摘要:
A polymer compound for use as a binder for a negative electrode of an electrical storage device is formed by condensing polyacrylic acid and a multifunctional amine represented by the following formula (1), in which Y represents a straight chain alkyl group having 1 to 4 carbon atoms, a phenylene group, or an oxygen atom, and R1 and R2 each independently represent one or more hydrogen atoms, methyl groups, ethyl groups, trifluoromethyl groups, or methoxy groups.
摘要:
A production process for carbon-coated silicon material includes the step of: heating CaSi2 and a halogen-containing polymer at a temperature being a carbonization temperature or more of the halogen-containing polymer in a state where the CaSi2 and the halogen-containing polymer coexist.
摘要:
A negative-electrode active material is used for a negative electrode, the negative-electrode active material including: agglomerated particles including nanometer-size silicon produced by heat treating a lamellar polysilane having a structure in which multiple six-membered rings constituted of a silicon atom are disposed one after another, and expressed by a compositional formula, (SiH)n; and a carbon layer including amorphous carbon, and covering at least some of the agglomerated particles to be composited therewith. An electric storage apparatus including the same is not only able to reduce the irreversible capacity, but also able to inhibit the generation of “SEI.”
摘要:
A negative electrode active material is composed of a silicon material coated with a carbon layer containing a Group 4 to 6 metal.A method for producing a negative electrode active material includes a step of decomposing a compound containing the Group 4 to 6 metal and a carbon source by heating in the presence of a silicon material, the compound, and the carbon source.
摘要:
A polymer compound is formed by condensing a polyacrylic acid having some of carboxyl groups converted into a lithium salt with a polyfunctional amine represented by the following general formula (1). A chain structure constituted by the polyacrylic acid has free carboxyl groups and carboxyl groups converted into a lithium salt. Y is a straight-chain alkyl group having 1 to 4 carbon atoms, a phenylene group, or an oxygen atom. R1 and R2 are each independently one or more hydrogen atoms, a methyl group, an ethyl group, a trifluoromethyl group, or a methoxy group.
摘要:
Providing a silicon-containing material having a novel structure being distinct from the structure of conventional silicon oxide disproportionated to use.A silicon-containing material according to the present invention includes at least the following: a continuous phase including silicon with Si—Si bond, and possessing a bubble-shaped skeleton being continuous three-dimensionally; and a dispersion phase including silicon with Si—O bond, and involved in an area demarcated by said continuous phase to be in a dispersed state.
摘要:
A method for producing a silicon material, the method including: a step of heating CaSi2 powder in a range of 400 to 1000° C.; a step of reacting acid with the CaSi2 powder having been subjected to the step of heating CaSi2 powder in a range of 400 to 1000° C., to obtain a layered silicon compound; and a step of heating the layered silicon compound at not less than 300° C.
摘要:
To provide a nonaqueous electrolyte secondary battery that suppresses elution of Al from a positive electrode current collector formed of aluminum or an aluminum alloy, and is superior in thermal characteristics and input-output characteristics. Provided is a nonaqueous electrolyte secondary battery including a positive electrode, a negative electrode, and an electrolytic solution. The positive electrode has a positive electrode current collector formed of aluminum or an aluminum alloy. The electrolytic solution contains a metal salt and an organic solvent having a heteroelement. Regarding an intensity of a peak derived from the organic solvent in a vibrational spectroscopy spectrum of the electrolytic solution, Is>Io is satisfied when an intensity of an original peak of the organic solvent is represented as Io and an intensity of a peak resulting from shifting of the original peak is represented as Is.
摘要:
Provided is a negative electrode active material including complex particles formed of: nano silicon aggregated particles produced by heating a layered polysilane represented by a composition formula of (SiH)n and having a structure in which multiple six-membered rings formed from silicon atoms are connected; and a composited carbon layer formed from an amorphous carbon and at least covering one portion of the aggregated particles. A mean particle diameter D50 of the aggregated particles is within a range of 0.2 μm to 30 μm, and a mean particle diameter D50 of the complex particles is within a range of 0.5 μm to 40 μm.
摘要:
Provided is a negative electrode for a nonaqueous secondary battery which achieves both suppression of reductive decomposition of an electrolyte or an electrolytic solution and suppression of an increase in resistance. Also provided are a method for producing such a negative electrode and a nonaqueous secondary battery employing such a negative electrode. A polymer coating layer is formed so as to coat at least part of surfaces of negative electrode active material particles containing silicon oxide (SiOx; 0.5≦x≦1.6). The polymer coating layer contains a cationic polymer having a positive zeta potential under neutral conditions. Since silicon oxide has a negative zeta potential, a thin uniform coating layer can be formed owing to Coulomb's force.