摘要:
Provided herein are foamed cement composition that comprises a hydraulic cement, water, a gas, a foaming and stabilizing surfactant, and a fluid loss control additive comprising a copolymer.
摘要:
Provided herein are settable spotting compositions that comprise cement kiln dust and associated methods of use. Also provided are methods that comprise providing a settable spotting composition comprising cement kiln dust; introducing the settable spotting composition into a well bore that penetrates the subterranean formation so as to displace at least a portion of a second fluid from the well bore.
摘要:
The present invention relates to foamed cement slurries, additives and methods. A foamed cement slurry of the invention comprises a hydraulic cement, sufficient water to form a slurry, sufficient gas to form a foam and an environmentally benign foaming and stabilizing additive comprising a mixture of an ammonium salt of an alkyl ether sulfate surfactant, a cocoamidopropyl betaine surfactant, a cocoamidopropyl dimethylamine oxide surfactant, sodium chloride and water.
摘要:
The present invention includes methods of cementing, cement compositions and a suspending agent comprising boron treated low molecular weight dry ground guar splits. A cement composition of the invention comprises hydraulic cement, water and a boron treated low molecular weight dry ground guar splits suspending agent. A method of cementing comprising the steps of preparing a cement composition that comprises hydraulic cement, water and a suspending agent comprising boron treated low molecular weight dry ground guar splits; placing the cement composition in a location to be cemented; and allowing the cement composition to set.
摘要:
The present invention provides cement compositions that comprise water, high alumina cement, a soluble phosphate, and cement kiln dust. The cement compositions optionally may be foamed with a gas. Methods of cementing also are provided that comprise: providing the cement composition; introducing the cement composition into a location to be cemented; and allowing the cement composition to set therein. The location to be cemented may be above ground or in a subterranean formation.
摘要:
The present invention provides settable compositions that comprise water and cement kiln dust. The settable compositions optionally may comprise an additive that comprises at least one of the following group: fly ash; shale; slag cement; zeolite; metakaolin; and combinations thereof. The settable compositions optionally may be foamed with a gas. Methods of cementing also are provided that comprise: providing the settable composition; introducing the settable composition into a location to be cemented; and allowing the settable composition to set therein. The location to be cemented may be above ground or in a subterranean formation.
摘要:
Methods of cementing and low density foamed cement compositions therefor are disclosed. A low density foamed cement composition of the invention comprises fly ash comprising calcium oxide or calcium hydroxide, water present in an amount sufficient to form a slurry, a foaming and foam stabilizing surfactant or a mixture of surfactants present in an amount sufficient to facilitate foam and stabilize the foamed cement composition, and sufficient gas to foam the foamed cement composition.
摘要:
The present invention provides settable compositions that comprise water and cement kiln dust. The settable compositions optionally may comprise an additive that comprises at least one of the following group: fly ash; shale; slag cement; zeolite; metakaolin; and combinations thereof. The settable compositions optionally may be foamed with a gas. Methods of cementing also are provided that comprise: providing the settable composition; introducing the settable composition into a location to be cemented; and allowing the settable composition to set therein. The location to be cemented may be above ground or in a subterranean formation.
摘要:
Settable compositions that comprise water, CKD, and microspheres, wherein the lightweight settable composition has a density less than about 13 pounds per gallon. Methods of cementing that comprise providing a lightweight settable composition having a density less than about 13 pounds per gallon, the lightweight settable composition comprising water, CKD, and microspheres, introducing the lightweight settable composition into a location to be cemented and allowing the lightweight settable composition to set therein.
摘要:
Cement compositions that include improved lost circulation materials are provided. In certain exemplary embodiments, the improved lost circulation materials include inelastic particles of polyethylene, polystyrene, and/or polypropylene. Optionally, the cement compositions also may include additives such as fly ash, a surfactant, a dispersant, a fluid loss control additive, a conventional lost circulation material, an accelerator, a retarder, a salt, a mica, fiber, a formation-conditioning agent, fumed silica, bentonite, expanding additives, microspheres, weighting materials, or a defoamer.