    摘要: This invention relates to a coating composition for precoated steel sheets which are required to have high hardness, high workability and high distinctness of image, and to a method for producing a precoated steel sheet having a coating film of the composition. The composition is prepared by adding a compound of any of the following (a) to (c) to a coating composition consisting essentially of a polyol and containing, as the curing agent, an isocyanate compound or an amino resin, and the coating film of the composition has both high-level workability and high-level hardness.(a) Polyester compounds comprising main repeating units of a general formula (1): ##STR1## wherein n is an integer; and R is an alkylene group having 10 or less carbon atoms, or a 1,4-cyclohexylene-dimethylene group, or a neopentylene group, or a polyoxyalkylene group.(b) Polyester compounds comprising main repeating units of a general formula (2): ##STR2## wherein n is an integer of 10 or less; and R is an alkylene group having 10 or less carbon atoms, or a 1,4-cyclohexylene-dimethylene group, or a neopentylene group.(c) Compounds having the structure of a general formula (3):HO--(CH.sub.2).sub.n --O--R--O--(CH.sub.2).sub.n --OH (3)wherein n is an integer of from 2 to 10; and R is ##STR3##

    摘要翻译: 本发明涉及要求具有高硬度,高加工性和高清晰度的预涂钢板用涂料组合物,以及具有该组合物涂膜的预涂钢板的制造方法。 通过将以下(a)〜(c)中任一项所述的化合物添加到基本上由多元醇组成的涂料组合物中,作为固化剂含有异氰酸酯化合物或氨基树脂, 该组合物具有高水平的可加工性和高水平的硬度。 (a)包含通式(1)的主要重复单元的聚酯化合物:其中n是整数; R为碳原子数为10以下的亚烷基,1,4-亚环己基 - 二亚甲基,新戊烯基或聚氧化烯基。 (b)包含通式(2)的主要重复单元的聚酯化合物:其中n为10以下的整数; R为碳原子数为10以下的亚烷基或1,4-亚环己基 - 二亚甲基或新戊烯基。 (c)具有通式(3)结构的化合物:HO-(CH2)n-O-R-O-(CH2)n-OH(3)其中n为2至10的整数; 和R是

    Coating composition for precoated steel sheet, precoated steel sheet,
and process for preparing the same
    2.
    发明授权
    Coating composition for precoated steel sheet, precoated steel sheet, and process for preparing the same 失效
    预涂钢板,预涂钢板的涂料组合物及其制备方法

    公开(公告)号:US06136455A

    公开(公告)日:2000-10-24

    申请号:US155275

    申请日:1998-10-22

    摘要: The invention relates to a thermosetting coating composition for precoated steel sheets which are required to have high hardness, good workability and stain resistance, to a precoated steel sheet having a film of the coating composition, and to a method for producing such precoated steel sheets. The coating composition for precoated steel sheets of the invention consists essentially of a polyol and contains a specific compound and a curing agent composed of polyisocyanate compounds added thereto, in which the curing agent is a mixture composed of a blocked polyisocyanate compound as obtained by blocking one or more polyisocyanate compounds selected from polyisocyanates of the following group (a) and their derivatives, and a blocked polyisocyanate compound as obtained by blocking one or more polyisocyanate compounds selected from polyisocyanates of the following group (b) and their derivatives:(a) 4,4'-diphenylmethane diisocyanate, isophorone diisocyanate, tolylene diisocyanate, xylylene diisocyanate, naphthalene-1,5-diisocyanate;(b) hexamethylene diisocyanate, trimethylhexamethylene diisocyanate, hydrogenated 4,4'-diphenylmethane diisocyanate, hydrogenated tolylene diisocyanate, hydrogenated xylylene diisocyanate.The coating composition forms a coating film having good workability, high hardness and good stain resistance.

