coating nozzle and the exhaust slot facing the coating zone. A second imaginary straight line is normal to the longitudinal axis of the coating nozzle, and the first imaginary line and the second imaginary line subtend an angle in the range of greater than zero degrees to 90 degrees.
摘要:
The durability of a transparent pyrolytic spray applied coating is improved by providing a spray solution of metal acetylacetonates having different particle size distribution. More particularly, the particle size distribution of each of the metal acetylacetonates is a function of its melting temperature, and optionally of its melting temperature and solubility.