Abstract:
A steel sheet for cans which exhibits excellent weldability; and a production method therefor include a steel sheet for cans with the surface of a steel sheet in order from the steel sheet side, a chromium metal layer and a hydrous chromium oxide layer. The deposited amount of the chromium metal layer is 65-200 mg/m2. The deposited amount of the hydrous chromium oxide layer in terms of chromium is 3-30 mg/m2. The chromium metal layer includes: a base part having a thickness of 7.0 nm or higher; and granular protrusions which are on the base part, have a maximum grain size of 100 nm or lower, and have a number density per unit area of at least 200 per μm2.
Abstract:
A steel sheet for cans has, on the surface thereof, in order from the steel sheet side, a chromium metal layer and a hydrous chromium oxide layer. The chromium metal layer is deposited in an amount of 50-200 mg/m2, and the hydrous chromium oxide layer is deposited in an amount of 3-15 mg/m2 in terms of chromium. The chromium metal layer includes: a flat chromium metal layer that has a thickness of at least 7 nm; and a granular chromium metal layer that includes granular protrusions that are formed on the surface of the flat chromium metal layer. The maximum grain size of the granular protrusions is 150 nm or smaller. The number density of the granular protrusions per unit area is 10/μm2 or higher.
Abstract:
A steel sheet for cans has, on the surface thereof, in order from the steel sheet side, a chromium metal layer and a hydrous chromium oxide layer. The chromium metal layer is deposited in an amount of 50-200 mg/m2, and the hydrous chromium oxide layer is deposited in an amount of 3-15 mg/m2 in terms of chromium. The chromium metal layer includes: a flat chromium metal layer that has a thickness of at least 7 nm; and a granular chromium metal layer that includes granular protrusions that are formed on the surface of the flat chromium metal layer. The maximum grain size of the granular protrusions is 150 nm or smaller. The number density of the granular protrusions per unit area is 10/μm2 or higher.
Abstract:
A can steel plate includes: equal or less than 0.0030% by mass of C; equal or less than 0.02% by mass of Si; 0.05-0.60% by mass of Mn; equal or less than 0.020% by mass of P; equal or less than 0.020% by mass of S; 0.010% to 0.100% by mass of Al; 0.0010-0.0050% by mass of N; 0.001-0.050% by mass of Nb; and balance Fe and impurities. Intensity of (111) [1-21] orientation (where −2 represents 2 with bar in Miller indices) and intensity of (111)[1-10] orientation (where −1 represents 1 with bar in Miller indices) satisfy the following equation (1), and in a rolling direction and 90° direction from the rolling direction in a horizontal plane, tensile strength TS (MPa) and fracture elongation El (%) satisfy relations of the following equations (2) and (3). (Intensity of (111) [1-21] orientation)/(Intensity of (111) [1-10] orientation)>0.9 . . . (1), TS>550 . . . (2), El>−0.02×TS+17.5 . . . (3).
Abstract:
Provided are a laminated metal sheet for containers that has excellent formability after heat treatment performed after coating, printing, etc. and is suitable for DR cans, a method for producing a metal can using the above metal sheet and a method for evaluating the formability of a metal sheet. The crystal structure of a top layer of a laminate layer of the laminated metal sheet for containers and the crystal structure inside the laminate layer are controlled in a sophisticated manner. Specifically, the intensity ratio I2968/I3085 of the Raman band intensity (I2968) at a peak position around 2,968 cm−1 to the Raman band intensity (I3085) at a peak position around 3,085 cm−1 that are obtained by laser Raman spectroscopy is used. This intensity ratio is controlled within a specific range.
Abstract:
Provided are: a multilayer structure in which a titanium oxide layer exhibits excellent photocatalytic activity; and a method for producing this multilayer structure. The above-described multilayer structure comprises: a conductive part which contains a metal element A other than Ti, while having electrical conductivity; and a titanium oxide layer which is arranged on the conductive part and contains 1.0% by atom or more of the metal element A.
Abstract:
A laminated metal sheet for a two-piece can includes: a metal sheet; and first and second polyester resin layers formed on outer and inner face sides of the container, respectively. The first polyester resin layer contains polyethylene terephthalate or a copolymerized polyethylene terephthalate with a content of a copolymerized component of less than 6 mol % in a ratio of 30% to 60% by mass, polybutylene terephthalate or a copolymerized polybutylene terephthalate with a content of a copolymerized component of less than 5 mol % in a ratio of 40% to 70% by mass, and a polyolefinic wax in an amount of 0.01% to 3.0% in outer percentage, the second polyester resin layer is a copolymerized polyethylene terephthalate with a content of a copolymerized component of less than 22 mol %, and residual degrees of orientation of the first and the second polyester resin layers are less than 30%.
Abstract:
A laminated metal sheet includes a metal sheet, a first polyester resin layer, and a second polyester resin layer, and the first polyester resin layer contains 30% by mass to 60% by mass of: polyethylene terephthalate; or copolymerized polyethylene terephthalate having a copolymerization component content of less than 6 mol %; and 40% by mass to 70% by mass of polybutylene terephthalate, the second polyester resin layer is copolymerized polyethylene terephthalate having a copolymerization component content of less than 14 mol %, residual orientations of the first and second polyester resin layers are less than 20%, and film thicknesses X and Y of the first and the second polyester resin layers before forming satisfy predetermined conditions.
Abstract:
A first polyester resin layer formed on a surface of a metal sheet to serve as the exterior of a container after being formed into the container contains 30% to 60% by mass of poly-ethylene terephthalate or copolymerized polyethylene terephthalate having a copolymerization component content of less than 6 mol %, and 40% to 70% by mass of polybutylene terephthalate. A second polyester resin layer formed on a surface of the metal sheet to serve as the interior of a container after being formed into the container is copolymerized polyethylene terephthalate having a copolymerization component content of less than 14 mol %. The degree of residual orientation of the first and the second polyester resin layers is in a range of 2% to 50%. The thicknesses of the first and the second polyester resin layers after lamination are not less than 6 μm.
Abstract:
There is provided a steel sheet for cans including, on a surface of a steel sheet, a chromium metal layer and a hydrated chromium oxide layer stacked in this order from the steel sheet side. The chromium metal layer has a coating weight of 50 to 200 mg/m2, and the hydrated chromium oxide layer has a coating weight of 3 to 30 mg/m2 in terms of chromium amount. The chromium metal layer includes a base portion of flat plate shape and granular protrusions provided on the base portion. At least 20% of the granular protrusions has a circularity C of 0.85 or less. The circularity C is expressed by C=4πA/U2, when the outer perimeter of a projection image of a granular protrusion is represented by U, and the area thereof is represented by A.