1.
公开(公告)号:US5973104A
公开(公告)日:1999-10-26
申请号:US955065
申请日:1997-10-21
IPC分类号: B01F7/04 , B29B7/46 , B29B7/48 , B29C47/38 , C08G63/668 , C08G63/78 , C08G63/91 , C08G65/48 , C08G85/00 , C08G63/12 , C08L67/00
CPC分类号: C08G63/914 , B29B7/46 , B29B7/487 , B29C47/38 , C08G63/668 , B29C47/0021
摘要: A film-formable high molecular polyetherpolyester comprising structural unit (1) of formula (1) and functional group (2) of formula (2) and having a number-average molecular weight of 40,000 to 10,000,000, wherein the molar ratio of functional group (2) to R in the polyetherpolyester is in the range of 1.0 to 3.0. This polyetherpolyester can be produced by carrying out a chain extension reaction of a low molecular polyalkylene oxide of 1,000 to 30,000 in number-average molecular weight with a polyvalent acid anhydride at 0.003 MPa or higher in a molar ratio of (acid anhydride group)/(hydroxyl group)=0.8 to 1.0. ##STR1##
摘要翻译: 一种可成膜的高分子量聚醚聚酯,其包含式(1)的结构单元(1)和式(2)的官能团(2),其数均分子量为40,000至10,000,000,其中官能团 2)与聚醚多酯中的R的摩尔比为1.0-3.0。 该聚醚多酯可以通过使数均分子量为1,000〜30,000的低分子量聚环氧烷与多元酸酐在0.003MPa以上以(酸酐基)/( 羟基)= 0.8〜1.0。
-
公开(公告)号:US5843573A
公开(公告)日:1998-12-01
申请号:US547837
申请日:1995-10-25
IPC分类号: C08K3/00 , C08G63/16 , C08G63/42 , C08G63/66 , C08J5/18 , C08K3/34 , C08K3/38 , C08K5/00 , C08L67/00 , C08L67/02 , C08L101/16 , D02G3/00
CPC分类号: C08J5/18 , C08K3/34 , C08K3/38 , C08L67/02 , C08J2367/02 , Y10T428/2913
摘要: A polyester resin composition comprises: an aliphatic polyester having a number-average molecular weight (Mn) in a range of 10,000 to 100,000; and a crystalline nucleating agent, wherein the aliphatic polyester and the crystalline nucleating agent are mixed in such that a half value width of an exothermic peak based on an annealing crystallization of the aliphatic polyester measured by differential scanning calorimetry in an atmosphere of nitrogen at a cooling rate of 3K/minute is not more than 15K. This polyester resin composition has a biodegradability and a high crystallization rate. The polyester resin composition also has excellent mechanical properties and eliminates a precise temperature control during a molding process which saves labor force resulting in desirable moldability and productivity. For the described beneficial properties, the polyester resin composition can be readily processed into a fiber, a molded article, sheet, film and the like. Accordingly, a film made of the polyester resin composition can be effectively used for disposable packing materials, miscellaneous goods for daily use, and the like.
摘要翻译: 聚酯树脂组合物包括:数均分子量(Mn)在10,000至100,000范围内的脂族聚酯; 和结晶成核剂,其中将脂肪族聚酯和结晶成核剂混合,使得基于通过差示扫描量热法在氮气氛中测量的脂肪族聚酯在冷却下的退火结晶的放热峰的半值宽度 速度3K /分钟不超过15K。 该聚酯树脂组合物具有生物降解性和高结晶速率。 聚酯树脂组合物还具有优异的机械性能,并且在模制过程中消除了精确的温度控制,这节省了劳动力,从而产生所需的成型性和生产率。 对于所述的有益性质,可以容易地将聚酯树脂组合物加工成纤维,模塑制品,片材,薄膜等。 因此,由聚酯树脂组合物制成的薄膜可以有效地用于一次性包装材料,日用杂货品等。
-
公开(公告)号:US5616681A
公开(公告)日:1997-04-01
申请号:US550964
申请日:1995-10-31
CPC分类号: C08G18/4244 , C08G18/4291 , C08G63/42 , C08G63/78 , C08G63/823 , C08G63/84 , C08G63/85 , C08G2230/00
摘要: A method for producing an aliphatic polyester having a biodegradability and a higher melting point than conventional aliphatic polyester by suppressing a volatile component generated by side reaction or decomposition reaction with industrially good efficiency and economically in a relatively short period of time, the method enabling a polymerization at vacuum which permits a use of general vacuum pump. The aliphatic polyester can be obtained, for example, by a ring-opening copolymerization of a cyclic acid anhydride with a cyclic ether in a presence of a zirconium compound. The aliphatic polyester also can be obtained by performing a polymerization of raw materials of the aliphatic polyester so as to have a degree of viscosity in the range of 10-10,000 poise when 0.1-30 hours elapsed after the reaction started at reaction temperature of the reaction system under conditions of reaction temperature in the range of 180.degree. C. to 280.degree. C. and reaction pressure in the range of 0.3 mmHg to 3.0 mmHg.