    摘要翻译: PCT No.PCT / JP98 / 00350 Sec。 371日期:1998年10月22日 102(e)1998年10月22日日期PCT提交1998年1月28日PCT公布。 出版物WO98 / 32808 日期:1998年7月30日本发明涉及对具有该涂料组合物的膜的预涂钢板,要求具有高硬度,良好的加工性和耐污性要求的预涂钢板的热固性涂料组合物, 这样的预涂钢板。 本发明的预涂钢板用涂料组合物基本上由多元醇组成,并含有特定的化合物和由加入的多异氰酸酯化合物组成的固化剂,其中固化剂是由封闭的多异氰酸酯化合物组成的混合物, 或更多种选自下列基团(a)的多异氰酸酯及其衍生物的多异氰酸酯化合物,以及通过封闭一种或多种选自以下组(b)的多异氰酸酯及其衍生物的多异氰酸酯化合物获得的封端多异氰酸酯化合物:(a)4 4'-二苯基甲烷二异氰酸酯,异佛尔酮二异氰酸酯,甲苯二异氰酸酯,苯二甲基二异氰酸酯,萘-1,5-二异氰酸酯; (b)六亚甲基二异氰酸酯,三甲基六亚甲基二异氰酸酯,氢化4,4'-二苯基甲烷二异氰酸酯,氢化甲苯二异氰酸酯,氢化苯二甲基二异氰酸酯。 涂料组合物形成具有良好的加工性,高硬度和良好耐污性的涂膜。

    Resin composition for toners
    3.
    发明授权
    Resin composition for toners 失效
    调色剂用树脂组合物

    公开(公告)号:US5409989A

    公开(公告)日:1995-04-25

    申请号:US173475

    申请日:1993-12-27

    摘要: A resin composition for toners, composed essentially of a suspension polymerizate of:(a) 5 to 40% by weight per total polymer of a polyester comprising at least one aromatic diol component an at least one aliphatic diol component, and having a weight average molecular weight of 3,000 to 30,000, an acid value of 0.5 to 10 mgKOH/g, and an OH value of 10 to 60 mgKOH/g;(b) 60 to 95% by weight per total polymer of a vinyl monomer; and(c) 0.1 to 1.0% by weight per total polymer of a divinyl monomer,wherein said suspension polymerizate hasa glass transition temperature of 40.degree. to 70.degree. C.,an acid value of 0.1 to 10 mgKOH/g, anda softening temperature of 100.degree. to 160.degree. C.

    摘要翻译: 一种用于调色剂的树脂组合物,其主要由以下组成的悬浮聚合物组成:(a)每聚合物总重量为5至40重量%,所述聚酯包含至少一种芳族二醇组分,至少一种脂族二醇组分,并且具有重均分子量 重量为3000〜30,000,酸值为0.5〜10mgKOH / g,OH值为10〜60mgKOH / g; (b)相对于乙烯基单体的总聚合物为60〜95重量% 和(c)相对于二乙烯基单体的总聚合物为0.1〜1.0重量%,其中所述悬浮聚合物的玻璃化转变温度为40〜70℃,酸值为0.1〜10mgKOH / g,软化 温度在100〜160℃

    Polymer for toner, process for preparation thereof and toner composition
    4.
    发明授权
    Polymer for toner, process for preparation thereof and toner composition 失效
    调色剂用聚合物,其制备方法和调色剂组合物

    公开(公告)号:US4971879A

    公开(公告)日:1990-11-20

    申请号:US349969

    申请日:1989-05-08

    摘要: A polymer binder, in which the content of a residual monomer is not more than 200 ppm, generates a smell only to a very slight extent and provides a toner having an improved blocking resistance and resistance against a plasticizer for polyvinyl chloride. The polymer binder is prepared by maintaining a polymer suspension obtained by suspension polymerization at a temperature of not lower than the glass transition temperature of the polymer and distilling water in an amount of 5 to 60% by weight based on the amount of water present at the time of termination of the polymerization.

    摘要翻译: 残留单体的含量不超过200ppm的聚合物粘合剂仅产生非常微小的气味,并提供具有改善的耐粘连性和耐聚氯乙烯增塑剂的调色剂。 聚合物粘合剂是通过将聚合物悬浮液保持在不低于聚合物的玻璃化转变温度的温度和蒸馏水中而制备的,所述聚合物悬浮液的量为5至60重量%,基于存在于 聚合终止时间。

    Copying apparatus equipped with control device
    5.
    发明授权
    Copying apparatus equipped with control device 失效
    配备控制装置的复印机

    公开(公告)号:US4455080A

    公开(公告)日:1984-06-19

    申请号:US315649

    申请日:1981-10-27

    IPC分类号: G03G15/00

    CPC分类号: G03G15/5012

    摘要: A copying apparatus equipped with an improved control device for controlling a copying operation, and including a device for generating a start signal for starting the copying operation, a paper feeding device for starting feeding of copy paper sheets in response to the starting of the copying operation. The control device comprises a device for generating a stop signal for stopping the copying operation and a device for preventing starting of operation of at least the paper feeding device when the stop signal is generated after the start signal has been generated and before the paper feeding device is operated.

