Method for producing magnetically active shape memory metal alloy
    3.
    发明授权
    Method for producing magnetically active shape memory metal alloy 失效
    制备磁性活性形状记忆金属合金的方法

    公开(公告)号:US07547367B2

    公开(公告)日:2009-06-16

    申请号:US10563173

    申请日:2003-07-03

    IPC分类号: H01F1/14 C22F1/10

    摘要: The invention relates to a method for producing magnetically active shape memory metal alloy, said metal alloy containing nickel, manganese and gallium. In the method, the different components of the metal alloy are melted, and the melt is homogenized essentially at the melting temperature; the obtained metal alloy is cast, and the cast metal alloy is subjected to directional solidification at 10-100° C. below the liquidus temperature of said metal alloy.

    摘要翻译: 本发明涉及一种用于制备磁性活性形状记忆金属合金的方法,所述金属合金含有镍,锰和镓。 在该方法中,金属合金的不同组分熔化,熔体基本上在熔融温度下均匀化; 将得到的金属合金铸造,铸造金属合金在所述金属合金的液相线温度以下10-100℃下进行定向凝固。

    Method for making a joint between copper and stainless steel
    4.
    发明授权
    Method for making a joint between copper and stainless steel 失效
    铜和不锈钢之间的接合方法

    公开(公告)号:US06740179B2

    公开(公告)日:2004-05-25

    申请号:US10203972

    申请日:2002-08-14

    IPC分类号: B23K20227

    摘要: A method for making a joint between copper or copper alloys and austenitic steel alloys, in which method in between the junction surfaces of the objects to be joined together, there is arranged at least one intermediate layer, so that the junction surfaces, including their intermediate layers, are pressed together, and at least the junction area is heated in order to create a diffusion joint. In the method, there is brought a first intermediate layer (3) on the junction surface of the steel object (2) or against said surface, in order to activate the creation of the diffusion joint.

    摘要翻译: 一种铜或铜合金与奥氏体钢合金之间的接合方法,其中在待接合物体的接合面之间的方法中至少设有一个中间层,使得接合面包括它们的中间层 层压在一起,并且至少加热接合区域以形成扩散接头。 在该方法中,为了激活扩散接头的产生,在钢体(2)的接合表面上或与所述表面接合的第一中间层(3)。

    Method for producing magnetically active shape memory metal alloy
    5.
    发明申请
    Method for producing magnetically active shape memory metal alloy 失效
    制备磁性活性形状记忆金属合金的方法

    公开(公告)号:US20070102067A1

    公开(公告)日:2007-05-10

    申请号:US10563173

    申请日:2003-07-03

    IPC分类号: H01F1/14

    摘要: The invention relates to a method for producing magnetically active shape memory metal alloy, said metal alloy containing nickel, manganese and gallium. In the method, the different components of the metal alloy are melted, and the melt is homogenized essentially at the melting temperature; the obtained metal alloy is cast, and the cast metal alloy is subjected to directional solidification at 10-100° C. below the liquidus temperature of said metal alloy.

    摘要翻译: 本发明涉及一种用于制备磁性活性形状记忆金属合金的方法,所述金属合金含有镍,锰和镓。 在该方法中,金属合金的不同组分熔化,熔体基本上在熔融温度下均匀化; 将得到的金属合金铸造,铸造金属合金在所述金属合金的液相线温度以下10-100℃下进行定向凝固。

    Method and device for treating anode slime
    7.
    发明授权
    Method and device for treating anode slime 失效
    用于处理阳极泥的方法和装置

    公开(公告)号:US07670575B2

    公开(公告)日:2010-03-02

    申请号:US11570857

    申请日:2005-07-05

    IPC分类号: C01B19/00 C22B7/00 F23B99/00

    摘要: The method and furnace according to the invention enable a continuous processing of anode slime and are particularly suited to be connected to a process where anode slime is treated by hydrometallurgic methods after roasting. In the method according to the invention, the slime containing valuable metals and selenium is dried, roasted, sulfatized and cooled. The method includes steps to be carried out in succession, in continuous operation, so that the slime forms a slime layer on the conveyor and is conveyed to be treated in successive drying, roasting, sulfatizing and sulfuric acid removal and cooling units.

    摘要翻译: 根据本发明的方法和炉能够连续处理阳极泥,并且特别适合于连接到焙烧后通过湿法冶金方法处理阳极泥的方法。 在根据本发明的方法中,含有有价金属和硒的泥被干燥,焙烧,硫酸化和冷却。 该方法包括在连续操作中连续执行的步骤,使得粘泥在输送机上形成粘液层,并被输送以在连续的干燥,焙烧,硫酸盐化和硫酸去除和冷却单元中进行处理。

    Method for the removal of mercury from sulphuric acid with thiosulphate precipitation
    8.
    发明授权
    Method for the removal of mercury from sulphuric acid with thiosulphate precipitation 有权
    用硫代硫酸盐沉淀从硫酸中去除汞的方法

    公开(公告)号:US07452521B2

    公开(公告)日:2008-11-18

    申请号:US10566680

    申请日:2004-07-16

    IPC分类号: C01B17/90

    摘要: This invention relates to a method for removing mercury from dilute sulphuric acid. According to the method sulphuric acid solution is scrubbed with an aqueous solution containing thiosulphate, which precipitates the mercury present in the sulphuric acid solution either as mercury sulphide or, in a chlorine-containing environment, as a mercury sulphide-mercury chloride double salt. The quantity of thiosulphate to be fed is adjusted so that it precipitates the mercury in the sulphuric acid solution, but still does not form elemental sulphur.

    摘要翻译: 本发明涉及从稀硫酸中去除汞的方法。 根据该方法,用含硫代硫酸盐的水溶液洗涤硫酸溶液,其将硫酸溶液中存在的汞作为硫化汞或在含氯环境中沉淀为硫化汞 - 氯化汞复盐。 调整供给的硫代硫酸盐的量,使其在硫酸溶液中析出汞,但仍不形成元素硫。

    Method for the stabilization of a fluidized bed in a roasting furnace
    9.
    发明授权
    Method for the stabilization of a fluidized bed in a roasting furnace 失效
    在焙烧炉中稳定流化床的方法

    公开(公告)号:US06926752B2

    公开(公告)日:2005-08-09

    申请号:US10416863

    申请日:2001-11-13

    IPC分类号: C22B1/02 C22B1/10 C22B19/02

    CPC分类号: C22B19/02 C22B1/10

    摘要: This invention relates to a method for stabilizing a fluidized bed used in roasting by adjusting the oxygen content of the roasting gas in the bed. The fine-grained material for roasting is fed into the furnace above the fluidized bed and the roasting gas, which causes the fluidizing, is fed into the bottom of the furnace through a grate. In this method, the total amount of oxygen in the roasting gas to be fed and the average total oxygen requirement of the material to be roasted are calculated and the ratio between them regulated so that the oxygen coefficient in the bed is over 1.

    摘要翻译: 本发明涉及通过调节床中焙烧气体的氧含量来稳定用于焙烧的流化床的方法。 用于焙烧的细粒材料被送入流化床上方的炉中,并且引起流化的焙烧气体通过炉排进入炉的底部。 在该方法中,计算要进料的焙烧气体中的氧气总量和待焙烧材料的平均总氧需求量,并且调节它们之间的比例,使床中的氧系数超过1。