摘要翻译: 通过抑制由副反应或分解反应产生的挥发性成分,具有生物降解性和熔点比普通脂肪族聚酯高的脂肪族聚酯的制造方法,具有工业上良好的效率和经济地在相当短的时间内生产的方法,能够进行聚合的方法 在允许使用一般真空泵的真空下。 脂肪族聚酯可以通过例如在锆化合物的存在下通过环状酸酐与环状醚的开环共聚获得。 脂肪族聚酯也可以通过进行脂肪族聚酯的原料的聚合而获得,使得在反应开始后的反应开始0.1〜30小时后,粘度在10〜10000泊的范围内 系统在反应温度在180℃至280℃的范围内,反应压力在0.3mmHg至3.0mmHg的范围内。
-
公开(公告)号:US20120204771A1
公开(公告)日:2012-08-16
申请号:US13500099
申请日:2010-09-24
申请人: Koji Fukuhara
发明人: Koji Fukuhara
IPC分类号: A47B5/04
CPC分类号: A47B5/04 , B60N3/002 , B64D11/0638 , Y02T50/46
摘要: A folding table is provided that includes: a table frame that enables a table body to move between the in-use position and the stowed position, that is disposed within the table body, and that supports the table body; a support member that pivotably supports the table frame; and a lock, provided in a position where the support member and the table frame are linked, that holds the table frame in the in-use position and prevents the table frame from pivoting. The lock has: a retaining member in which an engagement groove is formed; a pivoting member capable of engaging with and disengaging from the engagement groove; and a lock biaser that biases the pivoting member in the direction of engagement with the engagement groove.
摘要翻译: 提供一种折叠台,其包括:台架,其能够使台体在使用位置和收纳位置之间移动,其设置在桌子主体内,并且支撑桌子主体; 可枢转地支撑台架的支撑构件; 以及设置在所述支撑构件和所述台架被连接的位置的锁,其将所述台架保持在使用位置并防止所述台架枢转。 锁具有:形成有接合槽的保持构件; 枢转构件,其能够与所述接合槽接合和脱离; 以及锁定冲击器,其将枢转构件沿与接合槽接合的方向偏压。
-
公开(公告)号:US20120289626A1
公开(公告)日:2012-11-15
申请号:US13521012
申请日:2011-01-07
申请人: Toyoharu Nawa , Mari Masanaga , Koji Fukuhara
发明人: Toyoharu Nawa , Mari Masanaga , Koji Fukuhara
IPC分类号: C04B24/32
CPC分类号: C04B40/0039 , C04B28/02 , C04B2103/58 , C04B2111/29 , C04B2111/34 , C08L71/02 , C04B24/32 , C04B2103/304 , C04B2103/306 , C04B2103/50 , C04B24/08 , C04B24/16 , C04B24/226
摘要: Provided is a hydraulic material composition, including cement and a shrinkage-reducing agent for a hydraulic material, which does not require a combination with any other admixture, is inexpensive, and is capable of suppressing a reduction in strength of a hardened concrete material, suppressing generation of a crack in a hardened concrete material by virtue of its excellent shrinkage-reducing ability, and imparting excellent freeze-thaw resistance. The hydraulic material composition includes cement and a shrinkage-reducing agent for a hydraulic material including at least one kind of polyoxyalkylene compound (A) as an essential component, and has a spacing factor of 350 μm or less.
