    摘要: The present invention relates to electrochemical cells comprising (A) at least one cathode comprising at least one lithium ion-containing transition metal compound, (B) at least one anode, (C) at least one layer comprising (a) at least one lithium- and oxygen-containing, electrochemically active transition metal compound, and (b) optionally at least one binder, and (D) at least one electrically nonconductive, porous and ion-pervious layer positioned between cathode (A) and layer (C), and at least one electrically nonconductive, porous and ion-pervious layer positioned between anode (B) and layer (C). The present invention further relates to the use of inventive electrochemical cells, to the production thereof, and to a specific separator for the separation of a cathode and an anode in an electrochemical cell.

    摘要翻译: 本发明涉及电化学电池,其包含(A)至少一种阴极,其包含至少一种含锂离子的过渡金属化合物,(B)至少一种阳极,(C)至少一层,其包含(a)至少一种锂 和(b)任选的至少一种粘合剂,和(D)位于阴极(A)和层(C)之间的至少一个不导电,多孔和离子可渗透层, 以及位于阳极(B)和层(C)之间的至少一个不导电,多孔和离子可渗透层。 本发明还涉及本发明的电化学电池及其制备方法的使用,以及用于在电化学电池中分离阴极和阳极的特定隔板。

    Process for preparing precursors for transition metal mixed oxides
    9.
    发明授权
    Process for preparing precursors for transition metal mixed oxides 有权
    制备过渡金属混合氧化物前体的方法

    公开(公告)号:US09171652B2

    公开(公告)日:2015-10-27

    申请号:US13302007

    申请日:2011-11-22

    摘要: A process for preparing transition metal mixed oxide precursors, including: (A) precipitating, from aqueous solution at a pH of 8.0 to 9.0, a compound of formula (I): M(CO3)bOc(OH)dAmBe(SO4)fXg(PO4)h  (I), wherein: M is one or more transition metals, A is sodium or potassium, B is one or more metals of groups 1 to 3, excluding Na and potassium, X is halide, nitrate or carboxylate, b is 0.75 to 0.98, c is zero to 0.50, d is zero to 0.50, where the sum (c+d) is 0.02 to 0.50, e is zero to 0.1, f is zero to 0.05, g is zero to 0.05, h is zero to 0.10, m is 0.002 to 0.1, and (B) separating the precipitated material from the mother liquor, where the particles of material of formula (I) have a spherical shape.

    摘要翻译: 一种制备过渡金属混合氧化物前体的方法,包括:(A)从8.0至9.0的pH的水溶液中沉淀出式(I)化合物:M(CO 3)b O c(OH)d AmmBe(SO 4)f X g( PO 4)h(I),其中:M是一种或多种过渡金属,A是钠或钾,B是除了Na和钾之外的第1至3族的一种或多种金属,X是卤化物,硝酸盐或羧酸盐,b是 0.75至0.98,c为0至0.50,d为0至0.50,其中(c + d)之和为0.02至0.50,e为0至0.1,f为0至0.05,g为0至0.05,h为零 至0.10,m为0.002至0.1,和(B)将沉淀的材料与母液分离,其中式(I)的材料颗粒具有球形。