    摘要翻译: 一种复印装置,配备有用于控制复印操作的改进的控制装置,并且包括用于产生用于开始复印操作的开始信号的装置,用于响应于复印操作的开始而开始复印纸张的馈送的送纸装置 。 控制装置包括用于产生用于停止复印操作的停止信号的装置和用于在起动信号已经产生之后产生停止信号时以及在供纸装置之前防止至少送纸装置的操作开始的装置 被操作

    Curable Liquid Silicone Rubber Composition For Forming A Sealing Member And Sealing Member
    6.
    发明申请
    Curable Liquid Silicone Rubber Composition For Forming A Sealing Member And Sealing Member 有权
    用于形成密封件和密封件的可固化液体硅橡胶组合物

    公开(公告)号:US20130011606A1

    公开(公告)日:2013-01-10

    申请号:US13519300

    申请日:2010-12-28

    IPC分类号: C08L83/07 B29C43/02 C08K3/36

    摘要: A liquid silicone rubber composition comprising an alkenyl group-containing liquid organopolysiloxane, a reinforcing silica filler, an organohydrogenpolysiloxane, a platinum group catalyst, a liquid organopolysiloxane that is free of crosslinking groups and is compatible with the alkenyl group-containing liquid organopolysiloxane, and a liquid organopolysiloxane that is free of crosslinking groups and is incompatible with the alkenyl group-containing liquid organopolysiloxane, wherein the cured material therefrom has a JIS type A durometer hardness of 15 to 26 and a tensile stress at 100% elongation of 0.25 to 0.60 MPa. Also, a through hole-containing sealing member comprising this cured material.

    摘要翻译: 含有含链烯基的液体有机聚硅氧烷,增强二氧化硅填料,有机氢聚硅氧烷,铂族催化剂,不含交联基团且与含链烯基的液体有机聚硅氧烷相容的液体有机聚硅氧烷的液态硅橡胶组合物和 液态有机聚硅氧烷,其不含交联基团,与含链烯基的液体有机聚硅氧烷不相容,其中固化物的JIS A型硬度计硬度为15〜26,拉伸应力为100%伸长率为0.25〜0.60MPa。 而且,包括该固化材料的含通孔的密封构件。

    Filter Characteristics Regulating Method, Filter Characteristics Regulator, Filter, and Communication Apparatus
    7.
    发明申请
    Filter Characteristics Regulating Method, Filter Characteristics Regulator, Filter, and Communication Apparatus 审中-公开
    滤波器特性调节方法,滤波器特性调节器,滤波器和通信设备

    公开(公告)号:US20090289738A1

    公开(公告)日:2009-11-26

    申请号:US11886638

    申请日:2006-03-03

    IPC分类号: H03H7/12

    CPC分类号: H01P1/203 H01P1/2135

    摘要: When an attenuation pole produces, highly-efficient-izing and a miniaturization of a filter are enabled by changing the electric length between a branch point and each filter. The 1st band pass filter 5 that has the characteristics of center frequency f1, and the 2nd band pass filter 7 that has the characteristics of different center frequency f2 from center frequency f1, In co-planer filter 3 provided with transmission line 9 which connects the 1st band pass filter 5 and the 2nd band pass filter 7, and branch point 11 formed in transmission line 9. It is designed so that an attenuation pole may produce in either [at least] the 1st band pass filter 5 or the 2nd band pass filter 7, and the frequency region which the formation position of branch point 11 is adjusted and an attenuation pole produces is adjusted.

    摘要翻译: 当衰减极产生时,通过改变分支点和每个滤波器之间的电长度来实现滤波器的高效率化和小型化。 具有中心频率f1的特性的第一带通滤波器5和具有与中心频率f1不同的中心频率f2的特性的第二带通滤波器7.在配备有传输线9的共平面滤波器3中, 第一带通滤波器5和第二带通滤波器7以及在传输线9中形成的分支点11.它被设计成使得衰减极可以在[至少]第一带通滤波器5或第二带通 滤波器7和调整分支点11的形成位置并且衰减极产生的频率区域。

    Method For Preparation Of Aqueous Emulsion From Curable Silicone Composition And Suspension Of Cured Silicone Particles, And Apparatus Therefor
    8.
    发明申请
    Method For Preparation Of Aqueous Emulsion From Curable Silicone Composition And Suspension Of Cured Silicone Particles, And Apparatus Therefor 失效
    由固化硅酮组合物和固化硅氧烷颗粒悬浮液制备水性乳液的方法及其设备