摘要翻译: 提供一种水硬性材料组合物,其包含水泥和用于水硬性材料的减缩剂,其不需要与任何其它混合物的组合是便宜的,并且能够抑制硬化混凝土材料的强度降低,抑制 通过其优异的减缩能力,在硬化的混凝土材料中产生裂纹,赋予优异的抗冻融性。 水硬性材料组合物包括水泥材料和包含至少一种聚氧化烯化合物(A)作为必要成分的水硬性材料的减缩剂,并且间隔系数为350μm以下。
-
公开(公告)号:US07875115B2
公开(公告)日:2011-01-25
申请号:US11653070
申请日:2007-01-12
申请人: Katsuhiko Nakai , Koji Fukuhara
发明人: Katsuhiko Nakai , Koji Fukuhara
摘要: This disclosure is aimed at providing a method for producing an epitaxial wafer allowing uniform occurrence of oxygen precipitate in a substrate plane in the radial direction in a base plate and excelling in the crystal quality of an epi-layer.A method for the production of an epitaxial wafer, characterized by using as a substrate a base plate of nitrogen- and carbon-added silicon single crystal having a nitrogen concentration of 5×1014 to 5×1015 atoms/cm3 and a carbon concentration of 1×1016 to 1×1018 atoms/cm3, having a crystal growth condition during the production of silicon single crystal in a range in which the whole surface of substrate becomes an OSF region, and being pulled at a cooling speed of not less than 4° C./minute between 1100 and 1000° C. during the growth of crystal, and depositing the silicon single crystal layer on the surface of the substrate by the epitaxial method.
摘要翻译: 本公开内容旨在提供一种用于制造外延片的方法,其允许在基板中在径向方向上的基板平面中均匀地发生氧沉淀,并且具有优异的外延层的晶体质量。 一种外延晶片的制造方法,其特征在于,使用氮浓度为5×10 14〜5×10 15原子/ cm 3,碳浓度为1的氮和碳添加硅单晶的基板作为基板 ×1016〜1×1018原子/ cm3,在制造硅单晶时,在基板的整个表面成为OSF区域的范围内具有晶体生长条件,并且以不小于4°的冷却速度 在晶体生长期间在1100和1000℃之间/分钟,并通过外延法将硅单晶层沉积在衬底的表面上。
-
公开(公告)号:US07053575B2
公开(公告)日:2006-05-30
申请号:US10752147
申请日:2004-01-06
申请人: Koji Fukuhara , Hiromasa Matsushiro
发明人: Koji Fukuhara , Hiromasa Matsushiro
IPC分类号: H02K1/00
CPC分类号: B60N2/12 , B60N2/0244 , B60N2/0292
摘要: A method for controlling operations of power seats for a vehicle, comprises the steps of moving a first seat toward a second seat by a first reversible motor, causing a seat cushion of the first seat to be tipped up, by a second reversible motor, relative to a seat back of the first seat which stands up, sensing loads which are applied to the first and second reversible motors, once stopping the driving of the first reversible motor, when excessive load of the first reversible motor is sensed during the movement of the first seat toward the second seat, thereafter returning the first seat to a position at which the excessive load of the first reversible motor is not sensed and stopping the movement of the first seat, once stopping the tipping-up of the seat cushion, when excessive load of the second reversible motor is sensed during the tipping-up of the seat cushion, and thereafter returning the seat cushion to an original posture thereof and stopping the movement of the seat cushion.
