摘要:
A process for preparing a blend of thermoplastic polymer and resin modifier within a single-screw extruder, wherein the resin modifier is a hydrocarbon resin.
摘要:
Disclosed herein is a nonwoven fabric comprising within the range of from 50 to 99 wt %, by weight of the composition, of a reactor grade propylene-α-olefin copolymer possessing within the range of from 5 to 35 wt %, by weight of the copolymer, of units derived from one or more of ethylene and/or C4 to C12 α-olefins; a melt flow rate (230° C./2.16 kg) within the range of from 500 to 7500 g/10 min; and a weight average molecular weight of less than 200,000; and a second polypropylene having a melting point, Tm, of greater than 110° C. and a melt flow rate (230° C./2.16 kg) within the range of from 20 to 7500 g/10 min; wherein the fabric has a CD Elongation value of greater than 50% (measuring the fabric of 35 g/m2 basis weight). The fabric described herein can be used in structures comprising one or more layers of the fabric described herein, and can include any number of other fabric layers made from other materials.
摘要:
A non-woven fabric made from a composition prepared by combining a first propylene-based polymer blend, where the first polymer blend is prepared by combining a propylene-based elastomer with a propylene-based thermoplastic resin and where the first blend has an MFR (ASTM D-1238 2.16 kg @ (230° C.) equal to or less than 50 dg/min, with a second propylene-based polymer blend, where the second polymer blend is prepared by combining a propylene-based elastomer with a propylene-based thermoplastic resin and where said second blend has an MFR (ASTM D-1238 2.16 kg @ 230° C.) greater than 50 dg/min, where the propylene-based elastomers comprise from about 5% to 35% by weight units derived from ethylene or non-propylene alpha-olefin and have a heat of fusion, as determined by DSC, of less than 80 J/g, and where the propylene-based thermoplastic resins have a heat of fusion, as determined by DSC, equal to or greater than 80 J/g.
摘要:
Disclosed herein is a nonwoven fabric comprising within the range of from 50 to 99 wt %, by weight of the composition, of a reactor grade propylene-α-olefin copolymer possessing within the range of from 5 to 35 wt %, by weight of the copolymer, of units derived from one or more of ethylene and/or C4 to C12 α-olefins; a melt flow rate (230° C./2.16 kg) within the range of from 500 to 7500 g/10 min; and a weight average molecular weight of less than 200,000; and a second polypropylene having a melting point, Tm, of greater than 110° C. and a melt flow rate (230° C./2.16 kg) within the range of from 20 to 7500 g/10 min; wherein the fabric has a CD Elongation value of greater than 50% (measuring the fabric of 35 g/m2 basis weight). The fabric described herein can be used in structures comprising one or more layers of the fabric described herein, and can include any number of other fabric layers made from other materials.
摘要:
The present invention relates to plasticized polyolefin compositions comprising a polyolefin and a non-functionalized plasticizer; wherein the non-functionalized plasticizer may comprise C6 to C200 paraffins (including branched and normal paraffins) having a pour point of less than −5° C. In one embodiment, the non-functionalized plasticizer is an isoparaffin comprising C6 to C25 isoparaffins. In another embodiment the non-functionalized plasticizer is a polyalphaolefin comprising C10 to C100 n-paraffins. The polyolefin may be a polypropylene homopolymer, copolymer, impact copolymer, or blends thereof, and may include a plastomer. Non-limiting examples of desirable article of manufacture made from compositions of the invention include films, tubes, pipes, sheets, fibers, woven and nonwoven fabrics, automotive components, furniture, sporting equipment, food storage containers, transparent and semi-transparent articles, toys, tubing and pipes, and medical devices.
摘要:
The present invention relates to polypropylene copolymer alloys which are especially suited for soft fiber and fabric applications. These alloys comprise an ethylene-propylene random copolymer having an ethylene content of from about 1.0 to 5.0% by weight, in an amount of from about 40 to 90% by weight of the alloy; and an ethylene-propylene bipolymer having an ethylene content of from about 10 to 30% by weight, in an amount of from about 10 to 60% by weight of the alloy. The present invention further relates to fiber and fabric articles made from such alloys.
摘要:
The present invention relates to fibers and nonwovens made from plasticized polyolefin compositions comprising a polyolefin, a non-functionalized hydrocarbon plasticizer and a slip agent.
摘要:
Disclosed herein is a nonwoven fabric comprising within the range of from 50 to 99 wt %, by weight of the composition, of a reactor grade propylene-α-olefin copolymer possessing within the range of from 5 to 35 wt %, by weight of the copolymer, of units derived from one or more of ethylene and/or C4 to C12 α-olefins; a melt flow rate (230° C./2.16 kg) within the range of from 500 to 7500 g/10 min; and a weight average molecular weight of less than 200,000; and a second polypropylene having a melting point, Tm, of greater than 110° C. and a melt flow rate (230° C./2.16 kg) within the range of from 20 to 7500 g/10 min; wherein the fabric has a CD Elongation value of greater than 50% (measuring the fabric of 35 g/m2 basis weight). The fabric described herein can be used in structures comprising one or more layers of the fabric described herein, and can include any number of other fabric layers made from other materials.
摘要:
The present invention relates to fibers and nonwovens made from plasticized polyolefin compositions comprising a polyolefin, a non-functionalized hydrocarbon plasticizer and a slip agent.