    公开(公告)号:US20070155893A1

    公开(公告)日:2007-07-05

    申请号:US11680934

    申请日:2007-03-01

    IPC分类号: C08L83/00

    摘要: Method for preparation of an aqueous emulsion from a curable silicone composition consisting of (A) an organopolysiloxane having at least two silicon-bonded hydroxyl groups, (B) an organohydrogensiloxane, and (C) a curing catalyst, said method being characterized by (i) continuously supplying component (A), component (B) and component (C), or a mixture of components (A) and (B) and component (C) through individual inlet ports into a continuous mixer and mixing said components at a temperature not exceeding 10° C., (ii) continuously supplying the obtained mixture and (D) an aqueous solution of a surface-active agent to an emulsifier, and emulsifying the components at a temperature not exceeding 20° C. An apparatus for the preparation of an aqueous emulsion of a curable silicone composition comprising of a continuous mixer for mixing components (A) through (C), a distribution unit connected to the lower part of the mixer, and an emulsifier. Method for preparation of a suspension of cured silicone particles by allowing such emulsion to stand at room temperature, or heating the aforementioned emulsion.

    摘要翻译: 由(A)具有至少两个与硅键合的羟基的有机聚硅氧烷,(B)有机氢硅氧烷和(C)固化催化剂)组成的可固化有机硅组合物制备水乳液的方法,所述方法的特征在于(i )将组分(A),组分(B)和组分(C)或组分(A)和组分(B)和组分(C)的混合物通过各个入口端连续供给到连续混合器中,并在所述组分 不超过10℃,(ii)将所得混合物和(D)表面活性剂的水溶液连续供给到乳化剂中,并在不超过20℃的温度下乳化该组分。 的可固化硅氧烷组合物的水性乳液,其包含用于混合组分(A)至(C)的连续混合器,与混合器的下部连接的分配单元和乳化剂。 通过使这种乳液在室温下放置或加热上述乳液来制备固化的硅氧烷颗粒的悬浮液的方法。

    Toner resin composition and process for preparing same
    10.
    发明授权
    Toner resin composition and process for preparing same 失效
    调色剂树脂组合物及其制备方法

    公开(公告)号:US5342722A

    公开(公告)日:1994-08-30

    申请号:US878910

    申请日:1992-05-06

    摘要: A toner resin composition comprising 5 to 40% by weight of a polyester (A) having a weight average molecular weight of 3,000 to 20,000 and 50 to 95% by weight of a styrene-acrylic copolymer (B). The styrene-acrylic copolymer (B) is comprised of 10 to 25% by weight of a high molecular weight polymer (B1) having a weight average molecular weight of 500,000 to 1,100,000 and 75 to 90% by weight of a low molecular weight polymer (B2) having a weight average molecular weight of 5,000 to 100,000. The high molecular weight polymer (B1) is comprised of a styrene component (b-1) and an acrylic ester and/or methacrylic ester component (b-2). The low molecular weight polymer (B2) is comprised of a styrene component (b-1), an acrylic ester and/or methacrylic ester component (b-2), 0.3 to 3 parts by weight, per 100 parts of the total weight of said component (b-1) and component (b-2), of an .alpha.-methyl styrene dimer (b-3) and 0.5 to 30 parts by weight, per 100 parts by weight of said polyester (A), of a glycidyl methacrylate component (b-4).

    摘要翻译: 一种调色剂树脂组合物,其包含5至40重量%的重均分子量为3,000至20,000的聚酯(A)和50至95重量%的苯乙烯 - 丙烯酸共聚物(B)。 苯乙烯 - 丙烯酸共聚物(B)由10至25重量%的重均分子量为500,000至1,100,000和75至90重量%的低分子量聚合物的高分子量聚合物(B1) B2),其重均分子量为5,000〜100,000。 高分子量聚合物(B1)由苯乙烯组分(b-1)和丙烯酸酯和/或甲基丙烯酸酯组分(b-2)组成。 低分子量聚合物(B2)由苯乙烯组分(b-1),丙烯酸酯和/或甲基丙烯酸酯组分(b-2)组成,每100份总重量为0.3-3重量份 所述组分(b-1)和组分(b-2),α-甲基苯乙烯二聚物(b-3)和0.5-30重量份,相对于所述聚酯(A)100重量份, 甲基丙烯酸酯组分(b-4)。