摘要翻译: 一种用于控制用于车辆的动力座椅的操作的方法,包括以下步骤:通过第一可逆电动机将第一座椅朝向第二座椅移动,通过第二可逆电动机相对于第一座椅的座垫向上倾斜 在第一座椅的座椅靠背上站起来,一旦停止第一可逆电动机的驱动,则感测施加到第一和第二可逆电动机的负载,当在第一可逆电动机的运动期间感测到第一可逆电动机的过度负载时 第一座椅朝向第二座椅,然后一旦停止座垫的翻倒,将第一座椅返回到没有感测到第一可逆电动机的过度负载的位置并停止第一座椅的移动,当过度 在座垫倾翻期间感测到第二可逆电动机的负载,然后使座垫返回到其原始姿势并停止座垫的移动。
-
公开(公告)号:US08763538B2
公开(公告)日:2014-07-01
申请号:US13500099
申请日:2010-09-24
申请人: Koji Fukuhara
发明人: Koji Fukuhara
IPC分类号: A47B1/04
CPC分类号: A47B5/04 , B60N3/002 , B64D11/0638 , Y02T50/46
摘要: A folding table is provided that includes: a table frame that enables a table body to move between the in-use position and the stowed position, that is disposed within the table body, and that supports the table body; a support member that pivotably supports the table frame; and a lock, provided in a position where the support member and the table frame are linked, that holds the table frame in the in-use position and prevents the table frame from pivoting. The lock has: a retaining member in which an engagement groove is formed; a pivoting member capable of engaging with and disengaging from the engagement groove; and a lock biaser that biases the pivoting member in the direction of engagement with the engagement groove.
摘要翻译: 提供一种折叠台,其包括:台架,其能够使台体在使用位置和收纳位置之间移动,其设置在桌子主体内,并且支撑桌子主体; 可枢转地支撑台架的支撑构件; 以及设置在所述支撑构件和所述台架被连接的位置的锁,其将所述台架保持在使用位置并防止所述台架枢转。 锁具有:形成有接合槽的保持构件; 枢转构件,其能够与所述接合槽接合和脱离; 以及锁定冲击器,其将枢转构件沿与接合槽接合的方向偏压。
-
公开(公告)号:US08545622B2
公开(公告)日:2013-10-01
申请号:US11645017
申请日:2006-12-22
申请人: Katsuhiko Nakai , Koji Fukuhara
发明人: Katsuhiko Nakai , Koji Fukuhara
IPC分类号: C30B15/02
CPC分类号: H01L21/3225 , C30B15/04 , C30B15/203 , C30B29/06 , C30B33/02
摘要: An annealed wafer in which oxygen precipitation is uniform in the substrate plane and a manufacturing method thereof are provided. A nitrogen-doped silicon single crystal substrate pulled at the cooling rate of 4° C./minute or more during crystal growth between 1100 and 1000° C. wherein the nitrogen concentration is 1×1014 to 5×1015 atoms/cm3 and V/G satisfies predetermined conditions serves as a substrate, and the substrate is subjected to heat treatment in a non-oxidative atmosphere.
摘要翻译: 提供了在基板平面中氧析出均匀的退火晶片及其制造方法。 氮掺杂的硅单晶衬底在1100-1000℃的晶体生长期间以4℃/分钟以上的冷却速度拉伸,其中氮浓度为1×1014至5×1015原子/ cm3,V / G满足预定条件用作基板,并且在非氧化性气氛中对基板进行热处理。
-
公开(公告)号:US20070155134A1
公开(公告)日:2007-07-05
申请号:US11645017
申请日:2006-12-22
申请人: Katsuhiko Nakai , Koji Fukuhara
发明人: Katsuhiko Nakai , Koji Fukuhara
IPC分类号: H01L21/322
CPC分类号: H01L21/3225 , C30B15/04 , C30B15/203 , C30B29/06 , C30B33/02
摘要: An annealed wafer in which oxygen precipitation is uniform in the substrate plane and a manufacturing method thereof are provided. A nitrogen-doped silicon single crystal substrate pulled at the cooling rate of 4° C./minute or more during crystal growth between 1100 and 1000° C. wherein the nitrogen concentration is 1×1014 to 5×1015 atoms/cm3 and V/G satisfies predetermined conditions serves as a substrate, and the substrate is subjected to heat treatment in a non-oxidative atmosphere.
摘要翻译: 提供了在基板平面中氧析出均匀的退火晶片及其制造方法。 在1100和1000℃之间的晶体生长期间,以4℃/分钟或更高的冷却速率拉制氮掺杂硅单晶衬底,其中氮浓度为1×10 14至5×10 10 > 15原子/ cm 3和V / G满足预定条件用作基底,并且在非氧化性气氛中对基片进行热处理。
-
-
-
-
-
-
-
-
-